Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.0 - 1000 ohm | 1.0 - 1000 ohm | ASTM D257 |
PolyOne Stat-Tech™ NN-30CF/000 Black Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Surface Resistance | 1.0 - 10000 ohm | 1.0 - 10000 ohm | ASTM D4496 |
LNP Stat-Kon® PDX-E-99550 CCS Polyetherimide, Carbon Fiber Reinforcement
(discontinued **) Features: Low to None Ion Content, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued.. |
|||
Surface Resistance | 1.0 - 100 ohm | 1.0 - 100 ohm | ASTM D257 |
Techmer ES Electrablend® ABS 03009 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: Conductive, Electromagnetic Shielding (EMI) and Radio Frequency Shielding (RFI)Information provided.. |
|||
Surface Resistance | 1.0 - 5.0 ohm | 1.0 - 5.0 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON AE002 ABS (Asia Pacific) LNP* Stat-kon* AE002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Surface Resistance | 1.0 - 4.0 ohm | 1.0 - 4.0 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON AE006 ABS LNP* STAT-KON* AE006 is a compound based on ABS containing 30% Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
Surface Resistance | 1.0 - 6.0 ohm | 1.0 - 6.0 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON AX06518 ABS (Asia Pacific) LNP* Stat-kon* AX06518 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive, Fl.. |
|||
Surface Resistance | 1.0 ohm | 1.0 ohm | ASTM D257 |
Techmer ES Electrablend® PA6/6 05012 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveInformation provided by TP Composites, Inc. |
|||
Surface Resistance | 1.0 - 1000 ohm | 1.0 - 1000 ohm | ASTM D257 |
Techmer ES Electrablend® PC 04005 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by.. |
|||
Surface Resistance | 1.0 - 1000 ohm | 1.0 - 1000 ohm | ASTM D257 |
Techmer ES Electrablend® PC 04007 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by.. |
|||
Surface Resistance | 1.0 - 100 ohm | 1.0 - 100 ohm | ASTM D257 |
Techmer ES Electrablend® PC/ABS 033009 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: Electrically Conductive and ESD ProtectionInformation provided by TP Composites, Inc. |
|||
Surface Resistance | 1.0 - 1000 ohm | 1.0 - 1000 ohm | ASTM D257 |
Techmer ES Electrablend® PEI 04001 MB Stainless Steel Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI)Information provided by TP Composites, Inc. |
|||
Surface Resistance | 1.0 - 100 ohm | 1.0 - 100 ohm | ASTM D257 |
Techmer ES Electrablend® PEI 04008 MB Availability: North AmericaForms: PelletsFeatures: Conductive and CopolymerInformation provided by TP Composites, Inc. |
|||
Surface Resistance | 1.0 - 10 ohm | 1.0 - 10 ohm | ASTM D257 |
Techmer ES Electrafil® DB-1200/SS/7 ABS, 7% Stainless Steel Fiber Reinforced (dry blend) Superior cost-performance when compared with other electrically conductive resins is a hallmark of Electrafil stainless steel fiber reinforced ABS. Electrafil compounds can be formulated to meet UL.. |
|||
Surface Resistance | 1.0 - 4.0 ohm | 1.0 - 4.0 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DE0069F PC LNP* STAT-KON* DE0069F is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Superior Molding. |
|||
Surface Resistance | 1.0 - 3.0 ohm | 1.0 - 3.0 ohm | ASTM D 257 |
SABIC Innovative Plastics LNP Stat-kon EE008E PEI LNP STAT-KON* EE008E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas r.. |
|||
Surface Resistance | 1.0 - 3.0 ohm | 1.0 - 3.0 ohm | ROA; IEC 60093 |
SABIC Innovative Plastics LNP STAT-KON OEL13I PPS - Linear LNP* STAT-KON* OEL13I is a compound based on PPS-Linear resin containing 15% Carbon Fiber, 5% PTFE. Added features of this grade include: High Impact, Wear Resistant, Electrically Conductive. |
|||
Surface Resistance | 1.0 - 3.0 ohm | 1.0 - 3.0 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON OEL36A PPS - BRANCHED LNP* STAT-KON* OEL36A is a compound based on PPS - Branched resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
Surface Resistance | 1.0 - 6.0 ohm | 1.0 - 6.0 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON PFD06 PA 6 LNP* STAT-KON* PFD06 is a compound based on Nylon 6 resin containing 30% Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Surface Resistance | 1.0 - 4.0 ohm | 1.0 - 4.0 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON REL33 PA 66 LNP STAT-KON* REL33 is a compound based on Nylon 66 resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Surface Resistance | 1.0 - 3.0 ohm | 1.0 - 3.0 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON RFD03 PA 66 LNP* STAT-KON* RFD03 is a compound based on Nylon 66 containing 15% Glass Fiber. Added feature of this material is: Electrically Conductive. |
|||
Surface Resistance | 1.0 - 6.0 ohm | 1.0 - 6.0 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON RX05489 PA 66 (Asia Pacific) LNP* STAT-KON* RX05489 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Surface Resistance | 1.0 - 1000 ohm | 1.0 - 1000 ohm | ASTM D257 |
Techmer ES Electrablend® ABS 03011 FR BK MB 15% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 15% Filler by WeightFeatures: Flame Retardant and Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 7965121I.. |
|||
Surface Resistance | 1.0 - 1000 ohm | 1.0 - 1000 ohm | ASTM D257 |
Techmer ES Electrablend® ABS 04002 BK 16% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 16% Filler by WeightFeatures: Flame Retardant and Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 7965121I.. |
|||
Surface Resistance | 1.0 - 100 ohm | 1.0 - 100 ohm | ASTM D257 |
Techmer ES Electrablend® ABS CF15 FR BK 15% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 15% Filler by WeightFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Surface Resistance | 1.0 - 10 ohm | 1.0 - 10 ohm | ASTM D257 |
Techmer ES Electrablend® ABS SS15 BK MB 15% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 15% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Appearance: BlackInformation provided by TP Composi.. |
|||
Surface Resistance | 1.0 - 100 ohm | 1.0 - 100 ohm | ASTM D257 |
Techmer ES Electrablend® PA6/6 05002 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Surface Resistance | 1.0 - 10000 ohm | 1.0 - 10000 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON EX99550C PEI LNP* STAT-KON* EX99550C is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive. |
|||
Surface Resistance | 1.0 - 4.0 ohm | 1.0 - 4.0 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON RE0069S PA 66 (Asia Pacific) LNP* STAT-KON* RE0069S is a compound based on Nylon 66 resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Heat Stabil.. |
|||
Surface Resistance | 1.0 - 1000 ohm | 1.0 - 1000 ohm | ASTM D257 |
Techmer ES Electrablend® PA6 CF20 BK 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Conductive, Heat Stabilized and Lubric.. |
|||
Surface Resistance | 1.0 - 10 ohm | 1.0 - 10 ohm | ASTM D257 |
Techmer ES Electrafil® DB-50/SS/6 Polycarbonate, 6% Stainless Steel Fiber (dry blend) |