Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 10000 ohm | 10000 ohm | |
Lehmann & Voss LUVOCOM® 1105-7506 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista.. |
|||
Insulation Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 1105-7905 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista.. |
|||
Insulation Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 1115/XCF/40 PEK, with carbon fiber Applications: High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts, non flammable.Electrically c.. |
|||
Insulation Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 1200-8493 ABS, with steel fiber Applications: Office communication.Electrically conductive, suitable for continuous discharging of statically generated electricity.Isotropic shrinkage characteristics.Information provided by Lehman.. |
|||
Insulation Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 1850/CF/10/GF/10/GK/10/GS/5/FR PBT, with carbon fiber, glass fiber, glass spheres and glass flakes, fire protection Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High dimensionally stable precision parts, even at elevated temperatures and narrow tolerance r.. |
|||
Insulation Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 1850/CF/10/TF/10/EM PBT, with carbon fiber, PTFE, easy flowing Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Electrically conductive, suita.. |
|||
Insulation Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 19-7278 Polyamide 46, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Insulation Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 19-8195/FR Polyamide 46, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Insulation Resistance | 10000 - 1.00e+8 ohm | 10000 - 1.00e+8 ohm | |
Lehmann & Voss LUVOCOM® 20-8244 Polyphthalamide, with carbon fiber and glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Insulation Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 50-0833 Polycarbonate, with carbon fiber and glass fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Reduced moment of inertia compared with metal parts.Electrical.. |
|||
Insulation Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 50-1375 Polycarbonate, with carbon fiber, glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Insulation Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 50-7228 Polycarbonate, with carbon fiber, glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont.. |
|||
Insulation Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 50-7289 Polycarbonate, with carbon fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont.. |
|||
Insulation Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 50-7289/V2 Polycarbonate, with carbon fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont.. |
|||
Insulation Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 50-7586 Polycarbonate, with carbon fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts with low warpage and.. |
|||
Insulation Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 50-7856/FR/BK Polycarbonate, with carbon fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Insulation Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 50-8022 Polycarbonate, with carbon fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Reduced moment of inertia compared with me.. |
|||
Insulation Resistance | 10000 - 1.00e+8 ohm | 10000 - 1.00e+8 ohm | |
Lehmann & Voss LUVOCOM® 65-7311 PP-copolymer, with carbon fiber Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided by Lehmann & .. |
|||
Insulation Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 65-8347/RD PP-copolymer, with carbon fiber Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided by Lehmann & .. |
|||
Insulation Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 80-7555 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Insulation Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 80-7555/BK Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Insulation Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 1/CF/10/GF/20/BK Polyamide 66, with carbon fiber and glass fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Insulation Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 1-0889-2 Polyamide 66, with carbon fiber and glass fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically .. |
|||
Insulation Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 1-0889-4 Polyamide 66, with carbon fiber and glass fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically .. |
|||
Insulation Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 1105-7781/BK PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Insulation Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 1106-8374 Polyether imide, with carbon fiber and PTFE Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.Hig.. |
|||
Insulation Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 1-1119-1 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Insulation Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 1800-7519 PET, with carbon fiber, PTFE, mineral resin Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous d.. |
|||
Insulation Resistance | <= 10000 ohm | <= 10000 ohm | |
Lehmann & Voss LUVOCOM® 1/XCF/25 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Insulation Resistance | 10000 - 1.00e+11 ohm | 10000 - 1.00e+11 ohm | Average value: 3.33e+10 ohm Grade Count:3 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |