Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Flexible D9000 Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Flexible D9000 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
15 sec; ASTM D2240
90
90
ASTM D2240
Tensile Strength at Break 13.8 MPa
2000 psi
510 mm/min; ASTM D638
Tensile Strength 9.65 MPa

@Strain 100 %
1400 psi

@Strain 100 %
510 mm/min; ASTM D638
Elongation at Break 330 %
330 %
510 mm/min; ASTM D638
Tear Strength 64.8 kN/m
370 pli
Die C, 510 mm/min; ASTM D624
Compression Set 35 %

@Temperature 23.0 °C,
Time 79200 sec
35 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
Clash Berg Modulus 0.517 GPa
75.0 ksi
ASTM D1043
0.310 GPa

@Temperature -26.0 °C
45.0 ksi

@Temperature -14.8 °F
ASTM D1043
Thermal Properties Metric English Comments
Brittleness Temperature -25.0 °C
-13.0 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 177 - 182 °C
351 - 360 °F
Descriptive Properties Value Comments
Features General Purpose
Low Gloss
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Regional Availability Africa & Middle East