Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 18.0 kV/mm | 457 kV/in | |
Multibase TPSiV™ 3010-60A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | 50% RH; IEC 60243-1 |
Murtfeldt Murylon® A Nylon 66 This material combines the excellent properties of the Murylon® range with additional high tensile and compressive strength, increased wear resistance, and a lower level of moisture absorption than.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | in oil; ASTM D149 |
PTS PBT-20GFR 20% Glass Filled PBT, injection molding grade, 20% glass fiber reinforced, flame retardant, exceptional flowability and processability, colorable.Information provided by PTS LLC. |
|||
Dielectric Strength | 18.0 kV/mm @Temperature 23.0 °C |
457 kV/in @Temperature 73.4 °F |
IEC 60243-1 |
DuPont Performance Polymers Hytrel® 4069 TPC-ET
(Unverified Data**) Hytrel® 4069 is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injection.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 2.00 mm |
457 kV/in @Thickness 0.0787 in |
ASTM D149 |
Nilit Nilamid B3 H ZB Unfilled, Low Temperature Impact Resistant PA6 Description: Nilamid B3 H ZB is a high impact NYLON 6. The product has excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas inclu.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | ASTM D149 |
Plaskolite Optix® PL-200 Acrylic Resin
(discontinued **) Injection molding grade pellets.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | ASTM D149 |
Solvay Specialty Polymers Ryton® BR111BL Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® BR111BL is a glass and mineral filled polyphenylene sulfide compounds developed to provide a good combination of mechanical strength and electrical proper.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | JIS-K-6249; ASTM D-149 |
Fujipoly Industries Sarcon® GR-n Gap Filler Pad Sarcon GR-n is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | 60°C for 1,000 hrs with 90% RH; JIS-K-6249 |
Fujipoly Industries Sarcon® GR-n Gap Filler Pad Sarcon GR-n is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | JIS-K-6249; ASTM D-149 |
Fujipoly Industries Sarcon® XR-e Gap Filler Pad Sarcon XR-e and XR-j are highly conformable/thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of compon.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | IEC 60243-1 |
Mitsubishi Xantar® MX 1021 FD MX 1021 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 1.59 mm |
457 kV/in @Thickness 0.0625 in |
Perpendicular, Short Time in Oil and Air; ASTM D149 |
Haysite ETR-FR-C Glass Reinforced Polyester Sheet, Electrical Grade (GPO3) ETR-FR-C meets NEMA GPO-3 requirements and exceeds NEMA in dielectric strength, arc resistance, and track resistance. This U.L. recognized grade is highly flame retardant and low smoke generating. E.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | ASTM D149 |
Solvay Specialty Polymers Ryton® BR111BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® BR111BL Ryton® BR111 is a black-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outs.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | Wet, short term. ASTM D149 |
Sumitomo Bakelite North America RX® 3-2-520F-P Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SI.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | IEC 60243-1 |
Polyplastics Duracon® SF-20 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm, Temperature 23.0 °C |
457 kV/in @Thickness 0.126 in, Temperature 73.4 °F |
Short Time; ASTM D149 |
DuPont Performance Polymers Delrin® 111P NC010 Acetal Homopolymer Delrin® 111P is a high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, fewer voids). It has higher tensile strength and mod.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | |
Arkema Group Rilsan® BESN P40 W5 TL Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11-P,EFHL,22-003Flexible grade for tubes extrusion. Available color: milky white. Light and heat stabilized. Flame retardant agent.Fire-resistant. Flexibility. High impact str.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | |
AGY ZenTron® S-2 Generic S-Glass Fiber S-2 glass and S-glass have the same composition. S-glass is no longer made by AGY, but used to have a reactive epoxy size. Various silanes and starch oil are used as binders. Acid resistant. Mod.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS (Asia Pacific) NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. This grade has been certified for potable water applications up to 85C in Europe and North America, color .. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 2.00 mm |
457 kV/in @Thickness 0.0787 in |
ASTM D149 |
Chang Chun Plastic PBT2100 Fire Retardant PBT Information provided by Dowell Trading Company Ltd. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | IEC 60243 |
Solvay TECHNYL® 1015CR PA6, Conditioned Description: Polyamide 6, unfilled, standard for fast injection cycles, for injection molding Available in: Asia Pacific Product Applications: TECHNYL® 1015CR has high fluidity and a good mould re.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | IEC 60243 |
Solvay TECHNYL® 1021ST PA6, Conditioned Description: Polyamide 6, unfilled, super tough impact modified, for injection moldingAvailable in: Asia Pacific Product Applications: TECHNYL® 102ST has the highest level impact strength and balan.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | IEC 243/1 |
BASF Ultradur® B 4040 G4 20% Glass Filled PBT + PET PBT + PET, injection-molding grade containing 20% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor housin.. |
|||
Dielectric Strength | 18.0 kV/mm | 457 kV/in | Short Time; ASTM D149 |
Plenco 50030 PET, Pellet, Injection Molded, Natural Color
(discontinued **) PLENCO 50030 is an engineering grade glass reinforced polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in white, natural, and black.Information sup.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 2.00 mm |
457 kV/in @Thickness 0.0787 in |
IEC 60243 |
Manifattura Cattaneo POM c+PTFE Acetal, PTFE Filled Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |