Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 204 - 227 °C | 399 - 441 °F | |
PolyOne Versaflex™ FFC 2882-50 Thermoplastic Elastomer (TPE) Versaflex™ FFC 2882-50 is designed to pass several fatty food extraction conditions identified in EU Directive 82/711/EEC. Versaflex™ FFC 2882-50 will also overmold and co-extrude to polypropylene.. |
|||
Melt Temperature | 204 - 227 °C | 399 - 441 °F | |
PolyOne Versaflex™ FFC 2882-50 Thermoplastic Elastomer (TPE) Versaflex™ FFC 2882-50 is designed to pass several fatty food extraction conditions identified in EU Directive 82/711/EEC. Versaflex™ FFC 2882-50 will also overmold and co-extrude to polypropylene.. |
|||
Melt Temperature | 204 - 227 °C | 399 - 441 °F | |
PolyOne Versaflex™ FFC 2882-87 Thermoplastic Elastomer (TPE) Versaflex™ FFC 2882-87 is designed to pass several fatty food extraction conditions identified in EU Directive 2002/72/EC, FDA 21 CFR 177.2600, and GB 4806.1-94. Versaflex™ FFC 2882-87 will also o.. |
|||
Melt Temperature | 204 - 210 °C | 399 - 410 °F | |
PolyOne Geon™ HTX M6230 Polyvinyl Chloride Alloy (PVC Alloy) Information provided by PolyOne |
|||
Melt Temperature | 204 °C | 399 °F | |
Chevron Phillips 2151 High Impact, Liner Grade Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: High Impact Strength, Medium Slip, High Antiblock, Low Blocking and Good Openability, Good ProcessabilityApplications:Trash bags and other linersProcessing Co.. |
|||
Melt Temperature | 204 °C | 399 °F | |
Chevron Phillips 5036 LDPE High Clarity, Impact Film Resin
(discontinued **) Resin Type: Homopolymer; for General Purpose PackagingCharacteristics: Excellent Clarity, Good Impact Strength, High Slip, No Antiblock, Low Coefficient of Friction, Excellent ProcessabilityApplicat.. |
|||
Melt Temperature | 204 °C | 399 °F | |
Chevron Phillips 5554-H LDPE High Clarity, Medium Impact Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Excellent Clarity, Good Impact Strength, Excellent Processability, Low Coefficient of Friction, Good SealabilityApplications:Bread Bag, Dry Goods Packaging, P.. |
|||
Melt Temperature | 204 - 232 °C | 399 - 450 °F | Stock |
PolyOne Stat-Tech™ AS-7SS/000 ABS - 7% Stainless Steel Fiber
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 204 °C | 399 °F | |
Eastman 5251 LDPE 4% VA Copolymer, High Clarity, High Impact Film Resin for Laminations
(discontinued **) Resin Type: VA CopolymerCharacteristics: Excellent adhesion, Excellent processability and bubble stability, High slip and antiblock, Good impact strengthApplications:Laminations, Heavy produce and s.. |
|||
Melt Temperature | 204 °C | 399 °F | |
Eastman 5254 LDPE 4% VA Copolymer, High Clarity, High Impact Film Resin for Laminations
(discontinued **) Resin Type: VA CopolymerCharacteristics: Good adhesion, Good processability and bubble stability, Low slip, Medium antiblock, Good optical properties, Good impact strengthApplications:Laminations, H.. |
|||
Melt Temperature | 204 °C | 399 °F | |
Eastman 5269 LDPE 6.5% EVA Copolymer, Clarity, Ultra-high Impact Film Resin
(discontinued **) Resin Type: CopolymerCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flow for Injection Blow Molding Applications, Good Par.. |
|||
Melt Temperature | 204 - 260 °C | 399 - 500 °F | air purge at equilibrium conditions |
NOVA Chemicals DYLARK® 238 Impact Grade Engineering Resin Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn.. |
|||
Melt Temperature | 204 - 315 °C | 399 - 599 °F | Recommended oven temperature |
NOVA Chemicals Novapol® TR-0535-UI Hexene MDPE Rotational Molding Resin TR-0530-UI complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. TR-0530-UI is su.. |
|||
Melt Temperature | 204 - 215 °C | 399 - 419 °F | |
Huntsman PE1501 EVA Film Extrusion
(discontinued **) 5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Yields film with excellent impact strength, good heat seal, and good clarity.Applications: Film extrusion: greenhouse film, heavy-duty packa.. |
|||
Melt Temperature | 204 - 315 °C | 399 - 599 °F | |
NOVA Chemicals Novapol® PR-0636-UG Butene MDPE Rotational Molding Resin
(discontinued **) Very good processability, Very good ESCR, Good impact properties, NSF listed for Stds. 14, 24, and 61Applications: Toys, General purpose custom molding, Carts, Playground equipmentAdditives: Process.. |
