Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP STAT-KON AE002 ABS (Asia Pacific)

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON AE002 ABS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* Stat-kon* AE002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 78.0 MPa
11300 psi
ASTM D638
Elongation at Break 1.5 %
1.5 %
ASTM D638
Tensile Modulus 7.23 GPa
1050 ksi
50 mm/min; ASTM D638
Flexural Strength 117 MPa
17000 psi
ASTM D790
Flexural Modulus 7.03 GPa
1020 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.45 J/cm
4.59 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °C

@Thickness 3.20 mm
208 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 1.0 - 5.0 ohm
1.0 - 5.0 ohm
ASTM D257