Material Notes:
36% Chlorine. Tyrin® chlorinated polyethylene thermoplastic resins offer the compounding and fabrication industries end product properties in a range of hardnesses, and behave much like flexible PVC in many uses. Can be calendered, injection molded, or extruded into tough, chemical and weather resistent products that can also provide built-in ignition resistance.Performance highlights include: inherenr flexibility with plasticization; inherent chemical and ignition resistance; compatibility with PVC, PE, SAN, ABS, and other polymers, excellent low temperature properties, resistance to weathering, acceptance of fillers and heat/light stabilizers.This former DuPont Dow Elastomers product line is now produced by Dow Chemical.
Physical Properties Metric English Comments
Moisture Vapor Transmission 1.80 cc-mm/m²-24hr-atm
4.57 cc-mil/100 in²-24hr-atm
36% Cl content Tyrin resin w/ Ba-Cd stabilizer, Epoxidized soybean oil, phosphite chelator, and lubricant.
Oxygen Transmission 32.0 cc-mm/m²-24hr-atm
81.3 cc-mil/100 in²-24hr-atm
36% Cl content Tyrin resin w/ Ba-Cd stabilizer, Epoxidized soybean oil, phosphite chelator, and lubricant.
Viscosity Measurement 20000
20000
Nominal melt viscosity. DuPont Dow test method CPE-D3
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 23.0 MPa
3340 psi
typical Tyrin resin w/ Ba-Cd stabilizer, Epoxidized soybean oil, phosphite chelator, and lubricant.
Elongation at Break 425 %
425 %
typical Tyrin resin w/ Ba-Cd stabilizer, Epoxidized soybean oil, phosphite chelator, and lubricant.
100% Modulus 0.00140 GPa
0.203 ksi
Unfilled Tyrin compound; ASTM D412
Tear Strength Test 180
180
Unfilled Tyrin compound; ASTM D1004
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
Dielectric Constant 5.1

@Frequency 10000 Hz
5.1

@Frequency 10000 Hz
6.1

@Frequency 100 Hz
6.1

@Frequency 100 Hz
Dissipation Factor 0.010

@Frequency 100 Hz
0.010

@Frequency 100 Hz
0.10

@Frequency 10000 Hz
0.10

@Frequency 10000 Hz
36% Cl content Tyrin resin w/ Ba-Cd stabilizer, Epoxidized soybean oil, phosphite chelator, and lubricant.
Processing Properties Metric English Comments
Rear Barrel Temperature 93.0 - 106 °C
199 - 223 °F
for extrusion
Middle Barrel Temperature 106 - 149 °C
223 - 300 °F
for extrusion
Front Barrel Temperature 149 - 162 °C
300 - 324 °F
for extrusion
Nozzle Temperature 162 °C
324 °F
Extrusion die
Melt Temperature 177 °C
351 °F
Extrusion
Copyright © lookpolymers.com All Rights Reserved