Electrical Properties Metric English Comments
High Voltage Arc-Tracking Rate, HVTR 14.0 mm/min
0.551 in/min
UL 746
Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA)  (Unverified Data**)
Amodel AE-4133 is a 33% glass reinforced, hot-water moldable polyphthalamide (PPA) designed to work in the modern automotive electrical environment. This grade features a high heat deflection temper..
High Voltage Arc-Tracking Rate, HVTR 14.0 mm/min
0.551 in/min
UL 746
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Typical applications include ..
High Voltage Arc-Tracking Rate, HVTR 14.0 mm/min
0.551 in/min
UL 746
Solvay Specialty Polymers Amodel® A-4133 HH Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® A-4133 HH is a 33% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation ..
High Voltage Arc-Tracking Rate, HVTR 14.0 mm/min
0.551 in/min
UL 746
Solvay Specialty Polymers Amodel® A-4145 HH Polyphthalamide (PPA), 45% Glass Fiber (Dry)
Amodel® A-4145 HH is a 45% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation ..
High Voltage Arc-Tracking Rate, HVTR 14.0 mm/min
0.551 in/min
UL 746
Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AE-4133 is a 33% glass reinforced, hot-water moldable polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Good Chemical Resistance; Good Cree..
High Voltage Arc-Tracking Rate, HVTR 14.0 mm/min
0.551 in/min
UL 746
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Testing conducted on samp..
High Voltage Arc-Tracking Rate, HVTR 14.0 mm/min
0.551 in/min
UL 746
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications ..
High Voltage Arc-Tracking Rate, HVTR 14.0 mm/min
0.551 in/min
UL 746
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned)
Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad tempera..
High Voltage Arc-Tracking Rate, HVTR 14.0 mm/min
0.551 in/min
UL 746
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications incl..
High Voltage Arc-Tracking Rate, HVTR 14.0 mm/min
0.551 in/min
UL 746
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer
Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp..
High Voltage Arc-Tracking Rate, HVTR 14.0 mm/min
0.551 in/min
Conditioned; UL 746
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature..