Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 0.010 ohm-cm | 0.010 ohm-cm | |
Premix Thermoplastics PRESEAL 6080 Ag-Coated Glass Metal replacement is one of the fastest growing areas for conductive plastics. Plastics, with their lighter weight, good processability and optimal combination of mechanical properties have challeng.. |
|||
Volume Resistivity | 0.010 ohm-cm | 0.010 ohm-cm | ASTM D257 |
Premix Thermoplastics PRESEAL® TPE 6080 General Description:PRESEAL® TPE 6080 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It can also be used as conductors or in grounding.. |
|||
Volume Resistivity | <= 0.010 ohm-cm @Temperature 100 °C, Time 2700 sec |
<= 0.010 ohm-cm @Temperature 212 °F, Time 0.750 hour |
|
Parker Chomerics CHO-BOND 360-208 Conductive Epoxy Low cost, electrically conductive epoxy adhesive that combines the good adhesive characteristics as epoxy, and the superior electrical conductivity of silver. It is recommended as a thermo-setting E.. |
|||
Volume Resistivity | <= 0.010 ohm-cm | <= 0.010 ohm-cm | |
Parker Chomerics CHO-BOND® 1121 General Purpose Adhesive-Sealant Silver Silicone Description: Xylene-free version of CHO-BOND 1038; rec. bond line thickness: > 0.18 mm; primer promotes adhesion CHO-BOND® 1121 is an electrically conductive, one-component silicone adhesive-sealan.. |
|||
Volume Resistivity | 0.010 ohm-cm | 0.010 ohm-cm | Post Tensile Set; MIL-DTL-83528 Para.4.6.9 |
Parker Chomerics CHO-SEAL 1212 Conductive Elastomer High strength, hard (80 shore A) material for waveguide, choke, cover, and flanges with grooves for EMI and pressure sealing.Molded onlyRoHS Compliant Information provided by Chomerics |
|||
Volume Resistivity | 0.010 ohm-cm | 0.010 ohm-cm | Post Tensile Set; MIL-DTL-83528 Para.4.6.9 |
Parker Chomerics CHO-SEAL 1224 Conductive Elastomer Highest shielding effectiveness and through conductivity performance; higher physical properties; excellent processing; also available in a fabric reinforced format.Molded onlyRoHS CompliantInformat.. |
|||
Volume Resistivity | 0.010 ohm-cm | 0.010 ohm-cm | Post Tensile Set; MIL-G-83528 |
Parker Chomerics CHO-SEAL 1278 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Volume Resistivity | 0.010 ohm-cm | 0.010 ohm-cm | as supplied without pressure sensitive adhesive; MIL-DTL-83528 |
Parker Chomerics CHO-SEAL 1350 Conductive Elastomer Standard material for high volume injection and compression molding and small extrusions; high performance in non-corrosive environments; used in grounding applications with little or no vibration.R.. |
|||
Volume Resistivity | 0.010 ohm-cm | 0.010 ohm-cm | Post Tensile Set; MIL-DLT-83528 Para.4.6.9 |
Parker Chomerics CHO-SEAL 1350 Conductive Elastomer Standard material for high volume injection and compression molding and small extrusions; high performance in non-corrosive environments; used in grounding applications with little or no vibration.R.. |
|||
Volume Resistivity | 0.010 ohm-cm | 0.010 ohm-cm | as supplied without pressure sensitive adhesive; MIL-DTL-83528 |
Parker Chomerics CHO-SEAL 1401 Conductive Elastomer High performance for non-corrosive environments; soft(45 Shore A) for low closure force where gasket geometry cannot be exploited; low tear strength; no fluid resistance. Molded and ExtrudedRoHS Com.. |
|||
Volume Resistivity | <= 0.010 ohm-cm | <= 0.010 ohm-cm | |
Parker Chomerics Tecknit® 0002 Highly Conductive Adhesive-Sealant Silver Silicone Description: TECKNIT® 0002 is a pure silver filled, one component RTV silicone adhesive-sealant. It is ready to use without mixing and cures quickly at room temperature on exposure to moisture in .. |
|||
Volume Resistivity | <= 0.010 ohm-cm | <= 0.010 ohm-cm | |
Parker Chomerics Tecknit® 0035 Conductive Silicone Sealant/Adhesive Comments: Thin flexible pasteTypical Applications: Bonding elastomer gasketInformation provided by Chomerics |
|||
Volume Resistivity | <= 0.010 ohm-cm | <= 0.010 ohm-cm | |
Parker Chomerics Tecknit® 0236 Conductive Silicone Sealant/Adhesive Comments: Thick flexible pasteTypical Applications: Bonding Ag/Al elastomerInformation provided by Chomerics |
|||
Volume Resistivity | <= 0.010 ohm-cm | <= 0.010 ohm-cm | Cured; QA-1038 |
Parker Chomerics Tecknit® 72-00151 Silver-Filled Flexible Resin Caulking System Description: TECKNIT standard electrically conductive caulks consist of four one-component resin systems filled with silver plated glass or copper particles. These systems are formulated to provide .. |
|||
Volume Resistivity | <= 0.010 ohm-cm | <= 0.010 ohm-cm | Cured; QA-1038 |
