Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.000122 ohm-cm | 0.000122 ohm-cm | RT |
Haynes 242® alloy, cold reduced sheet, annealed, 20% cold work Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Electrical Resistivity | 0.000122 ohm-cm | 0.000122 ohm-cm | RT |
Haynes 242® alloy Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Electrical Resistivity | 0.000122 ohm-cm | 0.000122 ohm-cm | RT |
Haynes 242® alloy, after 1000 hours exposure at 650°C (1200°F) Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Electrical Resistivity | 0.000122 ohm-cm | 0.000122 ohm-cm | RT |
Haynes 242® alloy, after 4000 hours exposure at 650°C (1200°F) Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Electrical Resistivity | 0.000122 ohm-cm | 0.000122 ohm-cm | RT |
Haynes 242® alloy, cold reduced sheet, annealed Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Electrical Resistivity | 0.000122 ohm-cm | 0.000122 ohm-cm | RT |
Haynes 242® alloy, cold reduced sheet, annealed and 20% cold work Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Electrical Resistivity | 0.000122 ohm-cm | 0.000122 ohm-cm | RT |
Haynes 242® alloy, cold reduced sheet, annealed and 40% cold work Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Electrical Resistivity | 0.000122 ohm-cm | 0.000122 ohm-cm | RT |
Haynes 242® alloy, cold reduced sheet, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Electrical Resistivity | 0.000122 ohm-cm | 0.000122 ohm-cm | RT |
Haynes 242® alloy, cold reduced sheet, annealed, 40% cold work, aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Electrical Resistivity | 0.000122 ohm-cm | 0.000122 ohm-cm | RT |
Haynes 242® alloy, cold rolled sheet, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Electrical Resistivity | 0.000122 ohm-cm @Temperature 400 °C |
0.000122 ohm-cm @Temperature 752 °F |
|
Haynes 263® alloy, cold rolled sheet, solution treated and aged Very good aged strength properties, excellent fabrication characteristics when annealed, excellent intermediate temperature tensile ductility, is not normally subject to strain age cracking, excelle.. |
|||
Electrical Resistivity | 0.000122 ohm-cm @Temperature 100 °C |
0.000122 ohm-cm @Temperature 212 °F |
|
Haynes 718 alloy, cold rolled, solution-treated and aged sheet Cb and Ta content combined weight percentage of 5. Excellent high-temperature strength up to 650°C, good ductility, formability, and weldability. Very good welding characteristics. Applications i.. |
|||
Electrical Resistivity | 0.000122 ohm-cm | 0.000122 ohm-cm | |
Special Metals INCONEL® Alloy 617 A nickel-chromium-cobalt-molybdenum alloy with an exceptional combination of metallurgical stability, strength, and oxidation resistance at high temperatures. Resistance to oxidation is enhanced by.. |
|||
Electrical Resistivity | 0.000122 ohm-cm | 0.000122 ohm-cm | |
Special Metals INCONEL® Alloy 751 A nickel-chromium alloy similar to INCONEL ALLOY X-750 but with increased aluminum content for greater precipitation hardening. INCONEL alloy 751 was designed for use as exhaust valves in internal-.. |
|||
Electrical Resistivity | 0.000122 ohm-cm | 0.000122 ohm-cm | |
Special Metals INCONEL® Alloy X-750 A nickel-chromium alloy similar to INCONEL alloy 600 but made precipitation hardenable by additions of aluminum and titanium. The alloy has good resistance to corrosion and oxidation along with hig.. |
|||
Electrical Resistivity | 0.000122 ohm-cm @Temperature 20.0 °C |
0.000122 ohm-cm @Temperature 68.0 °F |
|
Alloy Wire International RW 122 Hot Cutting Wire - High Strength Maintains high strength at elevated temperatures. Used for cutting expanded polystyrene (EPS) foam and for the heat sealing of polypropylene bags.Information provided by Alloywire International. |
|||
Electrical Resistivity | 0.000122 ohm-cm | 0.000122 ohm-cm | RT |
Haynes 242® alloy, hot rolled plate, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good thermal.. |
|||
Electrical Resistivity | 0.000122 ohm-cm @Temperature 600 °C |
0.000122 ohm-cm @Temperature 1110 °F |
|
Special Metals INCOLOY® Alloy 903 A nickel-iron-cobalt alloy with additions of niobium, titanium, and aluminum for precipitation hardening. The alloy combines high strength with a low and constant coefficient of thermal expansion a.. |