Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+15 - 1.00e+16 ohm-cm | 1.00e+15 - 1.00e+16 ohm-cm | |
3M Dyneon™ Aflas® FA-150E PTFE Fluoroelastomer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 57%F in polymer with 19% Medium Thermal Carbon Black (N990), 4% Triallyl Isocyanurate (TAIC), 1% Percadox™ 14, 1% Sodium.. |
|||
Electrical Resistivity | 1000 - 1.00e+16 ohm-cm | 1000 - 1.00e+16 ohm-cm | Average value: 1.81e+15 ohm-cm Grade Count:19 |
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are.. |
|||
Electrical Resistivity | 0.100 - 1.00e+16 ohm-cm | 0.100 - 1.00e+16 ohm-cm | Average value: 7.69e+15 ohm-cm Grade Count:13 |
Overview of materials for Styrenic TPE
(Unverified Data**) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic TPE". Each property range of values reported is minimum and maximum values of appropriate MatWe.. |
|||
Electrical Resistivity | 0.200 - 1.00e+16 ohm-cm | 0.200 - 1.00e+16 ohm-cm | Average value: 1.73e+15 ohm-cm Grade Count:175 |
Overview of materials for Acetal Copolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | Average value: 4.42e+15 ohm-cm Grade Count:5 |
Overview of materials for Acetal Copolymer, Silicone Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values.. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | Average value: 1.51e+15 ohm-cm Grade Count:7 |
Overview of materials for Acetal Copolymer, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Electrical Resistivity | 1.00 - 1.00e+16 ohm-cm | 1.00 - 1.00e+16 ohm-cm | Average value: 8.33e+14 ohm-cm Grade Count:14 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Electrical Resistivity | 1.00e+15 - 1.00e+16 ohm-cm | 1.00e+15 - 1.00e+16 ohm-cm | Average value: 7.75e+15 ohm-cm Grade Count:4 |
Overview of materials for ABS/Polyester Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Electrical Resistivity | 1.00e+12 - 1.00e+16 ohm-cm | 1.00e+12 - 1.00e+16 ohm-cm | Average value: 2.42e+15 ohm-cm Grade Count:11 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
Electrical Resistivity | 1.00e+15 - 1.00e+16 ohm-cm | 1.00e+15 - 1.00e+16 ohm-cm | Average value: 2.90e+15 ohm-cm Grade Count:10 |
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Electrical Resistivity | 0.0500 - 1.00e+16 ohm-cm | 0.0500 - 1.00e+16 ohm-cm | Average value: 8.93e+14 ohm-cm Grade Count:7 |
Overview of materials for Silicone, Molded, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | Average value: 2.80e+15 ohm-cm Grade Count:4 |
Overview of materials for Polyphenylene Sulfide (PPS) with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with PTFE Filler". Each property range of values reported is minimum and max.. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | |
Kraton® D1102 (SBS) Linear Block Copolymer (SBS) styrene-butadiene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact .. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | |
Kraton® D1116 (SB)n Branched Copolymer (SB)n - styrene-butadiene multi-arm (branched) copolymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve .. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | |
Kraton® D4141 (SBS) Linear Block Copolymer (SBS) styrene-butadiene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact .. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | |
Kraton® D1101 (SBS) Linear Block Copolymer (SBS) styrene-butadiene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact .. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | |
Kraton® D1112P (SIS) Linear Block Copolymer (SIS) styrene-isoprene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact q.. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | Average value: 1.52e+15 ohm-cm Grade Count:64 |
Overview of materials for Nylon 66, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | Average value: 2.51e+15 ohm-cm Grade Count:20 |
Overview of materials for Nylon 66, Glass Fiber/MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/MoS2 Filled". Each property range of values reported is minimum and maximum values.. |
|||
Electrical Resistivity | 1000 - 1.00e+16 ohm-cm | 1000 - 1.00e+16 ohm-cm | Average value: 7.38e+15 ohm-cm Grade Count:53 |
Overview of materials for Polycarbonate, Glass + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | Average value: 8.35e+15 ohm-cm Grade Count:6 |
Overview of materials for Polyetherimide (PEI), Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Aramid Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | Average value: 8.35e+15 ohm-cm Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is .. |
|||
Electrical Resistivity | 3.00e+13 - 1.00e+16 ohm-cm | 3.00e+13 - 1.00e+16 ohm-cm | Average value: 3.00e+15 ohm-cm Grade Count:12 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |
|||
Electrical Resistivity | 1.00e+13 - 1.00e+16 ohm-cm | 1.00e+13 - 1.00e+16 ohm-cm | Average value: 5.77e+15 ohm-cm Grade Count:12 |
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% .. |
|||
Electrical Resistivity | 1.00e+12 - 1.00e+16 ohm-cm | 1.00e+12 - 1.00e+16 ohm-cm | Average value: 4.72e+15 ohm-cm Grade Count:10 |
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc.. |
|||
Electrical Resistivity | 1.00e+12 - 1.00e+16 ohm-cm | 1.00e+12 - 1.00e+16 ohm-cm | Average value: 3.34e+15 ohm-cm Grade Count:3 |
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc.. |
|||
Electrical Resistivity | 4.00e+14 - 1.00e+16 ohm-cm | 4.00e+14 - 1.00e+16 ohm-cm | Average value: 5.43e+15 ohm-cm Grade Count:7 |
Overview of materials for Polyphthalamide (PPA), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Electrical Resistivity | 25.0 - 1.00e+16 ohm-cm | 25.0 - 1.00e+16 ohm-cm | Average value: 2.95e+15 ohm-cm Grade Count:4 |
Overview of materials for Ethylene Butyl Acrylate This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Butyl Acrylate". Each property range of values reported is minimum and maximum values of approp.. |
|||
Electrical Resistivity | 100 - 1.00e+16 ohm-cm | 100 - 1.00e+16 ohm-cm | Average value: 5.17e+15 ohm-cm Grade Count:6 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |