Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D257 |
PolyOne Lubri-Tech™ AT-15CF/5T Acetal-Copolymer, Carbon Fiber Reinforced, PTFE Lubricated
(discontinued **)&l Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D257 |
PolyOne Lubri-Tech™ AS-15CF/15T Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced, PTFE Lubricated
&nb Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D257 |
PolyOne Edgetek® AS-20CF/000 Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D257 |
PolyOne Edgetek® NL-23CF/000 Nylon 6/12, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D257 |
PolyOne Lubri-Tech™ NL-30CF/10T-2S Nylon 6/12, Carbon Fiber Reinforced, PTFE Lubricated
(discontinued **) Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D648 |
Techmer ES Electrafil® J-4/25/CF/15 BK PA6/12 |
|||
Surface Resistivity per Square | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D648 |
Techmer ES Electrafil® J-4/25/CF/15 NAT PA6/12 |
|||
Surface Resistivity per Square | 1000 - 10000 ohm | 1000 - 10000 ohm | ASTM D648 |
Techmer ES Electrafil® M-1322 PA66 / PA6 |
|||
Surface Resistivity per Square | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D648 |
Techmer Lehvoss Compounds Luvotech™ J-4/30 BK PA6/12
(discontinued **) Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated. |
|||
Surface Resistivity per Square | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D257 |
PolyOne Lubri-Tech™ NI-30CF/10T-2S Nylon 6/10, Carbon Fiber Reinforced, PTFE/Silicone Lubricated
(discontinue Description/Features:Carbon Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D257 |
PolyOne Lubri-Tech™ MP-20CF/15T Modified Polyphenylene Oxide (mPPO), Carbon Fiber Reinforced, PTFE Lubricated
  Description/Features:Carbon Fiber ReinforcedPTFE LubricatedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D257 |
PolyOne Edgetek® PI-20CF/000 Polyetherimide (PEI), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D257 |
PolyOne Edgetek® AM-20CF/000 Polyphthalamide (PPA), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D257 |
PolyOne Edgetek® AM-20CF-20GF/000 Polyphthalamide (PPA), Glass/Carbon Fiber Filled
(discontinued **) Description/Features:Glass/Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |