Electrical Properties Metric English Comments
Dielectric Strength >= 3.00 kV/mm
>= 76.2 kV/in
Paratherm Corporation Paratherm™ HE Heat Transfer Fluid
Paratherm HE® is a high flash and fire point heat transfer fluid. Engineered for higher thermal and oxidative stability, it is efficient and cost effective. Its greater purity allows it to strong..
Dielectric Strength 3.00 - 4.00 kV/mm

@Temperature 20.0 °C
76.2 - 102 kV/in

@Temperature 68.0 °F
ASTM D877
Paratherm Corporation Paratherm™ NF Heat Transfer Fluid
Description: Paratherm NF® heat transfer fluid is highly efficient, thermally stable and cost-effective. It is also non-fouling, low pour and odor free. Completely non-toxic, it is exceptionally ..
Dielectric Strength 3.00 kV/mm

@Thickness 2.00 mm
76.2 kV/in

@Thickness 0.0787 in
IEC 243-1
LATI LATAN 13 K/30 30% Carbon Fiber Reinforced Polyoxymethylene Copolymer (POM)  (Unverified Data**)
Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea..
Dielectric Strength 3.00 - 37.0 kV/mm
76.2 - 940 kV/in
Average value: 18.3 kV/mm Grade Count:24
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum..
Dielectric Strength 3.00 kV/mm
76.2 kV/in
AC 60 Hz
Fujipoly Industries Sarcon® 15GHR Thin-Film GHR
Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of ..
Dielectric Strength 3.00 kV/mm
76.2 kV/in
150°C for 1,000 hrs
Fujipoly Industries Sarcon® 15GHR Thin-Film GHR
Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of ..
Dielectric Strength 3.00 kV/mm
76.2 kV/in
60°C for 500 hrs
Fujipoly Industries Sarcon® 15GTR Thin-Film GTR
Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of ..
Dielectric Strength 3.00 kV/mm
76.2 kV/in
AC 60 Hz; 200°C for 1,000 hrs
Fujipoly Industries Sarcon® 15GTR Thin-Film GTR
Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of ..
Dielectric Strength 3.00 kV/mm
76.2 kV/in
1 in. axial in oil; ASTM D149
Glastic Laminates/Shapes HIR Grade HIR Fiberglass-Reinforced Polyester Rod
Data provided by Glastic Corporation.A continuous-filament fiberglass-roving provides superior strength. Highest physical properties of GLASROD series.
Dielectric Strength 3.00 kV/mm
76.2 kV/in
1 in. axial in oil; ASTM D149
Glastic Laminates/Shapes MTS Grade MTS Fiberglass-Reinforced Polyester Rod
Data provided by Glastic Corporation.A continuous-filament fiberglass-roving provides superior strength.
Dielectric Strength 3.00 kV/mm
76.2 kV/in
1 in. axial in oil; ASTM D149
Glastic Laminates/Shapes SG-200 Fiberglass-Reinforced Polyester Rod
Data provided by Glastic Corporation.A continuous-filament fiberglass-roving provides superior strength. Excellent thermal endurance - used to replace silicone rod.
Dielectric Strength 3.00 kV/mm
76.2 kV/in
NF EN 60243.1
Isoflon Tisoflon® 3 AD Polytetrafluoroethylene Coated Glass Fabric
PTFE coated glass fabric one side adhesive TISOFLON® - Standard gradeInformation provided by Isoflon.
Dielectric Strength 3.00 kV/mm
76.2 kV/in
ASTM D149
Tipco Tipcolite® TMS 111 Phenolic Compound, Cellulose Pulp, in fluffy form, having Soft Flow & High Strength
Soft Flow Phenolic Compound, Reinforced with Cellulose Pulp, in fluffy formApplications: Defence ApplicationsProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industrie..
Dielectric Strength 3.00 kV/mm

@Thickness 3.00 mm
76.2 kV/in

@Thickness 0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60243-1; IEC/EN 61212-2 6.1.2.1
Elektro-Isola Etronax DN Phenolic, Cotton Fabric Reinforcement, Brown, Tubes
Description: A strong and tough material. Very low water absorption and the lowest swelling in water. Very good low-friction material. High wear resistance in aggressive and dust-filled environments..
Dielectric Strength 3.00 kV/mm

@Thickness 3.00 mm
76.2 kV/in

@Thickness 0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60243-1; IEC/EN 61212-2 6.1.2.1
Elektro-Isola Etronax MMF Phenolic, Cotton Fabric Reinforcement, Brown, Tubes
Description: Mechanical applications. Reinforced with finer fabric than Etronax MF. Can be used, in particular, for mechanical applications where fine tolerances and smoother surface finish are requ..
Dielectric Strength 3.00 kV/mm
76.2 kV/in
dry; IEC 60243-1
EMS-Grivory Grivory® HT2C-3X LF black 9833 PA6T/66-CF30
Product description: Grivory HT2C-3X LF black 9833 is a 30% carbon-fibre reinforced, PTFE modified engineering thermoplastic based on semicrystalline partially aromatic copolyamide. Polymer designat..
Dielectric Strength 3.00 kV/mm
76.2 kV/in
conditioned; IEC 60243-1
EMS-Grivory Grivory® HT2C-3X LF black 9833 PA6T/66-CF30
Product description: Grivory HT2C-3X LF black 9833 is a 30% carbon-fibre reinforced, PTFE modified engineering thermoplastic based on semicrystalline partially aromatic copolyamide. Polymer designat..
Dielectric Strength 3.00 kV/mm
76.2 kV/in
dry; IEC 60243-1
EMS-Grivory Grivory® XE 4102 black 9238 PA*-CF30
Grivory XE 4102 is a 30% carbon fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partially based on renewab..
Dielectric Strength 3.00 kV/mm
76.2 kV/in
conditioned; IEC 60243-1
EMS-Grivory Grivory® XE 4102 black 9238 PA*-CF30
Grivory XE 4102 is a 30% carbon fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partially based on renewab..
Dielectric Strength 3.00 kV/mm
76.2 kV/in
Accuratus Accuflect™ Light-Reflecting Ceramic
Accuflect™ is a specially formulated and processed ceramic developed by Accuratus to satisfy the market demand for diffuse reflectors in high temperature and high energy environments.Key Property: ..
Dielectric Strength 3.00 - 4.50 kV/mm

@Temperature 90.0 °C
76.2 - 114 kV/in

@Temperature 194 °F
IS 2584-1963
Amity Thermosets ATG 115 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- Black, BrownSoft/medium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic ..
Dielectric Strength 3.00 - 5.00 kV/mm

@Temperature 90.0 °C
76.2 - 127 kV/in

@Temperature 194 °F
IS 2584-1963
Amity Thermosets ATM 125 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Glossy surface free of filler marks Surface good & free of flaws Good mouldabilitySurface free of filler marks even after turningGood mechanical strengthColor-black, brownSoft/medium..
Dielectric Strength 3.00 - 5.00 kV/mm

@Temperature 90.0 °C
76.2 - 127 kV/in

@Temperature 194 °F
IS 2584-1963
Amity Thermosets ATG 116 Phenolic Molding Organic and inorganic Filler, Compression Molded
Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- BlackMedium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic appliance ha..
Dielectric Strength 3.00 kV/mm
76.2 kV/in
Von Roll Isola IMI Varnish 3405 Polyester Varnish for Electrical Insulation
Data provided by Von Roll Isola USA.Flash Point:
Dielectric Strength 3.00 - 23.0 kV/mm
76.2 - 584 kV/in
Average value: 12.4 kV/mm Grade Count:4