Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® 101 PC (Asia Pacific) Nonhalogenated, 7.0 MFR, for thicker sections without sinks. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® 104 PC (Asia Pacific) LEXAN 104 is a high viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information an.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® 121 PC (Asia Pacific) Nonhalogenated. 17.5 MFR, for small intricate parts. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® 124 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® 131 PC Nonhalogenated. 3.5 MFR. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® 241 PC General Purpose polycarbonate with 10.5 of melt flow rate. Improved flame retardance. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® 244RF PC (Asia Pacific) LEXAN 244RF resin grade is a medium viscosity multi purpose product with improved flame resistance and release properties. It is also FDA food contact compliant available in limited colors. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® 915RP PC (Asia Pacific) Lexan* 915RP Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating with good flow and mold release properties.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® 940ASR PC (Asia Pacific) More robust design of standard 900 series flame retardant grade. Internal mold release. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® 945AU PC (Asia Pacific) Lexan* 945AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a V0 UL rating and is UV stabilized, providing additiona.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | PLC code 2; UL 746A |
SABIC Innovative Plastics Lexan® EXL6414 PC (Europe-Africa-Middle East) PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® HF1140R PC High flow grade. Heat stabilized. Enhanced level of mold release. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported with biocompatib.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® HPH4504 PPC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® 920A PC (Asia Pacific) Low viscosity injection moldable, flame retardant PC. Exceptional surface appearance. Clear, tints and opaque colors. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® 925AU PC (Asia Pacific) Lexan* 925AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing addit.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® HP6NR PC Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® HP6NR PC (Asia Pacific) Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=2.10 mm |
30 - 60 sec @Thickness >=0.0827 in |
|
LG Chemical AF312B ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics ULTEM CRS5301 PEI (Asia Pacific) 30% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Valox® 357U PBT (Asia Pacific) Unreinforced PBTP, UL94 V-0/5VA rated. Improved UV resistant version of VALOX 357. Nonblooming flame retardant. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Valox® 365 PC+PET Unreinforced, opaque, provides chemical resistance and dimensional stability, UL94V-0 rated at 0.031"". |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Valox® 365 PET (Asia Pacific) Unreinforced, opaque, provides chemical resistance and dimensional stability, UL94V-0 rated at 0.031"". |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Valox® 420SE0U PBT PBT, 30% Glass Reinforced, Flame Retardant UL94 V-0/5VA rated, UV-Stabilized |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Valox® IQ357 PBT+PC Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 3.00 mm |
30 - 60 sec @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 1008 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | PLC code 2; UL 746A |
SABIC Innovative Plastics Noryl PC180X PPE+PS Nonbrominated, nonchlorinated flame retardant. V-1/5VA rated; 175F (90C) HDT. Improved productivity and reliability.This data was supplied by SABIC-IP for the Americas region. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 3.00 mm |
30 - 60 sec @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 1003 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 1.10 mm |
30 - 60 sec @Thickness 0.0433 in |
UL Rating PLC 2 (30-60 sec) |
Covestro Makrolon® 6465 Polycarbonate, Injection Grade Medium viscosity, flame retardant injection molding with easy mold burning behavior.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and offici.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 3.00 mm |
30 - 60 sec @Thickness 0.118 in |
UL Rating PLC 2 (30-60 sec) |
Covestro Makrolon® 6555 Polycarbonate, Injection Grade Medium viscosity, flame retardant injection molding with easy mold release, burning behavior.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG a.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
SABIC Innovative Plastics Lexan® 940A PC (Asia Pacific) Medium viscosity, flame retardant PC. Exceptional surface. Clear, tints and opaque colors. |