Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJAC36L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJJC330 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible A75M1 Trans 9000 Polyvinyl Chloride, Flexible (PVC, Flexible) This compound is certified for fuel hose applications(R1 Type B Class 1)under SAE J 1527 requirements.Information provided by PolyOne |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible A90U2 Polyvinyl Chloride, Flexible (PVC, Flexible) GENERAL PURPOSE CLEAR PVC COMPOUND WITH LOW LEVEL OF U.V. INHIBITOR, to be used only in interior applications.Information provided by PolyOne |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible R5185A Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible XV3830B Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 177 - 204 °C | 350 - 400 °F | Extrusion |
ExxonMobil Vyram™ 9101-55 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Melt Temperature | 177 - 216 °C | 350 - 420 °F | Extrusion |
ExxonMobil Vyram™ 9103-45 Thermoplastic Elastomer
(discontinued **) A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Flexible R5230C Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 177 °C | 351 °F | |
DuPont™ Surlyn® 1652-1 Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating
(discontinued **) Surlyn® 1652-1 is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylen.. |
|||
Melt Temperature | 177 - 193 °C | 350 - 380 °F | Injection |
Laurel BioComposite Bio-Resâ„¢ 20% Composite in HDPE Bio-Resâ„¢ can be blended with various resins in certain applications. It can be included at rates up to 40% in manufactured plastic products while maintaining or enhancing the desired characteri.. |
|||
Melt Temperature | 177 °C | 350 °F | |
Teknor Apex APEX® 3202-75 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Caps, Closure, Connectors, Food Service Applications, Safety Equipment, Valves/Valve Parts Appearance-Cl.. |
|||
Melt Temperature | 177 °C | 350 °F | |
Teknor Apex APEX® 3211-75 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Melt Temperature | 177 °C | 350 °F | |
Teknor Apex APEX® 3301-75NT Polyvinyl Chloride, Flexible Features: Non-DEHP Plasticizer; Ethylene Oxide Sterilizable Uses: Medical/Healthcare Applications; Toys; Tubing Processing Method: Extrusion Forms: PelletsInformation Provided by Teknor Apex |
|||
Melt Temperature | 177 °C | 351 °F | |
DuPont™ Surlyn® 1605 Sodium Ionomer Resin for Blown/Cast Film and Extrusion Coating Surlyn® 1605 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment and extrusion coating and coextrusion coating equipment designed to proces.. |
|||
Melt Temperature | 177 °C | 351 °F | |
DuPont™ Surlyn® 1652 Zinc Ionomer Resin for Flexible Packaging Surlyn® 1652 is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene .. |
|||
Melt Temperature | 177 °C | 351 °F | Extrusion |
Dow Tyrin® 4211P Chlorinated Polyethylene Elastomer 42% Chlorine. Tyrin® chlorinated polyethylene thermoplastic resins offer the compounding and fabrication industries end product properties in a range of hardnesses, and behave much like flexible P.. |
|||
Melt Temperature | 177 °C | 350 °F | |
Axiall 8852 Moldings & Extrusions Flexible PVC General purpose compound recommended for extrusion applications. Contains a biocide and is UV stabilized.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 177 °C | 350 °F | |
Axiall EX 3154 Plenum Flexible PVC Non-lead stabilized CAT 3 plenum jacket. Recommended for up to 25 pair, unshielded.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 177 °C | 350 °F | |
Axiall 113B-FR Moldings & Extrusions Flexible PVC Non-lead stabilized, 105°C rated injection molding compound. Rated 94 V-0 at 1.5 mm and 94 V-1 at 0.58 mm for all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation .. |
|||
Melt Temperature | 177 °C | 350 °F | |
Axiall 190 Moldings & Extrusions Flexible PVC 60C plug molding component. UL recognized component for 94 V-0 in all colors. 1.13 mm minimum thickness. UL QMFZ2 recognized component.Information provided by Georgia GulfGeorgia Gulf became Axia.. |
|||
Melt Temperature | 177 °C | 350 °F | |
Axiall 419-90D Coax & Telecom Flexible PVC 419-90D is a highly flame retardant jacket originally designed for CSA FT-4 type CATV applications and has good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axi.. |
|||
Melt Temperature | 177 °C | 350 °F | |
Axiall 10756 Wire & Cable Flexible PVC General purpose, non-lead stabilized jacketing compound recommended for a maximum service temperature of 80°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 177 °C | 350 °F | |
Teknor Apex APEX® 3201-75 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Melt Temperature | 177 °C | 351 °F | |
DuPont™ Surlyn® 1652SB Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating Surlyn® 1652SB is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylen.. |
|||
Melt Temperature | 177 - 204 °C | 350 - 400 °F | Extrusion |
ExxonMobil Santoprene® 201-64W175 Thermoplastic Elastomer
(discontinued **) A soft, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for thin wall .. |
|||
Melt Temperature | 177 - 188 °C | 351 - 370 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion L6256 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Melt Temperature | 177 - 191 °C | 350 - 375 °F | |
Sylvin Technologies 9604-95C Clear PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable W3301 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |