Electrical Properties Metric English Comments
Dielectric Strength 14.0 kV/mm

@Thickness 3.20 mm,
Temperature 23.0 °C
356 kV/in

@Thickness 0.126 in,
Temperature 73.4 °F
Short Time; ASTM D149
DuPont Performance Polymers Crastin® 6130 NC010 PBT  (Unverified Data**)
Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers
Dielectric Strength 14.0 kV/mm

@Thickness 3.18 mm
356 kV/in

@Thickness 0.125 in
Solvay Specialty Polymers Halar® 300 ECTFE Fluoropolymer  (discontinued **)
Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing..
Dielectric Strength 14.0 kV/mm

@Thickness 1.60 mm
356 kV/in

@Thickness 0.0630 in
Solvay Specialty Polymers Halar® 500 ECTFE Fluoropolymer  (discontinued **)
Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing..
Dielectric Strength 14.0 kV/mm

@Thickness 3.18 mm
356 kV/in

@Thickness 0.125 in
Solvay Specialty Polymers Halar® 500 ECTFE Fluoropolymer  (discontinued **)
Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing..
Dielectric Strength 14.0 kV/mm

@Thickness 1.60 mm
356 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
SABIC Innovative Plastics Xenoy® CL200 PBT+PC (Europe-Africa-Middle East)
XENOY CL200 is a semi-crystalline thermoplastic blend, specially developed to obtain good low temperature impact strength combined with excellent chemical resistance to occasional solvent and gasoli..
Dielectric Strength 14.0 kV/mm

@Frequency 60 Hz
356 kV/in

@Frequency 60 Hz
Wet, short time; ASTM D149
Sumitomo Bakelite North America RX® 640 Fiberglass Reinforced Phenolic Resole
RXÂ 640 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-5.Information supp..
Dielectric Strength 14.0 kV/mm

@Thickness 3.20 mm
356 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® 430 PBT (Europe-Africa-Middle East)
VALOX 430 is 33% glass reinforced, impact modified PBT injection moulding resin.
Dielectric Strength 14.0 kV/mm

@Frequency 60.0 Hz
356 kV/in

@Frequency 60.0 Hz
step-by-step, dry; ASTM D149
Sumitomo Bakelite North America E 16521A Electrical Encapsulation Grade Epoxy
E-16521A is an encapsulation grade epoxy molding compound suitable for electrical applications such as coils.Information provided by Sumitomo Bak North America, Inc.
Dielectric Strength 14.0 kV/mm

@Thickness 2.00 mm
356 kV/in

@Thickness 0.0787 in
Practical Use (Water Absorption 2.4%); ASTM-D149
Toyobo GLAMIDE® T-656E Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Dielectric Strength 14.0 kV/mm

@Thickness 2.00 mm
356 kV/in

@Thickness 0.0787 in
Practical Use (Water Absorption 2.9%); ASTM-D149
Toyobo GLAMIDE® TY-102ND Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Dielectric Strength 14.0 kV/mm

@Thickness 2.00 mm
356 kV/in

@Thickness 0.0787 in
Practical Use (Water Absorption 2.4%); ASTM-D149
Toyobo GLAMIDE® NB-1700 Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Dielectric Strength 14.0 kV/mm

@Thickness 3.00 mm
356 kV/in

@Thickness 0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60245-1; IEC/EN 60893-2 6.1.3.1
Elektro-Isola Etronit IS Phenolic, Paper Reinforcement, Dark Brown, Sheets
Description: Very good high-voltage insulation material. Very high breakdown voltage, in particular parallel to the layers. Dimensionally stable.Application: Insulation material in high-voltage tap ..
Dielectric Strength 14.0 kV/mm

@Thickness 3.20 mm,
Temperature 95.0 °C
356 kV/in

@Thickness 0.126 in,
Temperature 203 °F
500 V/s, in oil; Short Time; ASTM D149
DuPont Performance Polymers Rynite® 940 BK505 PET  (Unverified Data**)
Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers