Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 16.9 kV/mm | 430 kV/in | ASTM D149 |
Ravago Manufacturing Americas Hylex® P1010G10FRMA Polycarbonate, 10% Glass Filled Polycarbonate, 10% Glass Filled, Flame RetardantInformation provided by Ravago. |
|||
Dielectric Strength | 16.9 kV/mm @Thickness 3.17 mm |
430 kV/in @Thickness 0.125 in |
in air; ASTM D149 |
Ravago Manufacturing Americas Hylex® P1310G30 HB Polycarbonate, 30% Fiberglass Reinforced, UV Stabilized Information provided by Ravago. |
|||
Dielectric Strength | 16.9 - 47.5 kV/mm | 430 - 1210 kV/in | Average value: 29.2 kV/mm Grade Count:26 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Dielectric Strength | 16.9 - 24.0 kV/mm | 430 - 610 kV/in | Average value: 21.2 kV/mm Grade Count:4 |
Overview of materials for Nylon 66, 10% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ.. |
|||
Dielectric Strength | >= 16.9 kV/mm | >= 430 kV/in | ASTM D149 |
KYDEX® 100 Acrylic/PVC Thermoplastic Sheet High impact fire rated sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones. Hidden parts for equipment such as vending machines.. |
|||
Dielectric Strength | 16.9 kV/mm @Thickness 3.20 mm |
429 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® EH7020 PBT MINERAL FILLED, METALLIZABLE |
|||
Dielectric Strength | 16.9 kV/mm | 430 kV/in | |
Saint-Gobain CHR® G569 Glass Cloth Backing Acrylic Adhesive Pressure Sensitive Tape Description: Glass cloth offers excellent abrasion resistance and mechanical properties, as well as high tensile strength and extreme temperature resistance. Service temperatures range from -100°.. |
|||
Dielectric Strength | 16.9 kV/mm | 430 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PSU GF10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 16.9 kV/mm | 430 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Luriblend® PSU GF20 TL5 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 16.9 kV/mm | 430 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Luriblend® TPX-PA6/6-01072 Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral FillerAdditive: Molybdenum Disulfide LubricantFeatures: Lubricated, Low Friction and Good Wear ResistanceInformation provided b.. |
|||
Dielectric Strength | 16.9 kV/mm @Thickness 3.00 mm |
430 kV/in @Thickness 0.118 in |
ASTM D149 |
Teknor Apex Chemlon® 104 Nylon 66, Impact Grade Notes: Medium-Impact; General Purpose; Impact modified to provide excellent toughness Processing Method: Injection Molding Forms: Pellets Automotive Specifications: Chrysler MS-DB41 CPN3992 Color: W.. |
|||
Dielectric Strength | 16.9 kV/mm | 430 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill FR® PC FR UG X GY158 Availability: North AmericaForms: PelletsAdditive: Mold ReleaseFeatures: Flame Retardant and Good Mold ReleaseAppearance: GreyInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 16.9 kV/mm | 430 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PSU GF20 BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 16.9 kV/mm @Frequency 60.0 Hz |
429 kV/in @Frequency 60.0 Hz |
Wet, step by step; ASTM D149 |
Sumitomo Bakelite North America 52-40-40-P Long-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type GDI-30F.. |
|||
Dielectric Strength | 16.9 kV/mm | 430 kV/in | |
Tra-Con Tra-Bond F113 High Impact Optically Clear Epoxy Adhesive TRA-BOND F113 is an optically clear, low viscosity, high impact epoxy adhesive developed for bonding and small volume potting of plastic or glass optical fibers, lenses, and prisms, LED displays, an.. |
|||
Dielectric Strength | 16.9 kV/mm | 430 kV/in | |
Tra-Con Tra-Bond FS482 Long Pot Life High Tg Fiber Optic Epoxy Adhesive TRA-BOND FS-482 is a dark blue, low viscosity epoxy adhesive developed for fiber-optic bonding and small volume potting of plastic or glass optical fibers, lenses and prisms, LED displays, and other.. |
|||
Dielectric Strength | 16.9 kV/mm | 430 kV/in | |
Tra-Con Tra-Bond 2110 High Impact Epoxy Staking Compound TRA-BOND 2110 is a thixotropic epoxy resin and hardener formulation developed for industrial adhesive, staking, laminating, repair and manufacturing applications where long pot-life, good wetting, n.. |
|||
Dielectric Strength | 16.9 kV/mm | 430 kV/in | |
Trelleborg Emerson & Cuming Stycast® 1269A Two-Component Easy Mix Ratio Encapsulant Features and Typical ApplicationsPrimarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, .. |
|||
Dielectric Strength | 16.9 kV/mm | 430 kV/in | |
Dow Corning 1890 PROTECTIVE COATING Silicone RTV in solvent dispersionInformation provided by Dow Corning |
|||
Dielectric Strength | 16.9 kV/mm | 430 kV/in | ASTM D149 |
Arlon 56976XA026 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 1: cured silicone rubber; Substrate: 1564 fiberglass; Side 2: uncured silicone rubber |
|||
Dielectric Strength | 16.9 kV/mm | 430 kV/in | IPC TM-650 2.5.6.2 |
Arlon AD300C Commercial Microwave and RF Laminate Material Excellent Thermal Coefficient of Dielectric Constant (TCEr = -25 ppm/°C)Excellent PIM performanceHigh Thermal Conductivity ideal for Higher Power DesignsReduced Coefficient of Thermal Expansion in .. |
|||
Dielectric Strength | 16.9 kV/mm | 430 kV/in | ASTM D149 |
Arlon LW401A##-P3 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 40 mil thick, Blue, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length .. |
|||
Dielectric Strength | 16.9 kV/mm @Thickness 1.65 mm |
428 kV/in @Thickness 0.0650 in |
|
3M RJS--1 3/C Phase Rejacketing System 3M RJS Series Rejacking Sleeves are dinged so that 3M Cold Shrink QTII and QTIII Silicone Rubber Termination applications can be used on 3/C (three conductor) medium voltage shielded power cables of.. |
|||
Dielectric Strength | 16.9 kV/mm @Thickness 1.65 mm |
428 kV/in @Thickness 0.0650 in |
|
3M RJS-4 3/C Phase Rejacketing System 3M RJS Series Rejacking Sleeves are dinged so that 3M Cold Shrink QTII and QTIII Silicone Rubber Termination applications can be used on 3/C (three conductor) medium voltage shielded power cables of.. |
|||
Dielectric Strength | 16.9 kV/mm | 430 kV/in | |
Atom Adhesives AA-BOND F113 Epoxy Adhesive AA-BOND F113 is an Optically Clear, low viscosity , High impact epoxy adhesives developed for bonding and small volume potting of plastic or glass optical fibers, lenses and prisms, LED displays, an.. |
|||
Dielectric Strength | 16.9 kV/mm | 430 kV/in | perp |
Bulk Molding Compounds BMC 1605 Low Shrink, Medium Strength BMC 1605 is an excellent low-cost HB material with low shrink and medium strength. Has excellent surface finish and gloss. Can be injection, compression or transfer molded. UL® recognized. This mat.. |