| Category | Polymer , Adhesive , Thermoset , Epoxy | 
| Manufacturer | Abatron | 
| Trade Name | AboCast/AboCure | 
| Port | Shanghai port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Abatron AboCast/AboCure 8109-5.pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 1.22 g/cc | 0.0441 lb/in³ | |
| Water Absorption | 0.20 - 0.25 % | 0.20 - 0.25 % | (60x10X4 mm bar) after 1 hour at 100°C (212°F) | 
| 0.40 - 0.50 % | 0.40 - 0.50 % | (60x10X4 mm bar) after 10 days at 20°C (77°F) | |
| Viscosity |           20 - 30           cP           @Temperature 120 °C  | 
                  20 - 30           cP           @Temperature 248 °F  | 
        |
|           80 - 150           cP           @Temperature 70.0 °C  | 
                  80 - 150           cP           @Temperature 158 °F  | 
        ||
|           1500 - 2500           cP           @Temperature 25.0 °C  | 
                  1500 - 2500           cP           @Temperature 77.0 °F  | 
        ||
| Vapor Pressure | <=           0.0000267           bar           @Temperature 50.0 °C  | 
        <=           0.0200           torr           @Temperature 122 °F  | 
        AboCure | 
| <=           0.00133           bar           @Temperature 180 °C  | 
        <=           1.00           torr           @Temperature 356 °F  | 
        AboCast | |
|           0.00200           bar           @Temperature 100 °C  | 
                  1.50           torr           @Temperature 212 °F  | 
        AboCure | |
|           0.0293           bar           @Temperature 165 °C  | 
                  22.0           torr           @Temperature 329 °F  | 
        AboCure | |
|           0.0667           bar           @Temperature 180 °C  | 
                  50.0           torr           @Temperature 356 °F  | 
        AboCure | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Tensile Strength, Ultimate | 68.95 MPa | 10000 psi | |
| Modulus of Elasticity | 3.447 GPa | 500.0 ksi | |
| Flexural Yield Strength | 137.9 MPa | 20000 psi | |
| Compressive Yield Strength | 137.9 MPa | 20000 psi | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| CTE, linear |           55.0 - 65.0           µm/m-°C           @Temperature 20.0 °C  | 
                  30.6 - 36.1           µin/in-°F           @Temperature 68.0 °F  | 
        |
| Maximum Service Temperature, Air | 180 °C | 356 °F | Deflection temperature; load unknown. | 
| Electrical Properties | Metric | English | Comments | 
|---|---|---|---|
| Electrical Resistivity | >= 1.50e+16 ohm-cm | >= 1.50e+16 ohm-cm | |
| Dielectric Constant |           3.3 - 3.5                     @Frequency 1e+6 Hz  | 
                  3.3 - 3.5                     @Frequency 1e+6 Hz  | 
        |
|           3.6 - 3.8                     @Frequency 1000 Hz  | 
                  3.6 - 3.8                     @Frequency 1000 Hz  | 
        ||
|           3.7 - 3.9                     @Frequency 50 Hz  | 
                  3.7 - 3.9                     @Frequency 50 Hz  | 
        ||
| Dielectric Strength |           13.8 - 17.7           kV/mm           @Thickness 3.17 mm  | 
                  350 - 450           kV/in           @Thickness 0.125 in  | 
        Short time value | 
| Dissipation Factor |           0.0030 - 0.0050                     @Frequency 50 Hz  | 
                  0.0030 - 0.0050                     @Frequency 50 Hz  | 
        |
|           0.0050 - 0.0070                     @Frequency 1000 Hz  | 
                  0.0050 - 0.0070                     @Frequency 1000 Hz  | 
        ||
|           0.015 - 0.025                     @Frequency 1e+6 Hz  | 
                  0.015 - 0.025                     @Frequency 1e+6 Hz  | 
        
| Processing Properties | Metric | English | Comments | 
|---|---|---|---|
| Processing Temperature | 25.0 °C | 77.0 °F | |
| Pot Life |           300 - 420           min           @Temperature 60.0 °C  | 
                  300 - 420           min           @Temperature 140 °F  | 
        |
|           10080 - 14400           min           @Temperature 20.0 °C  | 
                  10080 - 14400           min           @Temperature 68.0 °F  |