Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Parker Chomerics Tecknit NC-Consil® 751 Nickel Coated Graphite Filled Silicone Elastomer

Category Polymer , Thermoset , Silicone
Manufacturer Parker Chomerics Tecknit
Trade Name NC-Consil®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics Tecknit NC-Consil® 751 Nickel Coated Graphite Filled Silicone Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil is designed to provide reliable cost effective shielding for a wide range of EMI applications ideal for the commercial market.Typical Applications: NC-Consil should be used where there is a need for high broadband shielding combined with excellent environmental sealing properties.Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 1.74 - 2.26 g/cc
1.74 - 2.26 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 45 - 65
45 - 65
ASTM D2240
Tensile Strength >= 1.03 MPa
>= 150 psi
ASTM D412
Elongation at Break >= 100 %
>= 100 %
ASTM D412
Tear Strength 7.01 kN/m
40.0 pli
ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 160 °C
320 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 0.10 ohm-cm
<= 0.10 ohm-cm
Shielding Effectiveness 85 dB

@Frequency 1.00e+10 Hz
85 dB

@Frequency 1.00e+10 Hz
Plane Wave
100 dB

@Frequency 100000 Hz
100 dB

@Frequency 100000 Hz
H-Field
100 dB

@Frequency 1.00e+7 Hz
100 dB

@Frequency 1.00e+7 Hz
E-Field
100 dB

@Frequency 1.00e+9 Hz
100 dB

@Frequency 1.00e+9 Hz
Plane Wave
Descriptive Properties Value Comments
Binder Silicone
Color Dark Gray
Filler Nickel Coated Graphite