Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1000 - 1.00e+16 ohm-cm | 1000 - 1.00e+16 ohm-cm | Average value: 1.81e+15 ohm-cm Grade Count:19 |
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are.. |
|||
Electrical Resistivity | 1000 - 1.00e+16 ohm-cm | 1000 - 1.00e+16 ohm-cm | Average value: 2.18e+15 ohm-cm Grade Count:12 |
Overview of materials for Polyphthalamide (PPA), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Aramid Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Electrical Resistivity | 1000 - 1.00e+18 ohm-cm | 1000 - 1.00e+18 ohm-cm | Average value: 1.25e+17 ohm-cm Grade Count:110 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Electrical Resistivity | 1000 - 1.00e+17 ohm-cm | 1000 - 1.00e+17 ohm-cm | Average value: 3.33e+16 ohm-cm Grade Count:6 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass + Mineral Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass + Mineral Filler". Each property range of values reported is mi.. |
|||
Electrical Resistivity | 1000 - 1.00e+16 ohm-cm | 1000 - 1.00e+16 ohm-cm | Average value: 1.95e+15 ohm-cm Grade Count:11 |
Overview of materials for PVC, Uncompounded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Electrical Resistivity | 1000 - 1.00e+17 ohm-cm | 1000 - 1.00e+17 ohm-cm | Average value: 2.40e+16 ohm-cm Grade Count:10 |
Overview of materials for Polyetherimide (PEI), 10% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 10% Glass Fiber". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Electrical Resistivity | 1000 - 3.00e+16 ohm-cm | 1000 - 3.00e+16 ohm-cm | Average value: 7.45e+15 ohm-cm Grade Count:11 |
Overview of materials for Polysulfone, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl.. |
|||
Electrical Resistivity | 1000 - 1.00e+15 ohm-cm | 1000 - 1.00e+15 ohm-cm | Average value: 2.65e+14 ohm-cm Grade Count:32 |
Overview of materials for Nylon 46, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Electrical Resistivity | 1000 - 1.00e+16 ohm-cm | 1000 - 1.00e+16 ohm-cm | Average value: 5.11e+15 ohm-cm Grade Count:11 |
Overview of materials for Polyphenylene Sulfide (PPS), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Aramid Fiber". Each property range of values reported is minimum and maximu.. |
|||
Electrical Resistivity | 1000 - 1.00e+18 ohm-cm | 1000 - 1.00e+18 ohm-cm | Average value: 3.64e+16 ohm-cm Grade Count:71 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |
|||
Electrical Resistivity | 1000 - 1.00e+15 ohm-cm | 1000 - 1.00e+15 ohm-cm | Average value: 1.99e+14 ohm-cm Grade Count:22 |
Overview of materials for Nylon 12, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Electrical Resistivity | 1000 - 10000 ohm-cm | 1000 - 10000 ohm-cm | ASTM C611 |
Techmer ES Electrafil® J-50/CF/10 Polycarbonate, 10% Carbon Fiber Reinforced Carbon Fiber Reinforced |
|||
Electrical Resistivity | <= 1000 ohm-cm @Temperature 1000 °C |
<= 1000 ohm-cm @Temperature 1830 °F |
ASTM D1829 |
CoorsTek Alumina-Zirconia Composite, AZ-25 Information provided by CoorsTek. |
|||
Electrical Resistivity | 1000 - 1.00e+17 ohm-cm | 1000 - 1.00e+17 ohm-cm | Average value: 6.43e+15 ohm-cm Grade Count:43 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Electrical Resistivity | 1000 - 1.00e+17 ohm-cm | 1000 - 1.00e+17 ohm-cm | Average value: 3.58e+15 ohm-cm Grade Count:28 |
Overview of materials for Polyether Block Amide (PEBA) This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a.. |
|||
Electrical Resistivity | <= 1000 ohm-cm | <= 1000 ohm-cm | IEC 60093 |
CENTROPLAST CENTROLEN PP LF Polypropylene conductive This material is a low density, easily machined plastic that can be welded and has good surface conductivity. Applications include filter heads and housings, conveyor equipment for flammable liquid.. |
|||
Electrical Resistivity | 1000 - 1.00e+18 ohm-cm | 1000 - 1.00e+18 ohm-cm | Average value: 2.85e+17 ohm-cm Grade Count:14 |
Overview of materials for Polypropylene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Electrical Resistivity | 1000 - 3.00e+16 ohm-cm | 1000 - 3.00e+16 ohm-cm | Average value: 3.87e+15 ohm-cm Grade Count:28 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |