Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® 104R PC (Asia Pacific) LEXAN 104R is a high viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information a.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® 201 PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® 244R PC 10.5 MFR. Improved flame retardance. USA FDA compliant (limited colors). Internal mold release. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® 4704 PPC (Asia Pacific) High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with .. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® 920A PC Low viscosity injection moldable, flame retardant PC. Exceptional surface appearance. Clear, tints and opaque colors. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® EXL6414 PC PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® EXL6414 PC (Asia Pacific) PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® FXD121R PC Transparent/translucent PC for light diffusion special effects. MFR of 18.2. Color package may affect performance. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® FXD941A PC (Europe-Africa-Middle East) Transparent/translucent PC for light diffusion special effects. Color package may affect performance. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | PLC code 2; UL 746A |
SABIC Innovative Plastics Lexan® FXD951A PC Visual effetcs diffusion, flame retardant PC with low/medium flow good for extrusion/injection molding applications. Ideal for light management platforms that require hiding power and transmission.T.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® HP2C PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | PLC code 2; UL 746A |
SABIC Innovative Plastics Lexan® PPC4504 PPC High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® 920A PC (Asia Pacific) Low viscosity injection moldable, flame retardant PC. Exceptional surface appearance. Clear, tints and opaque colors. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® 925U PC (Asia Pacific) Lexan* 925U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® 943A PC (Asia Pacific) Medium viscosity, superior flame retardance. UV-Stabilized. Clear, tints and opaque colors. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | PLC 2 |
PTS Tristar® PC-10GFR-(V) 10% Glass Reinforced UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® HP2NR PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® HP6 PC Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mo.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR2210 PC (Asia Pacific) Alternative polymeric wear additive technology. No silicones, superior processability/part appearance. Flow similar to LEXAN 121. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_SPN422L PPE+PS LNP* Lubricomp* Noryl_SPN422L compound is a wear resistant, fluorocarbon alloy, 235F (113C) HDT. UL94 HB rated. Check surface aesthetics prior to material specification. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics PREVEX VGAX PPE+PS Improved productivity and reliability. Nonchlorinated, nonbrominated flame retardant. 180F HDT. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics ULTEM CRS5201 PEI 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Valox® IQ357M PBT+PC Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics NORYL N190X PPE+HIPS (Asia Pacific) PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. Dielectric strength. Suitable for E/E market applications. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Valox® 815 PBT (Asia Pacific) 15% GR PBTP, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | PLC code 2; UL 746A |
SABIC Innovative Plastics Noryl BN30 PPE+PS Blowmoldable. DTUL 180F. UL rated.This data was supplied by SABIC-IP for the Americas region. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 3.00 mm |
30 - 60 sec @Thickness 0.118 in |
UL Rating PLC 2 (30-60 sec) |
Covestro Makrolon® 3105 Polycarbonate Injection molding and extrusion grade with high viscosity, with easy mold release.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and official.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 3.00 mm |
30 - 60 sec @Thickness 0.118 in |
UL Rating PLC 2 (30-60 sec) |
Covestro Makrolon® 6255 Polycarbonate, Flame Retardant, High Productivity, Mold Release Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® HF1110 PC (Asia Pacific) General purpose grade. Good clarity, heat resistance, property retention and dimensional stability. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Europe-Africa-Middle East) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |