Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 1.50 mm |
7.0 - 14 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 1.50 mm |
7.0 - 14 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 1.50 mm |
7.0 - 14 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 3.00 mm |
7.0 - 14 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R513H Black Nylon 66, 13% Glass Reinforced, DAM Vydyne® R513H Black is general-purpose, 13% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is an injection-molding grade that is lubricated for machine feed, flow, and m.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.750 mm |
7.0 - 14 sec @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 3.00 mm |
7.0 - 14 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 3.00 mm |
7.0 - 14 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R525H BK0201 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BK0201 is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.750 mm |
7.0 - 14 sec @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R525H Nylon 66, 25% Glass Filled, Dry as Molded Vydyne® R525H is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties whe.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 3.00 mm |
7.0 - 14 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R525H Nylon 66, 25% Glass Filled, Dry as Molded Vydyne® R525H is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties whe.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.750 mm |
7.0 - 14 sec @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R530H BK0201 Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H BK0201 is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the retention of p.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.750 mm |
7.0 - 14 sec @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R533 NT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533 NT is general-purpose, 33% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade that is lubricated for good machine feed, flow and mold release. Gl.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 1.50 mm |
7.0 - 14 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R533 NT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533 NT is general-purpose, 33% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade that is lubricated for good machine feed, flow and mold release. Gl.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 3.00 mm |
7.0 - 14 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R533 NT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533 NT is general-purpose, 33% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade that is lubricated for good machine feed, flow and mold release. Gl.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 3.00 mm |
7.0 - 14 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R533H NT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H NT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties .. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.750 mm |
7.0 - 14 sec @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R533H01 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H01 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties whe.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.750 mm |
7.0 - 14 sec @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R540 Nylon 66, 40% Glass Reinforced, DAM Vydyne® R540 is general-purpose, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 3.00 mm |
7.0 - 14 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R540H Nylon 66, 40% Glass Reinforced, DAM Vydyne® R540H is general-purpose, heat-stabilized, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 1.50 mm |
7.0 - 14 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, DAM Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 3.00 mm |
7.0 - 14 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R543H BK02 Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H BK02 is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 3.00 mm |
7.0 - 14 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R550 Nylon 66, 50% Glass Reinforced, DAM Vydyne® R550 is general-purpose, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is also lubricated for improved flow and offers superior surface appearance. G.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.750 mm |
7.0 - 14 sec @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R550H Nylon 66, 50% Glass Reinforced, DAM Vydyne® R550H is general-purpose, heat-stabilized, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 1.50 mm |
7.0 - 14 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 41H BK03 Nylon 66, Impact Modified, DAM Vydyne® 41H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.750 mm |
7.0 - 14 sec @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.750 mm |
7.0 - 14 sec @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® 47 BK11 Nylon 66, Impact Modified, DAM Vydyne® 47H BK11 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.710 mm |
7.0 - 14 sec @Thickness 0.0280 in |
UL 746A |
Ascend Performance Materials Vydyne® 66B Nylon 66, General Purpose, high viscosity, DAM Vydyne® 66B is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66B resin offers high strength, .. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.710 mm |
7.0 - 14 sec @Thickness 0.0280 in |
UL 746 |
Ascend Performance Materials Vydyne® 20NSP BLK Nylon 66, DAM Vydyne® 20NSP BLK is a general-purpose, high nucleated, lubricated PA66 resin. Available in black, it is designed to crystallize rapidly in order to reduce cycle times and increase productivity thr.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 1.50 mm |
7.0 - 14 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, DAM Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.400 mm |
7.0 - 14 sec @Thickness 0.0157 in |
UL 746 |
Ascend Performance Materials Vydyne® ECO366 Nylon 66, Flame-retardant, DAM Vydyne® ECO366 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for machin.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.750 mm |
7.0 - 14 sec @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R530H NAT Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H NAT is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of ph.. |
|||
Hot Wire Ignition, HWI | 7.0 - 14 sec @Thickness 0.750 mm |
7.0 - 14 sec @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R533H BK0201 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK0201 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |