Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | <= 0.10 ohm-cm | <= 0.10 ohm-cm | |
P & P Technology Conductive Elastomer Nickel Graphite particlesInformation provided by P & P Technology |
|||
Volume Resistivity | 0.10 ohm-cm | 0.10 ohm-cm | DC |
Parker Chomerics CHO-LUBE 4220 Electrically Conductive Grease CHO-LUBE 4220 conductive grease is based on silicone fluid, which is characterized by unusual chemical inertness and outstanding thermal stability. It is a silver-filled lubricant designed for surfa.. |
|||
Volume Resistivity | 0.10 ohm-cm | 0.10 ohm-cm | CEPS-0002 |
Parker Chomerics CHO-SEAL 6370 Conductive Elastomer Commercial Grade Conductive Elastomer Extrusions. These materials offer excellent cost/performance characteristics for commercial EMI gasket applications. These silicone and fluorosilicone based con.. |
|||
Volume Resistivity | 0.10 ohm-cm | 0.10 ohm-cm | as supplied without pressure sensitive adhesive |
Parker Chomerics CHO-SEAL S6304 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Volume Resistivity | 0.10 ohm-cm | 0.10 ohm-cm | as supplied without pressure sensitive adhesive; CEPS-0002 |
Parker Chomerics CHO-SEAL S6305 Conductive Elastomer Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded and Extruded.RoHS CompliantInformation provi.. |
|||
Volume Resistivity | <= 0.10 ohm-cm | <= 0.10 ohm-cm | without pressure-sensitive adhesive; CEPS-0002 |
Parker Chomerics CHO-SEAL® 6308 Conductive Elastomer Description: Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Extruded onlyRoHS CompliantInformation.. |
|||
Volume Resistivity | 0.10 ohm-cm | 0.10 ohm-cm | without pressure-sensitive adhesive; CEPS-0002 |
Parker Chomerics CHO-SEAL® 6310 Extruded Elastomer Low Cost Commercial Grade Extruded Elastomer. CHO-SEAL 6310 is the latest addition to Chomerics line of low cost, commercial grade EMI gaskets. This extruded material combines nickel-plated graphite.. |
|||
Volume Resistivity | 0.10 ohm-cm | 0.10 ohm-cm | |
Parker Chomerics CHO-SEAL® 6370 Conductive Elastomer Flame Retardant Conductive Silicone Elastomer. CHO-SEAL 6370 EMI gaskets are conductive elastomers engineered for use in commercial electronic equipment where a high degree of flame retardancy and c.. |
|||
Volume Resistivity | 0.10 ohm-cm | 0.10 ohm-cm | without psa; CEPS-002 |
Parker Chomerics CHO-SEAL® 6371 Conductive Elastomer Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded onlyRoHS Compliant Information provided by C.. |
|||
Volume Resistivity | <= 0.10 ohm-cm | <= 0.10 ohm-cm | Cured; QAP-1017 |
Parker Chomerics Tecknit CON/RTV-Ni 2 Part Nickel Filled RTV Description: TECKNIT electrically conductive, medium viscosity adhesive- sealant system. It is formulated with a special conductive material producing its own unique advantages. After full cure, the.. |
|||
Volume Resistivity | <= 0.10 ohm-cm | <= 0.10 ohm-cm | |
Parker Chomerics Tecknit NC-Consil® 750 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Volume Resistivity | <= 0.10 ohm-cm | <= 0.10 ohm-cm | |
Parker Chomerics Tecknit NC-Consil® 751 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Volume Resistivity | <= 0.10 ohm-cm | <= 0.10 ohm-cm | |
Parker Chomerics Tecknit NC-Consil® 770 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Volume Resistivity | <= 0.10 ohm-cm | <= 0.10 ohm-cm | |
Parker Chomerics Tecknit NC-Consil® FR750 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Volume Resistivity | <= 0.10 ohm-cm | <= 0.10 ohm-cm | |
Parker Chomerics Tecknit NC-Consil® FR751 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Volume Resistivity | 0.10 - 10 ohm-cm | 0.10 - 10 ohm-cm | IEC 60093 |
Teijin Panlite® BS-8120R Friction and Abrasion Resistant, Carbon Fiber Reinforced Polycarbonate Resin CF 20% reinforced grade, meeting UL 94 V-2. it is compounded with fluorine powder to improve friction and abrasion resistance and also exhibits a mold release property, maintaining excellent charact.. |
|||
Volume Resistivity | 0.10 ohm-cm | 0.10 ohm-cm | |
COI Ceramics Nicalon™ HI Type S SiC Ceramic Fiber Description: A stoichiometric beta-SiC fiber manufactured near-oxygen-free using decarbonization pyrolysis and electron-beam curing. It has higher modulus, creep resistance and oxidation resistance .. |
|||
Volume Resistivity | 0.10 - 10 ohm-cm | 0.10 - 10 ohm-cm | IEC 60093 |
Teijin Panlite® B-8120R Carbon Fiber Reinforced Polycarbonate Resin CF 20% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are low molding shrinkage and dimensional accuracy.Applica.. |
|||
Volume Resistivity | 0.10 - 10 ohm-cm | 0.10 - 10 ohm-cm | IEC 60093 |
Teijin Panlite® BN-8120R Improved Mold Release, Carbon Fiber Reinforced, Flame Resistant Polycarbonate Resin CF 20% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are flame retardance, low molding shrinkage and dimensiona.. |