Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.50e+16 ohm-cm | 1.50e+16 ohm-cm | Initial Insulation Resistance (50% Relative Humidity) |
Cytec CC-1191 (Conap) Acrylic Dielectric Conformal Coating Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i.. |
|||
Electrical Resistivity | 1.50e+16 ohm-cm | 1.50e+16 ohm-cm | Initial Insulation Resistance (50% Relative Humidity) |
Cytec CE-1170 (Conap) Acrylic Dielectric Conformal Coating Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i.. |
|||
Electrical Resistivity | 1.50e+16 ohm-cm | 1.50e+16 ohm-cm | Initial Insulation Resistance (50% Relative Humidity) |
Cytec CE-1171 (Conap) Acrylic Dielectric Conformal Coating Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i.. |
|||
Electrical Resistivity | >= 1.50e+16 ohm-cm | >= 1.50e+16 ohm-cm | |
Abatron AboCast/AboCure 8109-1 High melting point.Processing: 100/30 pbw; mix at 130-140°C (270 °F); cures in 16 h/120°C (250°F), 10 h/140°C (285°F), 8 h/160°C (320°F), 2 h/ 200°C (390°F).Applications: Heavy duty castin.. |
|||
Electrical Resistivity | >= 1.50e+16 ohm-cm | >= 1.50e+16 ohm-cm | |
Abatron AboCast/AboCure 8109-10 2-part, clear, slow casting/impregnating dielectric compound. Low dielectric constant, good flexibility and thermocycling properties. Abocast 8502-4 is a red (and other colors), filled version.Pro.. |
|||
Electrical Resistivity | >= 1.50e+16 ohm-cm | >= 1.50e+16 ohm-cm | |
Abatron AboCast/AboCure 8109-11 All-purpose, structural dielectric resin. Better thermal and chemical properties than 8109-8, but requires heat cure. Melts at 70-80°C and remains liquid (supercooled) for many hours at RT.Process.. |
|||
Electrical Resistivity | >= 1.50e+16 ohm-cm | >= 1.50e+16 ohm-cm | |
Abatron AboCast/AboCure 8109-12 1-part, contains latent hardener activated by higher temperature. 4-6 month shelf life at 20-25°C (68-77°F). Other versions available with longer shelf lives and cure cycles.Processing: Potlife:.. |
|||
Electrical Resistivity | >= 1.50e+16 ohm-cm | >= 1.50e+16 ohm-cm | |
Abatron AboCast/AboCure 8109-13 Liquid hardener version of AboCast/AboCure 8109-11.Processing: 100/23 pbw; Potlife: 3-5 h/20°C (68°F), 1-3 h/40°C (105°F), 0.5-1 h/60°C (140°F); mix at RT; cures in: 30 mins/60°C (140°F), 45.. |
|||
Electrical Resistivity | >= 1.50e+16 ohm-cm | >= 1.50e+16 ohm-cm | |
Abatron AboCast/AboCure 8109-2 High melting point. Filled version.Processing: 100/10 pbw; 90 minute potlife; mix at 130-140°C (270 °F); cures in 16 h/120°C (250°F), 10 h/140°C (285°F), 8 h/160°C (320°F), 2 h/ 200°C (390°.. |
|||
Electrical Resistivity | >= 1.50e+16 ohm-cm | >= 1.50e+16 ohm-cm | |
Abatron AboCast/AboCure 8109-3 Low viscosity, RT cure. Easy processing.Processing: 100/10 pbw; Potlife: 2.5 h/20°C (68°F), 30 min/40°C (105°F), 15 min/60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 h/60°C (140.. |
|||
Electrical Resistivity | >= 1.50e+16 ohm-cm | >= 1.50e+16 ohm-cm | |
Abatron AboCast/AboCure 8109-4 Safety hardener (minimum toxicity) version of 8109-3.Processing: 100/10 pbw; Potlife: 2.5 h/20°C (68°F), 30 min/40°C (105°F), 15 min/60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 .. |
|||
Electrical Resistivity | >= 1.50e+16 ohm-cm | >= 1.50e+16 ohm-cm | |
Abatron AboCast/AboCure 8109-5 High heat resistance. Easy to use.Processing: 100/20 pbw; Potlife: 7-10 days/20°C (68°F), 5-7h/60°C (140°F); mix at RT; cures in: 4 h/100°C (212°F) + 3 h/190°C (375°F) postcure.Applications.. |
|||
Electrical Resistivity | >= 1.50e+16 ohm-cm | >= 1.50e+16 ohm-cm | |
Abatron AboCast/AboCure 8109-6 High heat resistance. Easy to use.Processing: 100/90 pbw; Potlife: 15-20 days/20°C (68°F), 7-10 h/120°C (250°F); mix at RT; cures in: 3 h/100°C (212°F) + 3 h/190°C (375°F) postcure.Applicat.. |
|||
Electrical Resistivity | >= 1.50e+16 ohm-cm | >= 1.50e+16 ohm-cm | |
Abatron AboCast/AboCure 8109-8 All-purpose, structural dielectric resin. High thermal and chemical resistance and RT cure.Processing: 100/12 ratio; Potlife: 45 min/20°C (68°F), 20 min/40°C (105°F), 10 min /60°C (140°F); mi.. |
|||
Electrical Resistivity | >= 1.50e+16 ohm-cm | >= 1.50e+16 ohm-cm | |
Abatron AboCast/AboCure 8109-9 Minimum toxicity version of 8109-8.Processing: 100/25 ratio; Potlife: 45 min/20°C (68°F), 20 min/40°C (105°F), 10 min /60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 h/60°C (140°.. |
|||
Electrical Resistivity | >= 1.50e+16 ohm-cm | >= 1.50e+16 ohm-cm | |
Abatron AboCast/AboCure 8109-7 Processing: 100/80 pbw; Potlife: 6-7 days/20°C (68°F), 12-24 h/40°C (105°F), 0.75-7 h /60°C (140°F); mix at 50-80°C (120-175°F); cures in: 1 h/100°C (212°F) + 4 h/150°C (300°F) postcure... |