Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 100 sec | 100 sec | ASTM D495 |
Shell Carilon® DP P1000 Polyketone
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON® Thermoplastic Polymer DP P1000 is the first in a family of developmental engineering polyketone resins fr.. |
|||
Arc Resistance | 100 sec | 100 sec | IPC-TM-650.2.5.1 |
Park Electrochemical Nelco® N7000-2 HT/N7000-3 Toughened Polyimide Laminate and Prepreg The Nelco N7000-2 HT laminate and N7000-3 prepreg are a series of toughened polyimide materials for use in high-reliability multilayers. This combined resin system provides excellent thermal perform.. |
|||
Arc Resistance | 100 sec | 100 sec | Average value: 100 sec Grade Count:3 |
Overview of materials for Polysulfone, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl.. |
|||
Arc Resistance | 100 - 116 sec | 100 - 116 sec | Average value: 108 sec Grade Count:4 |
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor.. |
|||
Arc Resistance | 100 - 130 sec | 100 - 130 sec | Average value: 119 sec Grade Count:6 |
Overview of materials for Nylon 6, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Arc Resistance | 100 sec @Thickness 3.17 mm |
100 sec @Thickness 0.125 in |
ASTM D495 |
Industrial Laminates/Norplex NP130 Glass Fabric Description: Woven glass fabric combined with a halogenated epoxy resin system. Produced to printed circuit board quality standards. Flame retardant, meets UL-94 flammability classification V-0.Thic.. |
|||
Arc Resistance | 100 sec @Thickness 3.17 mm |
100 sec @Thickness 0.125 in |
ASTM D495 |
Industrial Laminates/Norplex NP504 Glass Fabric Description: Woven glass fabric with high temperature phenolic resin. Good flexural, compressive and impact strengths at elevated temperatures. Capable of continuous operation at 175° C, see note.. |
|||
Arc Resistance | 100 sec @Thickness 3.17 mm |
100 sec @Thickness 0.125 in |
ASTM D495 |
Industrial Laminates/Norplex NP680 Paper Base Laminate Description: Hot punching grade with electrical properties between NP611 to NP631.Thickness Tested: 0.062", 0.125" & 0.500" |
|||
Arc Resistance | 100 sec | 100 sec | ASTM D495 |
Gromax CCP PET 9130-104 30% Glass Filled Product Description: PET glass/mineral 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excell.. |
|||
Arc Resistance | 100 sec | 100 sec | ASTM D495 |
Haysite 48600 Polyester SMC, 30% Glass Reinforced The 48600 series sheet molding compound is formulated with a high temperature resin system (180º C). Designed for compression molding, this grade offers excellent retention of physical and electr.. |
|||
Arc Resistance | 100 sec | 100 sec | ASTM D495 |
Gromax PBT 2000-104D Product Description: PBT unreinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Excellent mechanic an.. |
|||
Arc Resistance | 100 sec | 100 sec | ASTM D495 |
Gromax PBT 3030-104 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Arc Resistance | 100 sec | 100 sec | ASTM D495 |
Solvay Specialty Polymers Ryton® XK2340 Polyphenylene Sulfide Alloy (PPS Alloy), 40% Glass Fiber Ryton® XK2340 40% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength, toughness, and rigidity, along with excellent flow in thin-walled parts, low .. |
|||
Arc Resistance | 100 sec | 100 sec | Absolute Drying; ASTM-D495 |
Toyobo GLAMIDE® T-403 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Arc Resistance | 100 sec | 100 sec | Absolute Drying; ASTM-D495 |
Toyobo GLAMIDE® T-663G30 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Arc Resistance | 100 sec | 100 sec | Absolute Drying; ASTM-D495 |
Toyobo GLAMIDE® TY-791GT 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Arc Resistance | 100 sec | 100 sec | Tungsten; ASTM D495 |
Asahi Kasei Xyron® 100V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Arc Resistance | 100 sec | 100 sec | Tungsten; ASTM D495 |
Asahi Kasei Xyron® 140V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Arc Resistance | 100 sec | 100 sec | Tungsten; ASTM D495 |
Asahi Kasei Xyron® 240V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Arc Resistance | 100 sec | 100 sec | Tungsten; ASTM D495 |
Asahi Kasei Xyron® 220V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Arc Resistance | 100 sec | 100 sec | ASTM D495 |
Gromax CCP PBT 3030-200HR 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Arc Resistance | 100 sec | 100 sec | ASTM D495 |
Gromax CCP PBT 3040-201 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Arc Resistance | 100 sec | 100 sec | ASTM D495 |
Gromax CCP PBT 4830-BK 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Arc Resistance | 100 sec | 100 sec | ASTM D495 |
Plenco 51015 PET, Pellet, Injection Molded, White
(discontinued **) PLENCO 51015 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL listed.Information supplied by.. |