Parker Chomerics Tecknit® 72-00152 Silver-Filled Flexible Resin Caulking System Description: TECKNIT standard electrically conductive caulks consist of four one-component resin systems filled with silver plated glass or copper particles. These systems are formulated to provide .. |
|||
Volume Resistivity | <= 0.010 ohm-cm | <= 0.010 ohm-cm | Cured; QA-1038 |
Parker Chomerics Tecknit CON/RTV-I One Part: Silver-Filled Silicone RTV Description: TECKNIT CON/RTV-I system is a pure silver loaded, one component RTV silicone adhesive sealant. It is ready to use without mixing and cures quickly at room temperature on exposure to moi.. |
|||
Volume Resistivity | <= 0.010 ohm-cm | <= 0.010 ohm-cm | |
Parker Chomerics Tecknit Consil®-C 875 Silver-Copper Filled Silicone Elastomer Description: CONSIL-C is a silicone or fluorosilicone elastomer filled with silver-plated copper particles designed to achieve maximum electrical conductivity. CONSIL-C provides one of the highest s.. |
|||
Volume Resistivity | <= 0.010 ohm-cm | <= 0.010 ohm-cm | |
Parker Chomerics Tecknit Consil®-II 842 Molded Silver-Filled Silicone Elastomer Description: CONSIL-II is a molded silicone elastomer filled with silver-coated inert particles. It provides high electrical conductivity, broadband shielding and moisture sealing. CONSIL-II is desi.. |
|||
Volume Resistivity | <= 0.010 ohm-cm | <= 0.010 ohm-cm | Cured; QAP-1017 |
Parker Chomerics Tecknit TeckBond™-A Silver-Plated Aluminum-Filled Adhesive Description: TECKBOND-A conductive system is a silicone based, two-component RTV, filled with silver-plated aluminum particles. After cure, the resultant bond or seal is flexible, resilient, and con.. |
|||
Volume Resistivity | <= 0.010 ohm-cm | <= 0.010 ohm-cm | |
Parker Chomerics Tecknit Teckfip™ HC FIP-C Formed in Place Conductive Elastomer Description: Heat cure compound. This compound is an all round high performance compound, and is very similar to a Consil C molded or extruded elastomer. It has been traditionally used for telecommu.. |
|||
Volume Resistivity | <= 0.010 ohm-cm | <= 0.010 ohm-cm | |
Parker Chomerics Tecknit Teckfip™ HC FIP-E Formed in Place Conductive Elastomer Heat cure compound. Commercial grade FIP compound designed for moderate shielding performance. The Ag/glass particles are very smooth which leads to very low compression set value.Information provid.. |
|||
Volume Resistivity | 0.010 - 1.0 ohm-cm | 0.010 - 1.0 ohm-cm | IEC 60093 |
Teijin Panlite® B-8130R Carbon Fiber Reinforced Polycarbonate Resin CF 30% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are low molding shrinkage and dimensional accuracy.Applica.. |
|||
Volume Resistivity | <= 0.010 ohm-cm | <= 0.010 ohm-cm | |
Master Bond EP79 Two Component, Silver Coated, Nickel Filled Conductive Epoxy Master Bond Polymer System EP79 is a two component, silver coated, nickel filled, electrically conductive adhesive for high performance bonding and sealing formulated to cure at room temperature or .. |
|||
Volume Resistivity | <= 0.010 ohm-cm | <= 0.010 ohm-cm | |
Master Bond EP79FL Two Component Silver Nickel Conductive Epoxy Adhesive Master Bond Polymer System EP79FL is a two component, silver-coated nickel, electrically conductive system for high performance bonding and sealing. Its most salient features are its high flexibilit.. |
|||
Volume Resistivity | 0.010 ohm-cm | 0.010 ohm-cm | cured 1 hr @ 65°C |
Tra-Con Tra-Duct 916H02 Room Temperature Cure, Conductive Silver Epoxy Adhesive TRA-DUCT 916H02 is an electrically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical pr.. |
|||
Volume Resistivity | <= 0.010 ohm-cm | <= 0.010 ohm-cm | |
Parker Chomerics CHO-BOND 1038 Conductive Silicone RTV Adhesive Electrically conductive, one component silicone adhesive/sealant that may be used for bonding EMI gaskets or for providing EMI and environmental protection as a caulk. This material cures on exposur.. |
|||
Volume Resistivity | 0.010 ohm-cm | 0.010 ohm-cm | as supplied without pressure sensitive adhesive; MIL-DTL-83528 |
Parker Chomerics CHO-SEAL 1217 Conductive Elastomer Resists highest level of EMP induced current; military gasket of choice in non-corrosive environments; excellent processing for molding and extrusion. Molded and ExtrudedRoHS Compliant Information p.. |
|||
Volume Resistivity | 0.010 ohm-cm | 0.010 ohm-cm | Post Tensile Set; MIL-G-83528. Para.4.6.9 |
Parker Chomerics CHO-SEAL 1221 Conductive Elastomer Highest shielding effectiveness and through conductivity performance; higher physical properties; excellent processing; also available in a fabric reinforced format.Molded onlyRoHS CompliantInformat.. |