Electrical Properties | Metric | English | Comments |
---|---|---|---|
High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min | UL 746A |
SABIC Innovative Plastics Cycoloy® C2950HF PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced impact and heat properties plus improved flow for various applications. |
|||
High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 503 PC 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. |
|||
High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 503R PC 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. Internal mold release. |
|||
High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 920A PC Low viscosity injection moldable, flame retardant PC. Exceptional surface appearance. Clear, tints and opaque colors. |
|||
High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 940ASR PC (Asia Pacific) More robust design of standard 900 series flame retardant grade. Internal mold release. |
|||
High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min | UL 746 |
Polymer Resources PC-FR1-D Polycarbonate, Improved Flame Retardant, Low Flow Polycarbonate, Improved Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal t.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min | UL 746 |
Polymer Resources PC-FR2-D Polycarbonate, Improved Flame Retardant, Medium Flow Polycarbonate, Improved Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min | UL 746A |
SABIC Innovative Plastics Lexan® FXD941A PC (Europe-Africa-Middle East) Transparent/translucent PC for light diffusion special effects. Color package may affect performance. |
|||
High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min | PLC 3 |
PTS Tristar® PC-10R-(IM) 10 MFI Impact Modified Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min | UL 746A |
SABIC Innovative Plastics Lexan® HPH4704 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 150 mm/min | 0.000 - 5.91 in/min | Average value: 30.5 mm/min Grade Count:10 |
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min | Average value: 115 mm/min Grade Count:4 |
Overview of materials for Polyphenylene Ether, Heat Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Heat Resistant". Each property range of values reported is minimum and maximum valu.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min | UL 746 |
Polymer Resources PC-FR1-D-[color]-3 Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples... |
|||
High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 4501 PPC High heat resistant polyphthlate carbonate, provides DTUL of 290F at 264 psi. |
|||
High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 953 PC Opaque colors, high viscosity, superior flame retardance. UV-stabilized. |
|||
High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min | PLC 3 |
PTS Tristar® PC-10FR-(VIM) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min | PLC 3 |
PTS Tristar® PC-10GFR-(V) 10% Glass Reinforced UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min | PLC 3 |
PTS Tristar® PC-10R-(V18) 18 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min | PLC 3 |
PTS Tristar® PC-10R-CL(V) 10 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 150 mm/min | 0.000 - 5.91 in/min | Average value: 49.3 mm/min Grade Count:6 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 150 mm/min | 0.394 - 5.91 in/min | Average value: 102 mm/min Grade Count:9 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 150 mm/min | 0.394 - 5.91 in/min | Average value: 65.3 mm/min Grade Count:25 |
Overview of materials for Polycarbonate, UV Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min | |
LG Chemical Lupox® GP1006FD PBT Description: Injection Molding, PBT, Flame Retardant, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 68928-70-1, 155123-66-3, 24968-12-5 and 1309-64-4Information provided by LG Chemica.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min | UL 746A |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_SPN422L PPE+HIPS (Europe-Africa-Middle East) LNP* Lubricomp Noryl_SPN422L is a wear resistant, fluorocarbon alloy, 235F (113C) HDT. UL94 HB rated. Check surface aesthetics prior to material specification. |
|||
High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min | UL 746A |
SABIC Innovative Plastics ULTEM CRS5111 PEI (Asia Pacific) 10% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5 VA listing. |
|||
High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min | UL 746A |
SABIC Innovative Plastics Valox® 553 PBT+PC (Asia Pacific) 30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc. |
|||
High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min | UL 746A |
SABIC Innovative Plastics Valox® 553U PBT+PC 30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc. |
|||
High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min @Thickness 1.50 mm |
3.15 - 5.91 in/min @Thickness 0.0591 in |
UL Rating PLC 3 (80-150 mm/min.) |
Covestro Makrolon® 6555 Polycarbonate, Injection Grade Medium viscosity, flame retardant injection molding with easy mold release, burning behavior.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG a.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 80.1 - 150 mm/min @Thickness 3.00 mm |
3.15 - 5.91 in/min @Thickness 0.118 in |
UL 746A |
Ascend Performance Materials Vydyne® 909 Nylon 66/6, 25% Glass Reinforced, Ignition Resistant, DAM Vydyne® 909 is halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwriters.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 950A PC Transparent, clear and colors, high viscosity, flame retardant with exceptional surface. |