Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Radici Radilon® A HSX (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Radici Radilon® A RV300RKC (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Radici Radilon® A RV330 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Radici Radilon® S 35HR (cond.) Nylon 6 PA6 medium-high viscosity injection molding grade. Easy mould release.Information provided by Radici group. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Radici Radilon® S CP400 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Volume Resistivity | >= 1.00e+11 ohm-cm | >= 1.00e+11 ohm-cm | |
Radici Radilon® S ESL128 (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Radici Radilon® S HSX88 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Radici Radilon® S RV200 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Volume Resistivity | >= 1.00e+11 ohm-cm | >= 1.00e+11 ohm-cm | |
Radici Radilon® S RV200 (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Radici Radilon® S RV300 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Volume Resistivity | >= 1.00e+11 ohm-cm | >= 1.00e+11 ohm-cm | |
Radici Radilon® S USZ200 (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Volume Resistivity | 1.00e+11 - 1.00e+12 ohm-cm | 1.00e+11 - 1.00e+12 ohm-cm | IEC 60093 |
Raschig Group MELOPLAS® 181 MF Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. High surface hardness, good electrical properties, good mechanical strength, high UV and heat resistanc.. |
|||
Volume Resistivity | 1.00e+11 - 1.00e+12 ohm-cm | 1.00e+11 - 1.00e+12 ohm-cm | IEC 60093 |
Raschig Group MELOPLAS® 3025 MF Cellulose-reinforced and inorganically filled MF molding compound in white and colored shades. High surface hardness, good UV and heat stability, very good resistance to chemicals - also to foodstu.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm @Temperature 23.0 °C |
1.00e+11 ohm-cm @Temperature 73.4 °F |
50%RH; IEC 60093 |
DuPont Performance Polymers Zytel® LM70G35HSLX BK314 Nylon 66
(Unverified Data**) Zytel® LM70G35HSLX is a 35% glass fiber reinforced, heat stabilized, lubricated polyamide 66 for injection molding. It is well suited for laser marking.Information provided by DuPont Performance Po.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | IEC 60093 |
Hexion Bakelite™ X65 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, inorganically/organically filled, good heat-resistance and dimensional stability, UL listed molding compound 3.0 mm/V-0 (BN, BK).Application areas: Oven strips.Information.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | IEC 60093 |
Solvay TECHNYL® B 230 PA66/6, Conditioned Description: Unreinforced and modified copolyamide 66/6, with high flexibility and improved impact resistance, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHN.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | ASTM D257 |
Tipco Tipcolite® THR 211 Phenolic Compound, Asbestos Wood Flour & Minerals, Soft Flow & High Electrical Properties Soft Flow Phenolic Compound, Reinforced with Asbestos Wood Flour & MineralsApplications: Switchgear, HRC FusesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industrie.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Tra-Con Tra-Bond F118CLR Fiber Optic Epoxy Adhesive TRA-BOND F118CLR is an impact resistant, fiber-optic adhesive designed for use in any optical connector. This two-part epoxy remains at a constant viscosity for a minimum of 30 minutes. This allows .. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | IEC 60093 |
Ter Hell Plastic Terez® PBT 6750 T Polybutylene Terephthalate, Impact Modified Description: Impact modified PBT.Application: For impact stressed, injection molding parts.Information provided by Ter Hell Plastic GMBH. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | dry; IEC 60093 |
EMS-Grivory Grivory® 2S 25 W 20 HL X black 9992 PA610 Product Description: Grilamid 2S 25 W 20 HL X black 9992 is a semi-flexible high viscosity heat stabilized, impact modified and plasticized Polyamide 610, especially suitable for extrusion applicati.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | dry; IEC 60093 |
EMS-Grivory Grivory® 2SV-30H black 9992 PA610-GF30 Product Description: GRILAMID XE 3976 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mate.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | conditioned; IEC 60093 |
EMS-Grivory Grivory® 2SV-30H nat PA610-GF30 Product Description: GRILAMID XE3976 natural 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mat.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | conditioned; IEC 60093 |
EMS-Grivory Grivory® XE 4073 nat PA610 Product description: Grilamid XE 4073 natural is a unreinforced, heat and UV stabilized polyamide 610 (PA610) injection molding grade. This product is to a large extent based on renewable raw materi.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | dry; IEC 60093 |
EMS-Grivory Grivory® HT XE 4027 black 9916 PA*-GF30 Product description: Grivory XE 4027 black 9916 is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semicrystalline, partially aromatic copolyam.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | 50%RH; IEC 60093 |
DuPont Performance Polymers Zytel® 103FHS NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103FHS NC010 is a heat stabilized internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivi.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | Conditioned; CEI 60093 |
Addiplast Addinyl A2 ZP40 Nylon 66, 40% Mineral Filled Mineral filled, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Volume Resistivity | 1.00e+11 ohm-cm @Thickness 0.750 mm |
1.00e+11 ohm-cm @Thickness 0.0295 in |
IEC 60093 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Volume Resistivity | >= 1.00e+11 ohm-cm | >= 1.00e+11 ohm-cm | |
Radici Radilon® A RV300 990 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | IEC 60093 |
Hexion Bakelite™ PF 4041 Phenolic Formaldehyde Resin, Resistant to High Temperatures
(discontinued **) Phenolic molding compound, glass fiber reinforced and inorganically filled, elasticized. Very good heat resistance, very good mechanical properties, reduced mold shrinkage and post-shrinkage, good .. |