Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 13.8 kV/mm | 351 kV/in | ASTM D149 |
Plenco 7000 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok 7000 is the replacement material for the former Union Carbide BMM-7000. It is a two-stage, woodflour-filled phenolic molding compound having versatile molding and preheating characteristics.. |
|||
Dielectric Strength | 13.8 kV/mm | 351 kV/in | ASTM D149 |
IDI Composites C-210 Thermoset Polyester, Sheet CORROSION - (Patent pending). Versatile family of compounds designed for pressurized and thermo-mechanically stressed applications. Excellent corrosion resistance and high strength.Data provided by .. |
|||
Dielectric Strength | 13.8 kV/mm | 351 kV/in | Step by step; ASTM D149 |
Sumitomo Bakelite Durez® 118 Phenolic, Compression Grade Durez 118 Black Phenolic is a two-stage, asbestos free, general purpose molding material. It exhibits improved impact strength and resistance to flexural fatigue for demanding automotive, electrica.. |
|||
Dielectric Strength | 13.8 kV/mm | 351 kV/in | Short Time; ASTM D149 |
Sumitomo Bakelite Durez® 152 Phenolic, Injection Grade Durez 152 Phenolic is a two-stage, heat resistant/electrical molding material. It exhibits superior dimensional stability, good strength retention at elevated temperature and good molded appearance.. |
|||
Dielectric Strength | 13.8 kV/mm | 351 kV/in | Short Time; ASTM D149 |
Sumitomo Bakelite Durez® 153 Phenolic, Injection Grade Durez 153 Black Phenolic is a two-stage, asbestos-free, heat resistant/electrical molding material. It exhibits good molded appearance and shock resistance for use on a wide variety of electrical a.. |
|||
Dielectric Strength | 13.8 kV/mm | 351 kV/in | Short Time; ASTM D149 |
Sumitomo Bakelite Durez® 156 Phenolic, Injection Grade Durez 156 Black Phenolic is a two-stage, asbestos-free, heat resistant/electrical molding material. It exhibits excellent dimensional stability, high heat resistance, good molded appearance, and UL.. |
|||
Dielectric Strength | 13.8 kV/mm | 351 kV/in | Short Time; ASTM D149 |
Sumitomo Bakelite Durez® 29502 B Phenolic, Compression Grade Durez 29502 B brown phenolic is a two stage, glass and mineral filled, special purpose molding material with improved mechanical and heat resistant properties. It is formulated for close tolerance .. |
|||
Dielectric Strength | 13.8 kV/mm | 351 kV/in | Wet, step-by-step. ASTM D149 |
Sumitomo Bakelite North America 52-01 Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG.Inf.. |
|||
Dielectric Strength | 13.8 kV/mm | 351 kV/in | Wet, step-by-step. ASTM D149 |
Sumitomo Bakelite North America 52-70-70-VO-P Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Conforms with the requirements of ASTM D5948 Type.. |
|||
Dielectric Strength | 13.8 kV/mm @Frequency 60.0 Hz |
351 kV/in @Frequency 60.0 Hz |
Wet, step by step; ASTM D149 |
Sumitomo Bakelite North America 73-70-70 C-P /73-70-70 VO-P Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG-F.I.. |
|||
Dielectric Strength | 13.8 kV/mm | 351 kV/in | step-by-step; ASTM D149 |
Sumitomo Bakelite Durez® 32245 Phenolic, Compression Grade Durez 32245 Black Phenolic is a two-stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional stabilit.. |
|||
Dielectric Strength | 13.8 kV/mm | 351 kV/in | step-by-step; ASTM D149 |
Sumitomo Bakelite Durez® 32245 Phenolic, Injection Grade Durez 32245 Black Phenolic is a two-stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional stabilit.. |
|||
Dielectric Strength | 13.8 kV/mm | 351 kV/in | ASTM D149 |
Chang Chun Plastic Longlite PM T310 Impact Phenolic Molding Compound ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd. |
|||
Dielectric Strength | 13.8 kV/mm | 351 kV/in | ASTM D149 |
Chang Chun Plastic Longlite PM T355J Impact Phenolic Molding Compound ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd. |
|||
Dielectric Strength | 13.8 kV/mm | 351 kV/in | ASTM D149 |
Chang Chun Plastic Longlite PM T376J Heat Resistant Phenolic Molding Compound ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd. |
|||
Dielectric Strength | 13.8 - 15.8 kV/mm | 351 - 401 kV/in | short time |
Bulk Molding Compounds BMC T10(14) General Purpose Molding Compound BMC T10(14) is a general purpose, low shrink molding compound. Due to the excellent flow and controlled reactivity, BMC T10(14) is well suited for injection, transfer or compression molding of intr.. |
|||
Dielectric Strength | 13.8 kV/mm | 351 kV/in | ASTM D149 |
Plaslok 7000 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 7000 is the replacement material for .. |
|||
Dielectric Strength | 13.8 kV/mm | 351 kV/in | ASTM D149 |
Chang Chun Plastic Longlite PM T375J Heat Resistant Phenolic Molding Compound ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd. |
|||
Dielectric Strength | 13.8 kV/mm | 351 kV/in | 60 Hz, wet, SS; ASTM D149 |
Sumitomo Bakelite North America FM 4017F Fiberglass and Mineral Reinforced Phenolic FM 4017F is a fiberglass and mineral reinforced phenolic molding compound, with excellent dimensional stability and good strength at elevated temperatures. Information supplied by Sumitomo Bak North.. |