Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 10.0 - 1.00e+17 ohm-cm | 10.0 - 1.00e+17 ohm-cm | Average value: 1.60e+16 ohm-cm Grade Count:30 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |
|||
Electrical Resistivity | 10.0 - 1.00e+15 ohm-cm | 10.0 - 1.00e+15 ohm-cm | Average value: 4.60e+14 ohm-cm Grade Count:89 |
Overview of materials for Nylon 66, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Electrical Resistivity | 10.0 - 7.80e+14 ohm-cm | 10.0 - 7.80e+14 ohm-cm | Average value: 7.09e+13 ohm-cm Grade Count:12 |
Overview of materials for Nylon 12, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Electrical Resistivity | 10.0 - 100 ohm-cm | 10.0 - 100 ohm-cm | ASTM C611 |
Techmer ES Electrafil® J-50/CF/30 Polycarbonate, 30% Carbon Fiber Reinforced Carbon Fiber Reinforced |
|||
Electrical Resistivity | 10.0 - 100 ohm-cm | 10.0 - 100 ohm-cm | ASTM C611 |
Techmer ES Electrafil® J-50/CF/30/TF/15 Polycarbonate, 30% Carbon Fiber Reinforced, PTFE Lubed Carbon Fiber Reinforced, PTFE Lubricated |
|||
Electrical Resistivity | 10.0 - 100 ohm-cm | 10.0 - 100 ohm-cm | ASTM C611 |
Techmer ES Electrafil® J-1200/CF/10 ABS, 10% Carbon Fiber Reinforced |
|||
Electrical Resistivity | >= 10.0 ohm-cm | >= 10.0 ohm-cm | ASTM D257 |
Plastic Lumber from the Plastic Lumber Co. Description: Plastic Lumber is a product similar to wood that is made from recycled plastic jugs. Products will never splinter, rot, crumble or need painting. Plastic Lumber has rapidly gained accep.. |
|||
Electrical Resistivity | 10.0 ohm-cm | 10.0 ohm-cm | |
Ceradyne Ceralloy® 546-3E Boron Carbide Features:low porosityhigh puritysingle phaseApplications:semiconductor componentsInformation provided by Ceradyne Company |
|||
Electrical Resistivity | 10.0 ohm-cm | 10.0 ohm-cm | |
Ceradyne Ceralloy® 546-4E Boron Carbide Features:neutron absorptionwear resistancehardnesslightweightApplications:semiconductor componentswear componentsballistic armorsputtering targetsnuclear shieldingInformation provided by Ceradyne Co.. |
|||
Electrical Resistivity | 10.0 ohm-cm | 10.0 ohm-cm | |
Ceradyne CeraTrex™ SC-P2 Silicon Carbide Features:purity>99.9995%corrosion resistancewear resistancenear net shape fabrication to 400 mm OD Applications:semiconductor componentswear componentsInformation provided by Ceradyne Company |
|||
Electrical Resistivity | 10.0 - 100 ohm-cm | 10.0 - 100 ohm-cm | |
A. Schulman ComAlloy E-17099B Nylon 6/6, Electrically Conductive - Carbon Fiber Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Electrical Resistivity | 10.0 ohm-cm | 10.0 ohm-cm | |
Ceradyne Ceralloy® 546 Boron Carbide Features:neutron absorptionwear resistancehardnesslightweightApplications:semiconductor componentswear componentsballistic armorsputtering targetsnuclear shieldingInformation provided by Ceradyne Co.. |
|||
Electrical Resistivity | 10.0 - 3.80e+17 ohm-cm | 10.0 - 3.80e+17 ohm-cm | Average value: 2.29e+16 ohm-cm Grade Count:43 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |
|||
Electrical Resistivity | 10.0 - 1.00e+9 ohm-cm | 10.0 - 1.00e+9 ohm-cm | Average value: 5.67e+7 ohm-cm Grade Count:19 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu.. |