Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | >= 1.00e+12 ohm-cm | >= 1.00e+12 ohm-cm | 50% RH; IEC 60093 |
Murtfeldt Murdopol® Nylon 12 Murdopol® has extremely high shock and impact resistance characteristics and good emergency running characteristics thanks to its high wear resistance. The main advantage of this material is its f.. |
|||
Electrical Resistivity | 1.00e+12 - 3.00e+16 ohm-cm | 1.00e+12 - 3.00e+16 ohm-cm | Average value: 1.14e+16 ohm-cm Grade Count:14 |
Overview of materials for Polyetherimide (PEI), 30% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 30% Glass Fiber". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
Plenco 501 Black Electrical Grade Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 501 is a two-stage, mineral and flock-filled phenolic molding compound designed for use in heat resistant and electrical applications. It is designed for elevated temperature exposure for e.. |
|||
Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
Plenco 304 Black Impact Grade Woodflour/Cellulose Filled Phenolic Molding Compound
(discontinued **) Plaslok 304 is a two-stage, woodflour and cellulose-filled phenolic molding compound having improved impact strength. It is suitable for automatic molding, and is recommended for thin-walled parts .. |
|||
Electrical Resistivity | 1.00e+12 - 1.00e+14 ohm-cm | 1.00e+12 - 1.00e+14 ohm-cm | Average value: 5.05e+13 ohm-cm Grade Count:6 |
Overview of materials for Nylon 63, 35% Glass-Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 63, 35% Glass-Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
Plaslok 201 Black General Purpose Woodflour/Mineral Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 201 is a two-stage, woodflour and min.. |
|||
Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
Plaslok 202 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 202 is a two-stage, woodflour-filled .. |
|||
Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
Plaslok 301 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 301 is a two-stage, woodflour and flo.. |
|||
Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
Sumitomo Bakelite Durez® 23570 Phenolic, Injection Grade Durez 23570 Black Phenolic is a glass and mineral filled two-stage, special purpose molding material. It is designed for high strength, good dimensional stability, and electrical properties even aft.. |
|||
Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
Sumitomo Bakelite Durez® 31735 Phenolic, Injection Grade Durez 31735 is a special purpose phenolic molding compound developed for automotive and industrial pulleys. This material is designed to optimize pulley performance relating to belt life, dimension.. |
|||
Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | |
Goodfellow Potassium Aluminosilicate (Muscovite Mica) Mica is a naturally occurring mineral and as such its exact composition varies between grades, as will its properties. Ruby Mica is the highest grade of Muscovite Mica. The name comes from the Latin.. |
|||
Electrical Resistivity | 1.00e+12 ohm-cm @Temperature 25.0 °C |
1.00e+12 ohm-cm @Temperature 77.0 °F |
|
Goodfellow Shapal™-M soft Aluminum Nitride (AlN) - Machinable Shapal-M® soft is a high purity, machinable ceramic with high strength and high thermal conductivity. Although the thermal conductivity is not as high as Aluminum Nitride, it is still 50 times that.. |
|||
Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | |
Arkema Group Rilsan® AESN P20 TL Nylon 12, Flexible Grade (Conditioned) Designation ISO 1874-PA12-P,EHL,22-005Flexible grade for overmolding. Available colors: natural and white. Light and heat stabilized. No lubricant.Flexibility. Very good ability to overmold Pebax an.. |
|||
Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | |
Arkema Group Rilsan® AZM 43 G9 T6LD Nylon 12, 43% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLS,16-080,(G+C)(F+D)(43+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab.. |
|||
Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | IEC 60093 |
CENTROPLAST CENTROMID 12 soft Polyamide 12 soft This extruded material is suitable for conveying foodstuffs and pharmaceutical products. It is used in flexible tubes for worm gears and spiral conveyors.Information provided by CENTROPLAST Enginee.. |
|||
Electrical Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
Toyobo Pelprene™ P-30B Polyester TPE Key Feature: Pelprene P typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'P' type is a block.. |
|||
Electrical Resistivity | 1.00e+12 - 1.00e+15 ohm-cm | 1.00e+12 - 1.00e+15 ohm-cm | Average value: 2.00e+14 ohm-cm Grade Count:12 |
Overview of materials for Nylon 6, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Electrical Resistivity | 1.00e+12 - 1.00e+15 ohm-cm | 1.00e+12 - 1.00e+15 ohm-cm | Average value: 3.52e+14 ohm-cm Grade Count:19 |
Overview of materials for Polyether Ester Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr.. |
|||
Electrical Resistivity | 1.00e+12 - 2.00e+16 ohm-cm | 1.00e+12 - 2.00e+16 ohm-cm | Average value: 8.00e+15 ohm-cm Grade Count:15 |
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% .. |
|||
Electrical Resistivity | 1.00e+12 - 1.00e+16 ohm-cm | 1.00e+12 - 1.00e+16 ohm-cm | Average value: 1.48e+15 ohm-cm Grade Count:15 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |