Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Cycoloy® CY6414 PC (Asia Pacific) |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® 124 PC (Asia Pacific) 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information and should not .. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® 915R PC Lexan* 915R Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating with good flow and mold release properties... |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® 940ASR PC More robust design of standard 900 series flame retardant grade. Internal mold release. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® 945AU PC (Asia Pacific) Lexan* 945AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a V0 UL rating and is UV stabilized, providing additiona.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® 950 PC Opaque colors, high viscosity, superior flame retardance. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | PLC code 2; UL 746A |
SABIC Innovative Plastics Lexan® 955U PC Lexan* 955U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | PLC code 2; UL 746A |
SABIC Innovative Plastics Lexan® HPH4504 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® HPH4504 PPC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 LNP* Konduit* PX08321 a compound based on PA6 resins containing mineral. Added features include: Thermally Conductive. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 compound |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | PLC code 2; UL 746A |
SABIC Innovative Plastics Cycoloy® C6800 PC+ABS PC+ABS, nonchlorinated, nonbrominated flame retardant.This data was supplied by SABIC-IP for the Americas region. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® 925A PC Lexan* 925A Polycarbonate (PC) resin is a non-filled, injection moldable grade of non-chlorinated, non-brominated flame retardant systems that has an UL-94 V0 rating. Lexan 925A is available in tran.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® 955U PC (Asia Pacific) Lexan* 955U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | PLC 2 |
PTS Tristar® PC-10GFR-(V) 10% Glass Reinforced UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® HP2NR PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® HP6 PC Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mo.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 1.50 mm |
30 - 60 sec @Thickness 0.0591 in |
UL Rating PLC 2 (30-60 sec) |
Covestro Apec® DP9-9351 High-Heat Polycarbonate, General Purpose
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics ULTEM CRS5201 PEI (Asia Pacific) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Valox® 357 PBT (Asia Pacific) PBT + PC, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Valox® 420SE0 PBT 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Valox® 420SE0 PBT (Europe-Africa-Middle East) 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Asia Pacific) Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | PLC code 2; UL 746A |
SABIC Innovative Plastics Noryl NH3060 PPE+HIPS NH3060 resin is a modified PPE + PS blend with an excellent balance of non-chlorinated non-brominated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific .. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 3.00 mm |
30 - 60 sec @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 1007 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 3.00 mm |
30 - 60 sec @Thickness 0.118 in |
UL Rating PLC 2 (30-60 sec) |
Covestro Makrolon® 2458 Polycarbonate, Injection Grade Very easy flowing BgVV- and FDA injection molding grade with easy mold release, for food contact applications, better resistance to hot water.Information provided by Bayer.As of 1 September 2015, Ba.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 3.00 mm |
30 - 60 sec @Thickness 0.118 in |
UL Rating PLC 2 (30-60 sec) |
Covestro Makrolon® 2858 Polycarbonate, Injection Grade Medium flowing BgVV- and FDA injection molding grade, for food contact applications, better resistance to hot water.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was se.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 1.10 mm |
30 - 60 sec @Thickness 0.0433 in |
UL Rating PLC 2 (30-60 sec) |
Covestro Makrolon® 6465 Polycarbonate, Injection Grade Medium viscosity, flame retardant injection molding with easy mold burning behavior.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and offici.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics NORYL PX2060 PPE+PS Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |