Electrical Properties | Metric | English | Comments |
---|---|---|---|
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 923A PC Low viscosity, flame retardant with exceptional surface. Clear, tints and opaque colors. UV-stabilized. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 923A PC (Asia Pacific) Low viscosity, flame retardant with exceptional surface. Clear, tints and opaque colors. UV-stabilized. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 943AR PC (Asia Pacific) Medium viscosity, superior flame retardance. UV-Stabilized. Clear, tints and opaque colors. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 955AU PC (Asia Pacific) Lexan* 955AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a V0 UL rating and is UV stabilized, providing additiona.. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | surface, PLC code 2; UL 746A |
SABIC Innovative Plastics Lexan® 955U PC Lexan* 955U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio.. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | surface, PLC code 2; UL 746A |
SABIC Innovative Plastics Lexan® 151 PC (Asia Pacific) Nonhalogenated. 2.5 MFR. Blowmolding/extrusion.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 925U PC (Asia Pacific) Lexan* 925U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio.. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 943A PC (Asia Pacific) Medium viscosity, superior flame retardance. UV-Stabilized. Clear, tints and opaque colors. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 945U PC (Asia Pacific) Lexan* 945U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio.. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® FL920 PC (Asia Pacific) Various weight reductions at .250"" (6.35 mm) wall, 20% GR. Excellent flex mod, high tensile strength/heat resistance. V-0/5V at .250"" (6.35mm). |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs @Thickness 2.10 mm |
30 - 60 arcs @Thickness 0.0827 in |
|
LG Chemical AF312B ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs @Thickness 3.00 mm |
30 - 60 arcs @Thickness 0.118 in |
|
LG Chemical LUSEP SP2300 SPS+GF30%, General Purpose Feature: Injection Molding, sPS+GF30%, General PurposeApplication: Pump Units, Pick-up Lends Holder, etc.CAS No. 9003-53-6 and 65997-17-3Information provided by LG Chemical |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics NORYL SE1GFN3 PPE+PS (Asia Pacific) GR 30%. 275F (135C) DTUL. UL94 V-1 rated. Halogen free flame retardant. For electrical construction market. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics ULTEM UC1200 PEI (Asia Pacific) 12% carbon fiber reinforced Polyetherimide (Tg 217C). ECO Conforming. UL94 V0 listing in recognized colors. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Valox® 815 PBT 15% GR PBT+ PET, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | surface, PLC code 2; UL 746A |
SABIC Innovative Plastics Valox® EF4530 PBT (Asia Pacific) Easy flow, 30% glass-reinforced, PBTP resin. Flame retardant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics NORYL GTX GTX830 PPE+PS+PA (Asia Pacific) GR 30%. Highest stiffness of 1200000 psi (8200 MPa) flexural modulus. Excellent chemical and high heat resistance. Application: under the bonnet. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics NORYL HS2000X PPE+PS PPE+PS blend. 17% Mineral reinforced. Non-brominated, non-chlorinated FR system. UL94 V0 and 5VA listing. UL746C f1. Radiant panel listing. Dielectric strength. Dimensional stability. Suitable for E.. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics NORYL N190X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. RTI Elec/Imp/Str 95/80/95. Dielectric strength. Suitable for E/E market applications. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH6020 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 mm an.. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics NORYL PN235 PPE+PS (Asia Pacific) Plating grade, primarily automotive applications. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Valox® 430 PBT (Asia Pacific) 33 % glass reinforced, impact modified. Connectors, etc. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Valox® 815 PBT (Asia Pacific) 15% GR PBTP, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_PX5379 PPE+HIPS (Europe-Africa-Middle East) LNP* Thermocomp* Noryl_PX5379 compound is a 10% GR. UL94 V-1 rated. Halogen free flame retardant. Typical applications are TV chassis, deflection yokes and connectors. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs @Thickness 3.00 mm |
30 - 60 arcs @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 4011 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs @Thickness 3.00 mm |
30 - 60 arcs @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 4020 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics NORYL PX1007 PPE+HIPS (Europe-Africa-Middle East) NORYL* PX1007 is an unfilled non-chlorinated, non-brominated flame retardant PPE/HIPS grade, targeted for flat panel TV enclosures. It has a Vicat B/120 temperature of 96 degC and UL-94 V0 @ 1.5mm .. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 953A PC Clear, tints and opaque colors, high viscosity, flame retardant with exceptional surface. UV-stabilized. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
SABIC Innovative Plastics NORYL PX1005X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. UL746C F1. Excelent dielectric strength. Suitable for E/E market in indoor/outdoor applications. |
|||
High Amp Arc Ignition, HAI | 30 - 60 arcs @Thickness 1.50 mm |
30 - 60 arcs @Thickness 0.0591 in |
(BK) |
Hexion Bakelite™ PF 2836 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage, UL Listed
&nbs Phenolic molding compound, inorganically/organically filled, increased heat resistance, increased tracking resistance, low shrinkage and post shrinkage, improved electrical properties, UL listed mol.. |