Parker Chomerics CHO-SEAL 1350 Conductive Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone
Manufacturer Parker Chomerics
Trade Name CHO-SEAL
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-SEAL 1350 Conductive Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Standard material for high volume injection and compression molding and small extrusions; high performance in non-corrosive environments; used in grounding applications with little or no vibration.RoHS CompliantInformation provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 1.65 - 2.15 g/cc
1.65 - 2.15 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 58 - 72
58 - 72
ASTM D2240
Tensile Strength at Break >= 1.38 MPa
>= 200 psi
ASTM D412
Elongation at Break 100 - 300 %
100 - 300 %
ASTM D412
Tear Strength 5.250 kN/m
29.96 pli
ASTM D624
Compression Set >= 30 %

@Temperature 100 °C,
Time 252000 sec
>= 30 %

@Temperature 212 °F,
Time 70.0 hour
ASTM D395 Method B
Thermal Properties Metric English Comments
Thermal Conductivity 1.20 W/m-K

@Pressure 2.07 MPa
8.33 BTU-in/hr-ft²-°F

@Pressure 300 psi
ASTM D5470
Maximum Service Temperature, Air 160 °C
320 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Flex TR10; ASTM D1329
Electrical Properties Metric English Comments
Volume Resistivity 0.010 ohm-cm
0.010 ohm-cm
as supplied without pressure sensitive adhesive; MIL-DTL-83528
0.010 ohm-cm
0.010 ohm-cm
Post Tensile Set; MIL-DLT-83528 Para.4.6.9
Shielding Effectiveness >= 100 dB
>= 100 dB
100 MHz (E Field); MIL-G-83528
>= 50 dB

@Frequency 200000 Hz
>= 50 dB

@Frequency 200000 Hz
H Field; MIL-DTL-83528 Para.4.6.12
>= 75 dB

@Frequency 4.00e+10 Hz
>= 75 dB

@Frequency 4.00e+10 Hz
Plane Wave; MIL-DTL-83528 Para.4.6.12
>= 80 dB

@Frequency 1.00e+10 Hz
>= 80 dB

@Frequency 1.00e+10 Hz
Plane Wave; MIL-DTL-83528 Para.4.6.12
>= 90 dB

@Frequency 2.00e+9 Hz
>= 90 dB

@Frequency 2.00e+9 Hz
Plane Wave; MIL-DTL-83528 Para.4.6.12
>= 100 dB

@Frequency 1.00e+8 Hz
>= 100 dB

@Frequency 1.00e+8 Hz
E Field; MIL-DTL-83528 Para.4.6.12
>= 100 dB

@Frequency 5.00e+8 Hz
>= 100 dB

@Frequency 5.00e+8 Hz
E Field; MIL-DTL-83528 Para.4.6.12
Descriptive Properties Value Comments
Binder Silicone
Filler Ag/Glass
Heat Aging ohm-cm max 0.01
Type M
MIL-DTL-83528