Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 17.3 kV/mm | 440 kV/in | |
Resinlab® EP1320 Heat Cure Epoxy Conformal Coating Resinlab™ EP1320 and EP1320LV are one part heat cure epoxy conformal coatings. They can also be used as a small mass potting compounds, structural adhesives, or insulating polymer systems where the.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | |
Resinlab® EP1330LV Heat Cure Epoxy Polymer System Resinlab™ EP1330 and EP1330LV are one part heat cure epoxy polymer systems. They can also be used as a small mass potting or staking compounds, or a dam adhesive in and “dam and fill” application.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6/6 GF4 IM L LE Availability: North AmericaForms: PelletsAdditive: Lubricant and Impact ModifierFeatures: Lubricant, Low Extractables and Impact ModifiedAppearance: Natural ColorInformation provided by TP Composite.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6/6 GF43 IM L 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedTPCI# 6439.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6/6 IM 408 L Nylon 66 Availability: North AmericaForms: PelletsAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc... |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6/6 IM L W Nylon 66 Availability: North AmericaForms: PelletsAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc... |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill FR® PC IM FR Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6/6 GB36 IM1 36% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 36% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6/6 GF33 BK024 33% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Comp.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6/6,6 GF33 HS L BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricatedFeatures: LubricatedProcessing Method: Injection MoldingAppearance: .. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Luriblend® TPX-PA6-03034 Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber ReinforcementAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and Low FrictionAppearance: BlackInformation pro.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Plastiblend® PA6/6 GF40 IM HS L BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Plastiblend® PA6/6,6 IM 3757 Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedProcessing Method: Injection Mold.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6/6 GF33 IM HS L BKN 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6/6 IM 3757 HS L Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Fast Molding Cycle, High Flow, Heat Stabilized, Lubricant and Impact ModifiedProcessing Met.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6/6 IM X Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill FR® PA6/6 GF25 FR NAT003 25% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and LubricatedUL Fil.. |
|||
Dielectric Strength | >= 17.3 kV/mm @Thickness 3.17 mm |
>= 440 kV/in @Thickness 0.125 in |
|
Master Bond EP112 Low Viscosity Heat Curing Cycloaliphatic Epoxy Adhesive Master Bond Polymer System EP112 is a solventless, low viscosity two component cycloaliphatic epoxy resin system which is specifically designed for high performance outdoor and indoor electrical & e.. |
|||
Dielectric Strength | 17.3 kV/mm @Thickness 3.17 mm |
440 kV/in @Thickness 0.125 in |
|
Master Bond EP21LV-LO Two Component, Lower Viscosity, Room Temperature Curing Epoxy System Product Description: Master Bond EP21LV-LO is a two component, lower viscosity, room temperature curing epoxy system for high performance bonding, sealing, coating and encapsulation. This user frien.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | |
Master Bond EP30HT-LO NASA Low Outgassing, Optically Clear Coating Description: Master Bond EP30HT-LO is a moderate viscosity, two component epoxy adhesive formulated to cure at room temperature or more rapidly at elevated temperatures, with a four to one mix ratio.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | ASTM D149 |
Plastics Group Polifil® 628-33GF Glass Fiber-Reinforced Nylon 6/6 (DAM) Polifil® GFN/MRN 6/6 reinforced series of compounds offer superior strength, rigidity and creep resistance. Glass fibers provide excellent thermal and dimensional stability while maintaining good h.. |
|||
Dielectric Strength | 17.3 kV/mm @Thickness 3.17 mm |
440 kV/in @Thickness 0.125 in |
|
Master Bond EP21LSCL-1 Two Component, Room Temperature Curing Epoxy Resin Product Description: Master Bond Polymer System EP21LSCL-1 is a two component, low viscosity epoxy resin system featuring optical clarity as well as non-yellowing properties. This system can be used.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | |
Master Bond EP30LV Optically Clear, Low Viscosity Epoxy Adhesive Description: Master Bond Polymer System EP30LV is a low viscosity, two component epoxy adhesive for general purpose bonding, coating, sealing and casting formulated to cure at room temperature or mo.. |
|||
Dielectric Strength | >= 17.3 kV/mm @Thickness 3.17 mm |
>= 440 kV/in @Thickness 0.125 in |
|
Master Bond EP41SMed Two Component, Low Viscosity, USP Class VI Epoxy System Master Bond Polymer Adhesive EP41S Medical is a two component low viscosity epoxy resin system for high performance bonding, sealing, coating, as well as small encapsulations, pottings and castings... |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | ASTM D149 |
Arlon 55589G028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Green silicone gum and rubber on fiberglass Th.. |
|||
Dielectric Strength | >= 17.3 kV/mm | >= 440 kV/in | |
Arlon 44250R011 0.011" (0.279 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. The data should not be used to wri.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | |
Resinlab® EP1026HP Epoxy Adhesive Resinlab™ EP1026HP is a high performance fast setting epoxy adhesive designed for bonding metals, ceramics, glass and most plastics. This product gives good resistance to water salt spray, inorgan.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill FR® PPO/HIPS MM20 FR 20% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 20% Filler by Weight Features: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | ASTM D149 |
Owens Corning Glass Fiber Reinforced Polypropylene, 20 wt.% glass Polypropylene provides good resistance to acids, alkalis and organic solvents even at higher temperatures. It is, however, soluble in chlorinated hydrocarbons. Data provided by the manufacturer, Ow.. |
|||
Dielectric Strength | 17.3 kV/mm | 440 kV/in | |
Resinlab® EP1121 Black Electronic Grade Epoxy Encapsulant Resinlab™ EP1121 Black is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexible polymer. I.. |