Techmer ES Electrablend® ABS CF15 FR BK 15% Carbon Filled

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled
Manufacturer Techmer ES
Trade Name Electrablend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Electrablend® ABS CF15 FR BK 15% Carbon Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 15% Filler by WeightFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Water Absorption 0.14 %

@Time 86400 sec
0.14 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0015 cm/cm

@Thickness 3.17 mm
0.0015 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785
Tensile Strength, Yield 96.5 MPa
14000 psi
ASTM D638
Elongation at Break 1.8 %
1.8 %
ASTM D638
Flexural Strength 138 MPa
20000 psi
ASTM D790
Flexural Modulus 1.05 GPa
153 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 30.6 µm/m-°C
17.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 113 °C
235 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
220 °F
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.0 - 100 ohm-cm
1.0 - 100 ohm-cm
ASTM D257
Surface Resistance 1.0 - 100 ohm
1.0 - 100 ohm
ASTM D257