|||
Melt Temperature | 204 - 315 °C | 399 - 599 °F | Varies with the mold shape and construction. Oven will also affect process time. |
NOVA Chemicals Sclair® TD-7915-UG Hexene MDPE Rotational Molding Resin
(discontinued **) Excellent low temperature impact properties, Excellent ESCR, Wide process window, NSF listing for Stds. 14, 24, and 61 pending, Retention of impact at long cook timesApplications: IBCs, Toys, Genera.. |
|||
Melt Temperature | 204 °C | 399 °F | |
LNP Stat-Kon® PDX-S-90398 Polyamide 12, Stainless Steel Fiber
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Melt Temperature | <= 204 °C | <= 399 °F | Cast Film |
Westlake ELEVATE™ EF529 18.5% Ethylene Vinyl Acetate Copolymer Westlake ELEVATE™ EF529 is an ethylene vinyl acetate copolymer with 18.5% VA. It contains no slip or antiblock and is designed for blown and cast films requiring excellent optics and low heat seal .. |
|||
Melt Temperature | 204 - 250 °C | 399 - 482 °F | Extrusion |
Total PPH 3762 Polypropylene, Extrusion Grade Homopolymer fiber grade for staple fiber and multifilament yarnsFading Resistance - FINA 3762 is formulated to resist gas fading while maintaining excellent processing stability up to 250oC.Process .. |
|||
Melt Temperature | 204 - 221 °C | 399 - 430 °F | Molding |
Lubrizol Estane® 2102-90A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Low compression setAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 20.. |
|||
Melt Temperature | 204 °C | 399 °F | |
Lubrizol Estane® 58144 Thermoplastic Polyurethane Type: Estane® 58144 is a 65D Polyether-type thermoplastic polyurethane (TPU) compound.Features: FDA (contact Lubrizol for details). Pre-drying: 2 hours at 104C (220F) in Dehumidifying Hopper Dryer.. |
|||
Melt Temperature | 204 °C | 399 °F | |
Chevron Phillips 5754 LDPE High Clarity, High Impact Film Resin for General Purpose Packaging Resin Type: HomopolymerCharacteristics: Excellent Impact Strength, High Clarity, Medium Slip, Medium Antiblock, Low Coefficient of Friction, Good OpenabilityApplications:Heavy Produce Bags, Frozen F.. |
|||
Melt Temperature | 204 °C | 399 °F | |
Chevron Phillips MarFlex® 5755 LDPE High Clarity, High Impact Film Resin Resin Type: HomopolymerCharacteristics: High Clarity, Excellent Impact Strength, Medium Slip, High Antiblock, Moderately High Coefficient of Friction, Excellent ProcessabilityApplications:Case Shrin.. |
|||
Melt Temperature | 204 °C | 399 °F | |
DuPont™ Surlyn® 2601 Sodium Ionomer Resin for Blown and Cast Film Surlyn® 2601 is an ionomer resin available for use in blown and cast film operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene resins. Applicati.. |
|||
Melt Temperature | 204 - 238 °C | 399 - 460 °F | |
Ineos Nova Zylar® 530 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:High clarityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationMeets USP XXIII specifications for Class VI plasticsUL94 HB @ 1.5 mm for uncolored ma.. |
|||
Melt Temperature | 204 - 227 °C | 399 - 441 °F | |
Ineos Nova 8048 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Improved toughness, Custom colorsApplications: Designed for injection molding applications requiring clarity and toughnessPerformance grades of polystyrene are engineered to have specific properties.. |
|||
Melt Temperature | 204 - 221 °C | 399 - 430 °F | Molding |
Lubrizol Estane® 2102-55D Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Load-bearing capacityAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product line from Dow in.. |
|||
Melt Temperature | 204 - 215 °C | 399 - 419 °F | |
Huntsman PE1451 EVA Film Extrusion
(discontinued **) 4.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |
|||
Melt Temperature | 204 - 315 °C | 399 - 599 °F | |
NOVA Chemicals Novapol® TR-0535-UG Hexene MDPE Rotational Molding Resin
(discontinued **) Molded Plaque Properties. Features: excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer. |
|||
Melt Temperature | 204 - 315 °C | 399 - 599 °F | |
NOVA Chemicals Novapol® PR-0636-U Butene MDPE Rotational Molding Resin
(discontinued **) Very good processability, Very good ESCR, Good impact properties, NSF listed for Stds. 14, 24, and 61Applications: Toys, General purpose custom molding, Carts, Playground equipmentAdditives: Process.. |