Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Electrafil® DB-50/SS/6 Polycarbonate, 6% Stainless Steel Fiber (dry blend)

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Stainless Steel Fiber
Manufacturer Techmer ES
Trade Name Electrafil®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Techmer ES Electrafil® DB-50/SS/6 Polycarbonate, 6% Stainless Steel Fiber (dry blend).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 62.1 MPa
9000 psi
ASTM D638
Elongation at Break 9.0 %
9.0 %
ASTM D638
Flexural Yield Strength 89.6 MPa
13000 psi
ASTM D790
Izod Impact, Notched 0.694 J/cm

@Thickness 3.17 mm
1.30 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 138 °C
280 °F
ASTM D648
Electrical Properties Metric English Comments
Electrical Resistivity 10.0 - 100 ohm-cm
10.0 - 100 ohm-cm
ASTM C611
Surface Resistance 1.0 - 10 ohm
1.0 - 10 ohm
ASTM D257