| Category | Metal , Superalloy , Iron Base |
| Manufacturer | Special Metals (includes the former Inco Alloys International Inc.) |
| Trade Name | INCOLOY® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Special Metals INCOLOY® Alloy 903.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 8.25 g/cc | 0.298 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 1310 MPa | 190000 psi | Precipitation Hardened |
| Tensile Strength, Yield | 1100 MPa <br>@Strain 0.200 % |
160000 psi <br>@Strain 0.200 % |
Precipitation Hardened |
| Elongation at Break | 14 % | 14 % | Precipitation Hardened |
| Modulus of Elasticity | 146.8 GPa <br>@Temperature 0.000 °C |
21290 ksi <br>@Temperature 32.0 °F |
|
| 146.9 GPa <br>@Temperature -50.0 °C |
21310 ksi <br>@Temperature -58.0 °F |
||
| 146.9 GPa <br>@Temperature 50.0 °C |
21310 ksi <br>@Temperature 122 °F |
||
| 147.2 GPa <br>@Temperature 100 °C |
21350 ksi <br>@Temperature 212 °F |
||
| 147.4 GPa <br>@Temperature -100 °C |
21380 ksi <br>@Temperature -148 °F |
||
| 147.8 GPa <br>@Temperature 150 °C |
21440 ksi <br>@Temperature 302 °F |
||
| 148.4 GPa <br>@Temperature 200 °C |
21520 ksi <br>@Temperature 392 °F |
||
| 148.9 GPa <br>@Temperature -195 °C |
21600 ksi <br>@Temperature -319 °F |
||
| 149.3 GPa <br>@Temperature 250 °C |
21650 ksi <br>@Temperature 482 °F |
||
| 149.8 GPa <br>@Temperature 600 °C |
21730 ksi <br>@Temperature 1110 °F |
||
| 150.2 GPa <br>@Temperature 300 °C |
21790 ksi <br>@Temperature 572 °F |
||
| 151.3 GPa <br>@Temperature 350 °C |
21940 ksi <br>@Temperature 662 °F |
||
| 151.8 GPa <br>@Temperature 550 °C |
22020 ksi <br>@Temperature 1020 °F |
||
| 152.4 GPa <br>@Temperature 400 °C |
22100 ksi <br>@Temperature 752 °F |
||
| 153.5 GPa <br>@Temperature 450 °C |
22260 ksi <br>@Temperature 842 °F |
||
| 153.9 GPa <br>@Temperature 500 °C |
22320 ksi <br>@Temperature 932 °F |
||
| Poissons Ratio | 0.226 <br>@Temperature 250 °C |
0.226 <br>@Temperature 482 °F |
|
| 0.227 <br>@Temperature 300 °C |
0.227 <br>@Temperature 572 °F |
||
| 0.231 <br>@Temperature 200 °C |
0.231 <br>@Temperature 392 °F |
||
| 0.236 <br>@Temperature 350 °C |
0.236 <br>@Temperature 662 °F |
||
| 0.239 <br>@Temperature 50.0 °C |
0.239 <br>@Temperature 122 °F |
||
| 0.241 <br>@Temperature 400 °C |
0.241 <br>@Temperature 752 °F |
||
| 0.242 <br>@Temperature 150 °C |
0.242 <br>@Temperature 302 °F |
||
| 0.247 <br>@Temperature 100 °C |
0.247 <br>@Temperature 212 °F |
||
| 0.273 <br>@Temperature 450 °C |
0.273 <br>@Temperature 842 °F |
||
| 0.30 <br>@Temperature 500 °C |
0.30 <br>@Temperature 932 °F |
||
| 0.318 <br>@Temperature 550 °C |
0.318 <br>@Temperature 1020 °F |
||
| 0.352 <br>@Temperature 600 °C |
0.352 <br>@Temperature 1110 °F |
||
| Shear Modulus | 55.4 GPa <br>@Temperature 600 °C |
8040 ksi <br>@Temperature 1110 °F |
|
| 57.6 GPa <br>@Temperature 550 °C |
8350 ksi <br>@Temperature 1020 °F |
||
| 59.0 GPa <br>@Temperature 100 °C |
8560 ksi <br>@Temperature 212 °F |
||
| 59.2 GPa <br>@Temperature 500 °C |
