Goodfellow Shapal™-M soft Aluminum Nitride (AlN) - Machinable

Category Ceramic , Machinable Ceramic , Nitride
Manufacturer Goodfellow
Trade Name Shapal™-M soft
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Goodfellow Shapal™-M soft Aluminum Nitride (AlN) - Machinable.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Shapal-M® soft is a high purity, machinable ceramic with high strength and high thermal conductivity. Although the thermal conductivity is not as high as Aluminum Nitride, it is still 50 times that of machinable glass ceramic. Like aluminum nitride, applications include heat sinks and electronically insulating components for the high power electronic industry, and crucibles for molten metals. Shapal-M® also has the advantage that much more complex shapes may be used. It may be machined by using carbide tools and is resistant to acids and bases.Information provided by Goodfellow. SHAPAL™-M is a trademark of Tokuyama Corporation.
Physical Properties Metric English Comments
Density 2.95 g/cc
0.107 lb/in³
Porosity 0.00 %
0.00 %
Apparent Porosity
Mechanical Properties Metric English Comments
Vickers Microhardness 390

@Load 0.300 kg
390

@Load 0.662 lb
kg/mm²
Tensile Modulus 186 GPa
27000 ksi
Flexural Strength 294 MPa
42600 psi
Compressive Strength 1180 MPa
171000 psi
Poissons Ratio 0.31
0.31
Shear Modulus 71.0 GPa
10300 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 4.40 µm/m-°C

@Temperature 20.0 - 400 °C
2.44 µin/in-°F

@Temperature 68.0 - 752 °F
4.80 µm/m-°C

@Temperature 20.0 - 600 °C
2.67 µin/in-°F

@Temperature 68.0 - 1110 °F
5.10 µm/m-°C

@Temperature 20.0 - 800 °C
2.83 µin/in-°F

@Temperature 68.0 - 1470 °F
Thermal Conductivity 80.0 W/m-K

@Temperature 200 °C
555 BTU-in/hr-ft²-°F

@Temperature 392 °F
86.0 W/m-K

@Temperature 100 °C
597 BTU-in/hr-ft²-°F

@Temperature 212 °F
90.0 W/m-K

@Temperature 25.0 °C
625 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
Maximum Service Temperature, Air 1000 °C
1830 °F
Maximum Service Temperature, Inert 1900 °C
3450 °F
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+12 ohm-cm

@Temperature 25.0 °C
1.00e+12 ohm-cm

@Temperature 77.0 °F
Dielectric Constant 7.1

@Frequency 1.00e+6 Hz
7.1

@Frequency 1.00e+6 Hz
Dielectric Strength 40.0 kV/mm
1020 kV/in
Dissipation Factor 0.0010

@Frequency 1.00e+6 Hz
0.0010

@Frequency 1.00e+6 Hz
Descriptive Properties Value Comments
Acid Resistance 0.2 mg/cm² wt. loss
10% HCl (24 hrs.; 25°C)
Alkali Resistance 60 mg/cm² wt. loss
10% NaOH (24 hrs.; 25°C)
Thermal Shock Resistance (ΔT) 400°C
Water Quench