| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.0 - 10 ohm-cm | 1.0 - 10 ohm-cm | ASTM D257 |
| PolyOne Therma-Tech™ LC-6000 TC Liquid Crystal Polymer (LCP) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
| Volume Resistivity | 1.0 - 10 ohm-cm | 1.0 - 10 ohm-cm | ASTM D257 |
| PolyOne Stat-Tech™ PK-30NCF/10T PEEK - 30% Nickel Coated Carbon Fiber - 10% PTFE
(discontinued **) Data provided by PolyOne. |
|||
| Volume Resistivity | 1.0 - 10 ohm-cm | 1.0 - 10 ohm-cm | ASTM D257 |
| PolyOne Stat-Tech™ AS-15NCF/000 ABS - 15% Nickel Coated Carbon Fiber
(discontinued **) Data provided by PolyOne. |
|||
| Volume Resistivity | 1.0 - 10 ohm-cm | 1.0 - 10 ohm-cm | ASTM D257 |
| PolyOne Therma-Tech™ SF-6000 TC Polyphenylene Sulfide (PPS)
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
| Volume Resistivity | 1.0 - 10 ohm-cm | 1.0 - 10 ohm-cm | ASTM D257 |
| Techmer ES Electrablend® ABS SS5 5% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 5% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Information provided by TP Composites, Inc. |
|||
| Volume Resistivity | 1.0 - 10 ohm-cm | 1.0 - 10 ohm-cm | ASTM D257 |
| Techmer ES Electrablend® ABS SS5 FR 5% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 5% Filler by WeightFeatures: Electromagnetic Shielding (EMI) and Flame RetardantInformation provided by TP Compo.. |
|||
| Volume Resistivity | 1.0 - 10 ohm-cm | 1.0 - 10 ohm-cm | ASTM D648 |
| Techmer ES Electrafil® J-1/CF/40 BK PA66 |
|||
| Volume Resistivity | 1.0 - 10 ohm-cm | 1.0 - 10 ohm-cm | ASTM D648 |
| Techmer ES Electrafil® J-1/CF/40 NAT PA66 |
|||
| Volume Resistivity | 1.0 - 10 ohm-cm | 1.0 - 10 ohm-cm | ASTM D648 |
| Techmer ES Electrafil® J-1200/CF/20 NAT ABS |
|||
| Volume Resistivity | 1.0 - 10 ohm-cm | 1.0 - 10 ohm-cm | ASTM D648 |
| Techmer ES Electrafil® J-80/CF/20 NAT Acetal (POM) Copolymer |
|||
| Volume Resistivity | 0.10 - 10 ohm-cm | 0.10 - 10 ohm-cm | IEC 60093 |
| Teijin Panlite® BS-8120R Friction and Abrasion Resistant, Carbon Fiber Reinforced Polycarbonate Resin CF 20% reinforced grade, meeting UL 94 V-2. it is compounded with fluorine powder to improve friction and abrasion resistance and also exhibits a mold release property, maintaining excellent charact.. |
|||
| Volume Resistivity | 1.0 - 10 ohm-cm | 1.0 - 10 ohm-cm | ASTM D257 |
| Techmer ES Electrablend® ABS SS15 BK MB 15% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 15% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Appearance: BlackInformation provided by TP Composi.. |
|||
| Volume Resistivity | 1.0 - 10 ohm-cm | 1.0 - 10 ohm-cm | ASTM D257 |
| Techmer ES Electrablend® HDPE C BK Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveAppearance: BlackTPCI# 9411115Information provided by TP Composites, Inc. |
|||
| Volume Resistivity | 1.0 - 10 ohm-cm | 1.0 - 10 ohm-cm | ASTM D257 |
| Techmer ES Electrablend® PA6 04001 BK MB Glass/Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Stainless Steel FiberAdditive: LubricatedFeatures: Electromagnetic Shielding (EMI), Lubricated and Radio Frequency Shielding (RFI.. |
|||
| Volume Resistivity | 1.0 - 10 ohm-cm | 1.0 - 10 ohm-cm | ASTM D257 |
| Techmer ES Electrablend® PA6 04001 BL Glass/Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Stainless Steel FiberAdditive: LubricatedFeatures: Electromagnetic Shielding (EMI), Lubricated and Radio Frequency Shielding (RFI.. |
|||
| Volume Resistivity | 1.0 - 10 ohm-cm | 1.0 - 10 ohm-cm | ASTM D257 |
| Techmer ES Electrablend® PA6 04001 FR MB Glass/Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Stainless Steel FiberAdditive: LubricatedFeatures: Electromagnetic Shielding (EMI), Lubricated, Flame Retardant and Radio Frequen.. |
|||
| Volume Resistivity | 5.0 - 10 ohm-cm | 5.0 - 10 ohm-cm | |
| Master Bond EP21TDCN Two Component Nickel Conductive Epoxy Adhesive Product Description: Master Bond Polymer System EP21TDCN is a two component, nickel filled, electrically conductive, adhesive for high performance bonding, formulated to cure at room temperature or .. |
|||
| Volume Resistivity | 5.0 - 10 ohm-cm | 5.0 - 10 ohm-cm | |
| Master Bond EP21TDCNFL Two Component Nickel Conductive Epoxy Adhesive Master Bond Polymer System EP21TDCNFL is a two component, nickel filled, electrically conductive system for high performance bonding and sealing formulated to cure at room temperature or more rapidl.. |
|||
| Volume Resistivity | 5.0 - 10 ohm-cm | 5.0 - 10 ohm-cm | |
| Master Bond EP76M-F Electrically Conductive, Two Part Epoxy Description: Master Bond EP76M-F is a two component, nickel filled, electrically conductive epoxy system for high performance bonding, sealing, and coating formulated to cure at room temperature or .. |
|||
| Volume Resistivity | 0.10 - 10 ohm-cm | 0.10 - 10 ohm-cm | IEC 60093 |
| Teijin Panlite® B-8120R Carbon Fiber Reinforced Polycarbonate Resin CF 20% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are low molding shrinkage and dimensional accuracy.Applica.. |
|||
| Volume Resistivity | 0.10 - 10 ohm-cm | 0.10 - 10 ohm-cm | IEC 60093 |
| Teijin Panlite® BN-8120R Improved Mold Release, Carbon Fiber Reinforced, Flame Resistant Polycarbonate Resin CF 20% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are flame retardance, low molding shrinkage and dimensiona.. |
|||