Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+10 - 1.00e+15 ohm-cm | 1.00e+10 - 1.00e+15 ohm-cm | Average value: 7.50e+14 ohm-cm Grade Count:4 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum .. |
|||
Electrical Resistivity | 400 - 1.00e+15 ohm-cm | 400 - 1.00e+15 ohm-cm | Average value: 7.50e+14 ohm-cm Grade Count:4 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum .. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | Average value: 3.25e+14 ohm-cm Grade Count:4 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a.. |
|||
Electrical Resistivity | 1.00e+8 - 1.00e+15 ohm-cm @Temperature 66.0 - 130 °C |
1.00e+8 - 1.00e+15 ohm-cm @Temperature 151 - 266 °F |
Average value: 7.80e+13 ohm-cm Grade Count:7 |
Overview of materials for Epoxy, Cast, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Unreinforced". Each property range of values reported is minimum and maximum values of appr.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite Butyrate 465E2R30012 Natural, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 12%. Weight loss on heating = 1.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Electrical Resistivity | 1.00e+10 - 1.00e+15 ohm-cm | 1.00e+10 - 1.00e+15 ohm-cm | Average value: 4.78e+14 ohm-cm Grade Count:48 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Electrical Resistivity | 1.00e+8 - 1.00e+15 ohm-cm | 1.00e+8 - 1.00e+15 ohm-cm | Average value: 7.50e+14 ohm-cm Grade Count:11 |
Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |
|||
Electrical Resistivity | 1.00e+9 - 1.00e+15 ohm-cm | 1.00e+9 - 1.00e+15 ohm-cm | Average value: 2.37e+14 ohm-cm Grade Count:72 |
Overview of materials for Nylon 6, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Electrical Resistivity | 1.00e+9 - 1.00e+15 ohm-cm | 1.00e+9 - 1.00e+15 ohm-cm | Average value: 4.88e+14 ohm-cm Grade Count:28 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Electrical Resistivity | 1.00e+10 - 1.00e+15 ohm-cm | 1.00e+10 - 1.00e+15 ohm-cm | Average value: 1.43e+14 ohm-cm Grade Count:29 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
Electrical Resistivity | 1.00e+10 - 1.00e+15 ohm-cm | 1.00e+10 - 1.00e+15 ohm-cm | Average value: 9.50e+13 ohm-cm Grade Count:8 |
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl.. |
|||
Electrical Resistivity | 3.00e+12 - 1.00e+15 ohm-cm | 3.00e+12 - 1.00e+15 ohm-cm | Average value: 4.80e+14 ohm-cm Grade Count:16 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
Electrical Resistivity | 1.00e+12 - 1.00e+15 ohm-cm | 1.00e+12 - 1.00e+15 ohm-cm | Average value: 3.00e+14 ohm-cm Grade Count:4 |
Overview of materials for Nylon 11, Cable Sheathing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Cable Sheathing Grade". Each property range of values reported is minimum and maximum values o.. |
|||
Electrical Resistivity | 2.00e+8 - 1.00e+15 ohm-cm | 2.00e+8 - 1.00e+15 ohm-cm | Average value: 9.97e+13 ohm-cm Grade Count:20 |
Overview of materials for Nylon 12, Extrusion/Tubing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Extrusion/Tubing Grade". Each property range of values reported is minimum and maximum values .. |
|||
Electrical Resistivity | 1000 - 1.00e+15 ohm-cm | 1000 - 1.00e+15 ohm-cm | Average value: 1.99e+14 ohm-cm Grade Count:22 |
Overview of materials for Nylon 12, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite Acetate 105E1R26033 Clear, Trsp Cellulose Acetate Plasticizer 29%. Weight loss on heating = 2.6% per ASTM D 707. Soluble matter loss = 0.4% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite Butyrate 264E0096908 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 22%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite Butyrate 550E4861316 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite Butyrate 565A2R30016 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite Butyrate 576E3720010 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite Propionate 371A2R30009 Natural, Trsp Cellulose Acetate Propionate Plasticizer 9%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite Propionate 376E4000012 Clear, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite Propionate 383A2R30009 Natural, Trsp Cellulose Acetate Propionate Plasticizer 9%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite Propionate 384A4000016 Clear, Trsp Cellulose Acetate Propionate Plasticizer 16%. Weight loss on heating = 1.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite Propionate 358A4000008 Clear, Trsp Cellulose Acetate Propionate Plasticizer 14%. Weight loss on heating = 0.6% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | Minimum |
Ceradyne Ceralloy® 147-31E Sintered Reaction Bonded Silicon Nitride (Si3N4) Ceralloy® 147 Reaction Bonded Silicon Nitride (RBSN) is a high purity grade of silicon nitride. RBSN has excellent thermal shock resistance and outstanding compatibility with non-ferrous molten met.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+15 ohm-cm | 1.00e+11 - 1.00e+15 ohm-cm | Average value: 8.78e+13 ohm-cm Grade Count:6 |
Overview of materials for Nylon 66/6, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, Mineral Reinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | Average value: 7.60e+14 ohm-cm Grade Count:15 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Electrical Resistivity | 500 - 1.00e+15 ohm-cm | 500 - 1.00e+15 ohm-cm | Average value: 5.67e+14 ohm-cm Grade Count:31 |
Overview of materials for Low Density Polyethylene (LDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi.. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
Eastman Tenite Butyrate 581A3720016 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |