Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 32.0 kV/mm | 813 kV/in | IEC 60243-1 |
Lanxess Durethan® BKV 330 H2.0 901510 Nylon 6, 30% Glass Fiber PA 6, injection molding type, 30% glass fibers, branched/structural viscosity, good weldability (vibration or hot plate), good heat-ageing resistance |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | ASTM D149 |
Solvay Specialty Polymers Polidan® EC/MD Polyethylene, Crosslinked (XLPE) Medium density polyethylene based compound crosslinkable by moisture; it consists of a silane pregrafted base compound (Sioplas® method) to be used with a catalyst masterbatch.Standards complying.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | IEC 60243 |
Teijin Panlite® LN-2250Y Flame Resistant, Translucent Polycarbonate Resin Flame retardant and mold release grade with normal fluidity, while maintaining intrinsic transparency of polycarbonate resin. It is suitable for injection molding applications.Applications:Electric,.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | IEC 60250 |
Polyram PlusTek PD1002NT Nylon 12 for Extrusion Medium viscosity Nylon 12 for extrusion application.Information provided by Polyram. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® BGZ-15 PA6-GF15 Information provided by EMS Grivory |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® HTM-4H1 PA6T/6I-MD40 Product description: Grivory HTM-4H1 is a 40 % mineral reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO: PA .. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® L 16 GM nat PA12 Grilamd L16 GM is a low-viscosity, non-reinforced PA 12 grade, UV- and heat-stabilized. The modification with a crystallization regulator causes a quick freeze and a fine, crystalline structure. Due.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® L 16 nat PA12 Low viscosity unmodified polyamide 12Information provided by EMS Grivory |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® L 25 nat 6112 PA12 Product Description: Grilamid L 25 natural 6112 is a high viscous, Polyamide 12 extrusion grade. Grilamid L 25 natural 6112 fulfils the requirements of DIN 73378, Type PA 12-H. Application examples:.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | AC Rapid Rise; ASTM D149 |
DuPont™ Nomex® 410 Paper, 10 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® LV-3A H PA12-GF30 Grilamid LV-3A H is a 30 % glass fibre reinforced PA12 for injection moulding. Grilamid LV-3A H is very stiff and tough and offers an improved hydrolysis resistance compared to standard PA12 GF 30.I.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® XE 4065 black 9238 PA*-GF50 Product description: Grivory XE 4065 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® XE 4128 black 9221 PA610 Product description: Grilamid XE 4128 black 9221 is a modified high viscosity Polyamide 610 for extrusion as well as injection molding. A characteristic of tubes made out of this material is the hig.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | IEC 60243-1 |
DuPont Performance Polymers Crastin® SK608 BK509 Polybutylene Terephthalate (PBT)
(Unverified Data**) 45% Glass Reinforced Polybutylene Terephthalate Crastin SK608 BK509 is a 45% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | ASTM D149, IEC 243 |
EPICHEM Epilac ABS Acrylonitrile Butadiene Styrene |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | IEC 60243-1 |
DuPont Performance Polymers Sorona® 3030G BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& 30% Glass Reinforced Polytrimethylene Terephthalate Sorona 3030G BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% polymer basis) with good .. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® L 20H FWA nat PA12 Product Description: Grilamid L 20 H FWA natural is a medium viscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 20 H FWA natural is used for technical injection molded parts.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® L 25 H PA12 Product Description: Grilamid L 25 H is a high viscosity heat stabilized Polyamide 12 extrusion grade and is suitable for application requiring a long-term usage temperature of 100 - 120°C. The mai.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® L 25 W 10 H X PA12 Product Description: Grilamid L 25 W 10 HX is a semi flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 10 HX is impact modified and heat and UV stabilized.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® L 25 W 20 PA12 Product Description: Grilamid L 25 W 20 is a semi-flexible plasticized high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 20 is UV and heat stabilized. The main features of Grila.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® L 25 W 40 HL X PA12-I Product Description: Grilamid L 25 W 40 HLX is a flexible Polyamide 12 grade with an excellent cold impact strength and heat stability. Grilamid L 25 W 40 HLX is specially suitable for flexible tube.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® L 25 W 40 NZ PA12-I Product Description: Grilamid L 25 W 40 NZ is a flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 NZ is impact modified and heat and UV stabilized. The.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® L 25 W 40 PA12 Product Description: Grilamid L 25 W 40 is a flexible, plasticised, high viscosity extrusion grade of Polyamide 12 (PA12) Grilamid L 25 W 40 is UV and heat stabilized. The main features of Grilamid .. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | IEC 243-1 |
Azoty Tarnow™ Tarnamid® T-27 GF50 Polyamide 6 - Glass Fiber Reinforced 50% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | IEC 243-1 |
Azoty Tarnow™ Tarnamid® T-27 GF30 Polyamide 6 - Glass Fiber Reinforced 30% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | in transformer oil; IEC 60243-1 |
CENTROPLAST CENTROMID 12 Polyamide 12 This extruded material has good impact resistance, low moisture absorption and good chemical resistance. It is used in precision elements, drive parts, cases and housingsInformation provided by CEN.. |
|||
Dielectric Strength | 32.0 kV/mm | 813 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® TR 55 LZ PA12/MACMI Product description: Grilamid TR grades are transparent thermoplastic polyamides based on aliphatic and cycloaliphatic blocks. Grilamid TR 55 LZ offers a variety of interesting properties such as: c.. |