Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 14.2 kV/mm | 360 kV/in | ASTM D149 |
Quadrant EPP Quadrant PPSU LSG PPSU, Extruded, Unfilled, Polyphenylsulfone (ASTM Product Data Sheet) |
|||
Dielectric Strength | 14.2 kV/mm @Thickness 3.17 mm |
361 kV/in @Thickness 0.125 in |
ASTM D149 |
ExxonMobil Escorene® LD-402 LDPE Electrical Jacketing Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A low density polyethylene homopolymer resin designed for high speed extrusions. |
|||
Dielectric Strength | 14.2 kV/mm | 361 kV/in | ASTM D149 |
Plaslok 201 Black General Purpose Woodflour/Mineral Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 201 is a two-stage, woodflour and min.. |
|||
Dielectric Strength | 14.2 kV/mm | 360 kV/in | ASTM D149 |
Mar-Bal MB3000-15NY Thermoset Polyester Composite Molding Compound A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Dielectric Strength | 14.2 kV/mm | 360 kV/in | ASTM D149 |
Mar-Bal MB3000-20NY Thermoset Polyester Composite Molding Compound A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Dielectric Strength | 14.2 kV/mm | 361 kV/in | ASTM D149 |
IDI Composites A-207 Thermoset Polyester, Sheet AUTOMOTIVE - Versatile family of compounds specifically designed for automotive structural applications. Low shrink characteristics, heat resistance, long-term dimensional stability, and corrosion r.. |
|||
Dielectric Strength | 14.2 kV/mm | 361 kV/in | ASTM D149 |
IDI Composites E-205 Thermoset Polyester, Sheet ELECTRICAL - U.L. recognized (E53587). Versatile family of compounds designed to meet the most demanding electrical and electronic applications. Excellent dielectric properties and arc/track resista.. |
|||
Dielectric Strength | 14.2 kV/mm @Thickness 3.00 mm |
360 kV/in @Thickness 0.118 in |
ASTM D149 |
Teknor Apex Chemlon® 223 Nylon 6, Unreinforced Features: Nucleated for fast cyclingProcessing Method: Injection MoldingForms: Pellets Additive: Nucleating AgentInformation Provided by Teknor Apex |
|||
Dielectric Strength | 14.2 kV/mm @Frequency 60.0 Hz |
361 kV/in @Frequency 60.0 Hz |
short time, dry; ASTM D149 |
Sumitomo Bakelite North America E 2748A Short Glass Fiber Reinforced Epoxy E 2748A is a glass reinforced epoxy molding compound, with good impact strength combined with soft flow for the encapsulation of devices requiring high quality and thermal shock resistance.Informati.. |
|||
Dielectric Strength | 14.2 kV/mm | 361 kV/in | Short Time; ASTM D149 |
Plenco 2308 Phenolic, Granular, Compression Molded PLENCO 02308 is a general purpose organic filled phenolic molding compound, offering improved heat resistance and optimized cure properties. UL recognized under component file E40654. 02308 is avai.. |
|||
Dielectric Strength | 14.2 kV/mm | 361 kV/in | Short Time; ASTM D149 |
Plenco 2408 Phenolic, Granular, Compression Molded PLENCO 02408 is a general purpose, organic filled phenolic molding compound, offering excellent cosmetic characteristics and improved electrical strength properties. UL recognized under component fi.. |
|||
Dielectric Strength | 14.2 kV/mm | 360 kV/in | ASTM D149 |
Westlake Plastics Radel® R 5500 Polyphenylsulfone Stock shapes extruded from Radel R resins offer a superior combination of high performance properties that include excellent thermal stability, outstanding toughness, and good environmental stress c.. |
|||
Dielectric Strength | 14.2 kV/mm | 360 kV/in | |
Tra-Con Tra-Bond 2162D Color Coded Smooth Paste Epoxy Adhesive TRA-BOND 2162D epoxy system is color-coded for easy mixing and handling as a smooth paste, and it develops strong bonds to most materials including metals, glass, ceramics, leather, wood, concrete a.. |
|||
Dielectric Strength | 14.2 kV/mm | 360 kV/in | |
Trelleborg Emerson & Cuming Stycast® XT-1122 Two-Component Epoxy Flexible Encapsulant Emerson & Cuming XT-1122 Stycast® Two-Component Epoxy Flexible EncapsulantHeat, thermal shock and impact resistance. Good chemical resistance, Low Viscosity, Unfilled. Mix Ratio (by weight) = 100:6.. |
|||
Dielectric Strength | 14.2 kV/mm | 360 kV/in | ASTM D149 |
Ensinger TECASON™ P MT Polyphenylsulfone (PPSU) TECASON™ P MT is a polyphenylsulfone suited primarily to applications in the medical industry. It has improved performance in terms of temperature, impact strength and chemical resistance, as well.. |
|||
Dielectric Strength | 14.2 kV/mm | 360 kV/in | ASTM D149 |
Ensinger TECASON™ P Polyphenylsulfone (PPSU) TECASON™ P is a polyphenylsulfone that exhibits excellent temperature, impact and chemical resistance properties. |
|||
Dielectric Strength | 14.2 kV/mm | 360 kV/in | ASTM D149 |
Ensinger RADEL® R-5500 Polyphenylsulfone (PPSU) RADEL® R is a Polyphenysulfone produced by Solvay Advanced Polymers. RADEL® R is in the same performance category as products like Polysulfone and ULTEM® (PEI). RADEL® R has increased performa.. |
|||
Dielectric Strength | 14.2 kV/mm | 360 kV/in | ASTM D149 |
AdvanSource Biomaterials ChronoFlex® C 80A Biodurable Medical Grade Polyurethane ChronoFlex® C is a family of premium polycarbonate aromatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® C medical-grade elastome.. |
|||
Dielectric Strength | >= 14.2 kV/mm | >= 360 kV/in | Cured property; 0.1 inch; ASTM D149 |
Aptek 2100-A7C/B Low modulus urethane staking compound APTEK 2100-A7C/B is a thixotropic, two component, electrically insulating, low modulus urethane system designed for the staking of electrical/electronic components to printed circuit boards. Althoug.. |
|||
Dielectric Strength | 14.2 kV/mm | 360 kV/in | |
Bulk Molding Compounds BMC 610 Mineral filled, glass-fiber-reinforced polyester compound BMC 610 molding compound is a mineral filled, glass fiber reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is set a part form other medium impact.. |
|||
Dielectric Strength | 14.2 kV/mm | 360 kV/in | Short Time |
Bulk Molding Compounds BMC 620 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, and stuffer injection molding It is characterized by good moldability high impact st.. |
|||
Dielectric Strength | 14.2 kV/mm | 360 kV/in | Short Time |
Bulk Molding Compounds BMC 620M Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620M molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, and stuffer injection molding It is characterized by high impact strength, good mol.. |
|||
Dielectric Strength | 14.2 - 30.0 kV/mm | 360 - 762 kV/in | Average value: 18.5 kV/mm Grade Count:14 |
Overview of materials for Nylon 6, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Dielectric Strength | 14.2 - 19.7 kV/mm | 360 - 500 kV/in | Average value: 17.0 kV/mm Grade Count:7 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi.. |
|||
Dielectric Strength | 14.2 kV/mm @Thickness 1.60 mm |
361 kV/in @Thickness 0.0630 in |
ASTM D149 |
E-Polymers SEPAZ® K115HF 15% Glass Fiber Reinforced High Flow PPS Resin Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit.. |