Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 210 - 221 °C | 410 - 430 °F | |
PlastiComp Complet® LCF50 - PP Homopolymer Polypropylene, 50% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Melt Temperature | 210 - 221 °C | 410 - 430 °F | |
PlastiComp Complet® LGF30 - PP Homopolymer Polypropylene, 30% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 30% long glass fiber reinforcementInformation provided by PlastiCom.. |
|||
Melt Temperature | 210 - 221 °C | 410 - 430 °F | |
PlastiComp Complet® LGF50 - PP Homopolymer Polypropylene, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 50% long glass fiber reinforcementInformation provided by PlastiCom.. |
|||
Melt Temperature | 210 - 221 °C | 410 - 430 °F | |
PolyOne Versaflex™ CL2250 Thermoplastic Elastomer (TPE) Versaflex™ CL2250 is an easy processing compound designed for use in injection molding applications where FDA compliance, clarity and enhanced heat resistance are required. - Excellent Clarity - Ov.. |
|||
Melt Temperature | 193 - 221 °C | 379 - 430 °F | |
PolyOne Versaflex™ OM 1060X-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 1060X-1 is an overmolding TPE with very good adhesion to PC or ABS-based plastics. - Good Surface Aesthetics - Rubbery Feel - Soft Touch - Very Good Bond to PC, ABS, PC/ABSColor conce.. |
|||
Melt Temperature | 188 - 221 °C | 370 - 430 °F | Molding |
PolyOne Edgetek® PE-10GF/000 High Density Polyethylene (HDPE), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 182 - 221 °C | 360 - 430 °F | Injection Molding |
Teknor Apex Sarlink® 3145D Thermoplastic Elastomer A high hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3145D can be processed by injection blow molding, molding or .. |
|||
Melt Temperature | 182 - 221 °C | 360 - 430 °F | Injection Molding |
Teknor Apex Sarlink® 3160 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3160 can be processed by injection molding or extrusion for ap.. |
|||
Melt Temperature | 182 - 221 °C | 360 - 430 °F | Injection Molding |
Teknor Apex Sarlink® 3445D Thermoplastic Elastomer A NSF certified, high hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inje.. |
|||
Melt Temperature | 182 - 221 °C | 360 - 430 °F | Injection Molding |
Teknor Apex Sarlink® 3470N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Melt Temperature | 182 - 221 °C | 360 - 430 °F | Injection Molding |
Teknor Apex Sarlink® 4175 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4175 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical.. |
|||
Melt Temperature | 182 - 221 °C | 360 - 430 °F | Injection Molding |
Teknor Apex Sarlink® 4180 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4180 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical.. |
|||
Melt Temperature | 204 - 221 °C | 399 - 430 °F | Extrusion |
Lubrizol Pellethane® 2363-75D Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Melt Temperature | 204 - 221 °C | 399 - 430 °F | Molding |
Lubrizol Estane® 2103-90A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Low compression setAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 20.. |
|||
Melt Temperature | 204 - 221 °C | 400 - 430 °F | |
Ecomass® 4703TU95 Tungsten Filled Polyurethane Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsHigh Specific GravityTungsten Powder Filled Polyurethane (TPU)FlexibleInformation provided by Technical Po.. |
|||
Melt Temperature | 204 - 221 °C | 400 - 430 °F | |
Ecomass® 4703ZB92 Filled Polyurethane Nontoxic alternative to Lead (Pb), radiation shielding applicationsModerate Specific GravityFilled Polyurethane (TPU) Base ResinFlexibleInformation provided by Technical Polymers |
|||
Melt Temperature | 204 - 221 °C | 400 - 430 °F | |
Ecomass® 4703ZC87 Stainless Steel Filled Polyurethane Nontoxic alternative to Lead (Pb), weighting and balancing applicationsModerate Specific GravityStainless Steel Filled Polyurethane (TPU)FlexibleInformation provided by Technical Polymers |
|||
Melt Temperature | 204 - 221 °C | 400 - 430 °F | |
Ecomass® 4703ZD84 Tungsten Filled Polyurethane Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsModerate Specific GravityTungsten Powder Filled Polyurethane (TPU)FlexibleInformation provided by Technica.. |
|||
Melt Temperature | 191 - 221 °C | 375 - 430 °F | |
Clariant Renol PPSP0006HW Polypropylene Homopolymer, Heavy Weight Compound Data provided by Clariant Masterbatches |
|||
Melt Temperature | 193 - 221 °C | 380 - 430 °F | |
Clariant Renol PPT20BN-346 Polypropylene Copolymer, Talc Filled Data provided by Clariant Masterbatches |
|||
Melt Temperature | 199 - 221 °C | 390 - 430 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6080 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6080NC/BK are designed to be a general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR
6080NC/BK have excellent soft touc.. |
|||
Melt Temperature | 182 - 221 °C | 360 - 430 °F | |
M. Holland Company LL106 LLDPE
(discontinued **) Additives: Antiblock, SlipFeatures: Unspecified Antiblocking, Hexane Comonomer, Copolymer, Good Drawdown, Good Processability, Unspecified SlipUses: Film, LinersApprovals: FDA 21 CFR 177.1520(c) 2.2.. |
|||
Melt Temperature | 182 - 221 °C | 360 - 430 °F | Injection Molding |
Teknor Apex Sarlink® 3140 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3140 can be processed by injection molding or extrusion for appl.. |
|||
Melt Temperature | 182 - 221 °C | 360 - 430 °F | Injection Molding |
Teknor Apex Sarlink® 3490 Thermoplastic Elastomer A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj.. |
|||
Melt Temperature | 182 - 221 °C | 360 - 430 °F | Injection Molding |
Teknor Apex Sarlink® 4139D Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4139D is a high hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |
|||
Melt Temperature | 204 - 221 °C | 400 - 430 °F | Molding |
PolyOne Edgetek® PE-25CF/000 High Density Polyethylene (HDPE), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 182 - 221 °C | 360 - 430 °F | Injection Molding |
Teknor Apex Sarlink® 3150 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3150 can be processed by injection molding or extrusion for appl.. |
|||
Melt Temperature | 182 - 221 °C | 360 - 430 °F | Injection Molding |
Teknor Apex Sarlink® 3180 Thermoplastic Elastomer A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3180 can be processed by blow molding injection molding or ex.. |
|||
Melt Temperature | 182 - 221 °C | 360 - 430 °F | Injection Molding |
Teknor Apex Sarlink® 4149D Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4149D is a high hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |