Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 3.00 mm |
30 - 60 sec @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-FR3-D Polycarbonate, Improved Flame Retardant, High Flow Polycarbonate, Improved Flame Retardant, High FlowFeatures: • High Impact Resistance • Self Extinguishing • Low ViscosityProcess: Injection MoldingNotes: All physical, mechanical and thermal t.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 1.50 mm |
30 - 60 sec @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-GP3-D Polycarbonate, General Purpose, High Flow Polycarbonate, General Purpose, High FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inc.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 1.50 mm |
30 - 60 sec @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-HM-FR1-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 3.00 mm |
30 - 60 sec @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-UV1-D-[color]-1 Polycarbonate, UV-stabilized, Low Flow with Mold Release Polycarbonate, UV-stabilized, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 1.50 mm |
30 - 60 sec @Thickness 0.0591 in |
UL 746 |
Polymer Resources TP-G30 Polybutylene Terephthalate, 30% Glass Reinforced Polybutylene Terephthalate, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 3.00 mm |
30 - 60 sec @Thickness 0.118 in |
PLC 2 |
PTS PCA-2201NH Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 3.00 mm |
30 - 60 sec @Thickness 0.118 in |
PLC 2 |
PTS Tristar® PC-10R-(V15) 15 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 3.00 mm |
30 - 60 sec @Thickness 0.118 in |
PLC 2 |
PTS Tristar® PC-10R-(VE) 12 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 3.00 mm |
30 - 60 sec @Thickness 0.118 in |
PLC 2 |
PTS Tristar® PC-10R-CL(V22) 22 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 1.50 mm |
30 - 60 sec @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-FR1-D-[color]-3 Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples... |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 3.00 mm |
30 - 60 sec @Thickness 0.118 in |
PLC 2 |
PTS Tristar® PC-10FR-(8) 8 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 3.00 mm |
30 - 60 sec @Thickness 0.118 in |
PLC 2 |
PTS Tristar® PC-10FR-(V18) 18 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 3.00 mm |
30 - 60 sec @Thickness 0.118 in |
PLC 2 |
PTS Tristar® PC-10R-(V22) 22 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 3.00 mm |
30 - 60 sec @Thickness 0.118 in |
PLC 2 |
PTS Tristar® PC-10R-CL 10 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=3.00 mm |
30 - 60 sec @Thickness >=0.118 in |
|
LG Chemical KEYFLEX BT 1040D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=3.00 mm |
30 - 60 sec @Thickness >=0.118 in |
|
LG Chemical LUMAX GP5106FI PBT+ABS+GF10%, Flame Retardant Description: Injection Molding Grade, PBT+ABS+GF10%, Flame Retardant, Impact Modified, Dimensional StabilityApplication: E&E (Switch)CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 an.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=1.50 mm |
30 - 60 sec @Thickness >=0.0591 in |
|
LG Chemical Lupox® GP2306FC PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=1.50 mm |
30 - 60 sec @Thickness >=0.0591 in |
|
LG Chemical Lupox® GP2306FI PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant, High Impact Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=1.00 mm |
30 - 60 sec @Thickness >=0.0394 in |
|
LG Chemical Lupox® TE5006F PET+PC Description: Injection Molding, PET+PC, Flame Retardant, GWIT, CTIApplication: IT/OA, E&E (Connector)CAS No. 68928-70-1, 103598-77-2, 25038-59-9 and 1309-64-4Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=1.50 mm |
30 - 60 sec @Thickness >=0.0591 in |
|
LG Chemical Lupoy 1301V-10 Polycarbonate Resin Description: LUPOY PC 1301V-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=1.60 mm |
30 - 60 sec @Thickness >=0.0630 in |
|
LG Chemical Lupoy 1302-05 Polycarbonate Resin Description: LUPOY 1302-5 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=3.00 mm |
30 - 60 sec @Thickness >=0.118 in |
|
LG Chemical Lupoy 1302-07 Polycarbonate Resin Description: LUPOY PC 1302-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=1.50 mm |
30 - 60 sec @Thickness >=0.0591 in |
|
LG Chemical Lupoy 1303EP-22 Polycarbonate Resin Description: LUPOY PC 1303EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=3.00 mm |
30 - 60 sec @Thickness >=0.118 in |
|
LG Chemical LUPOY GP5008BF FR PC/ABS, Flame Retardance, Heat Resistance Description: Injection Molding, PC/ABS, Flame Retardance, Heat ResistanceApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1 and 1309-64-4Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=3.00 mm |
30 - 60 sec @Thickness >=0.118 in |
|
LG Chemical ER461 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=3.00 mm |
30 - 60 sec @Thickness >=0.118 in |
|
LG Chemical Lupoy 1302HP-22 Polycarbonate Resin Description: LUPOY PC 1302HP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=2.50 mm |
30 - 60 sec @Thickness >=0.0984 in |
|
LG Chemical LUPOY GN5001RF PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Good FlowApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=1.50 mm |
30 - 60 sec @Thickness >=0.0591 in |
|
LG Chemical LUPOY GP1000MU PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, UV StabilityApplication: IT/OA Housing and Components, Automotive Exterior and InteriorCAS: 103598-77-2Information provided by LG C.. |
|||
Hot Wire Ignition, HWI | 30 - 59 sec @Thickness 3.00 mm |
30 - 59 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® ECO366 Nylon 66, Flame-retardant, DAM Vydyne® ECO366 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for machin.. |
|||
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=2.50 mm |
30 - 60 sec @Thickness >=0.0984 in |
|
LG Chemical Lupoy 1302HP-07 Polycarbonate Resin Description: LUPOY PC 1302HP-07 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics.. |