8590 ksi <br>@Temperature 932 °F |
||
| 59.3 GPa <br>@Temperature 50.0 °C |
8600 ksi <br>@Temperature 122 °F |
||
| 59.5 GPa <br>@Temperature 150 °C |
8630 ksi <br>@Temperature 302 °F |
||
| 60.3 GPa <br>@Temperature 200 °C |
8750 ksi <br>@Temperature 392 °F |
||
| 60.3 GPa <br>@Temperature 450 °C |
8750 ksi <br>@Temperature 842 °F |
||
| 60.9 GPa <br>@Temperature 250 °C |
8830 ksi <br>@Temperature 482 °F |
||
| 61.2 GPa <br>@Temperature 300 °C |
8880 ksi <br>@Temperature 572 °F |
||
| 61.2 GPa <br>@Temperature 350 °C |
8880 ksi <br>@Temperature 662 °F |
||
| 61.4 GPa <br>@Temperature 400 °C |
8910 ksi <br>@Temperature 752 °F |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 7.65 µm/m-°C <br>@Temperature 25.0 - 427 °C |
4.25 µin/in-°F <br>@Temperature 77.0 - 801 °F |
|
| Specific Heat Capacity | 0.435 J/g-°C | 0.104 BTU/lb-°F | test temperature not reported |
| 0.442 J/g-°C <br>@Temperature 50.0 °C |
0.106 BTU/lb-°F <br>@Temperature 122 °F |
||
| 0.454 J/g-°C <br>@Temperature 100 °C |
0.109 BTU/lb-°F <br>@Temperature 212 °F |
||
| 0.482 J/g-°C <br>@Temperature 200 °C |
0.115 BTU/lb-°F <br>@Temperature 392 °F |
||
| 0.507 J/g-°C <br>@Temperature 300 °C |
0.121 BTU/lb-°F <br>@Temperature 572 °F |
||
| 0.532 J/g-°C <br>@Temperature 400 °C |
0.127 BTU/lb-°F <br>@Temperature 752 °F |
||
| 0.559 J/g-°C <br>@Temperature 500 °C |
0.134 BTU/lb-°F <br>@Temperature 932 °F |
||
| 0.584 J/g-°C <br>@Temperature 600 °C |
0.140 BTU/lb-°F <br>@Temperature 1110 °F |
||
| Thermal Conductivity | 16.7 W/m-K | 116 BTU-in/hr-ft²-°F | test temperature unknown |
| 16.9 W/m-K <br>@Temperature 50.0 °C |
117 BTU-in/hr-ft²-°F <br>@Temperature 122 °F |
||
| 17.2 W/m-K <br>@Temperature 100 °C |
119 BTU-in/hr-ft²-°F <br>@Temperature 212 °F |
||
| 17.9 W/m-K <br>@Temperature 200 °C |
124 BTU-in/hr-ft²-°F <br>@Temperature 392 °F |
||
| 18.3 W/m-K <br>@Temperature 300 °C |
127 BTU-in/hr-ft²-°F <br>@Temperature 572 °F |
||
| 19.0 W/m-K <br>@Temperature 400 °C |
132 BTU-in/hr-ft²-°F <br>@Temperature 752 °F |
||
| 20.3 W/m-K <br>@Temperature 500 °C |
141 BTU-in/hr-ft²-°F <br>@Temperature 932 °F |
||
| 21.9 W/m-K <br>@Temperature 600 °C |
152 BTU-in/hr-ft²-°F <br>@Temperature 1110 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 0.0000610 ohm-cm | 0.0000610 ohm-cm | |
| 0.0000650 ohm-cm <br>@Temperature 50.0 °C |
0.0000650 ohm-cm <br>@Temperature 122 °F |
||
| 0.0000735 ohm-cm <br>@Temperature 100 °C |
0.0000735 ohm-cm <br>@Temperature 212 °F |
||
| 0.0000880 ohm-cm <br>@Temperature 200 °C |
0.0000880 ohm-cm <br>@Temperature 392 °F |
||
| 0.000102 ohm-cm <br>@Temperature 300 °C |
0.000102 ohm-cm <br>@Temperature 572 °F |
||
| 0.0001135 ohm-cm <br>@Temperature 400 °C |
0.0001135 ohm-cm <br>@Temperature 752 °F |
||
| 0.0001195 ohm-cm <br>@Temperature 500 °C |
0.0001195 ohm-cm <br>@Temperature 932 °F |
||
| 0.000122 ohm-cm <br>@Temperature 600 °C |
0.000122 ohm-cm <br>@Temperature 1110 °F |
||
| Curie Temperature | 415 - 470 °C | 779 - 878 °F |