Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 360 min | 6.00 hour | On metal (Full) |
ND Industries 612 Heptane-Acetone Anaerobic Primer Fast acting anaerobic primer. On part life 7 days. Non-ozone depleting but flammable solvent |
|||
Cure Time | 360 min | 6.00 hour | Ambient Set |
Reltek BONDiT™ B-482 Adhesive, Sealant & Coating System Key Properties: Excellent balance of chemical, electrical, and mechanical properties.Ruggedized, semi-flexible system.Very clean system.Ease of use.Applications: Encapsule sensitive instrumentation .. |
|||
Cure Time | 360 - 960 min @Temperature 23.0 °C |
6.00 - 16.0 hour @Temperature 73.4 °F |
M10 steel, handling strength |
Permabond LH054 Anaerobic Threadsealant Permabond® LH054 is an anaerobic curing, calibrated strength pipe sealant that allows for easier disassembly – especially of larger diameter pipes. It cures anaerobically when in contact with meta.. |
|||
Cure Time | 360 - 480 min @Temperature 25.0 °C |
6.00 - 8.00 hour @Temperature 77.0 °F |
Full Cure |
Fibre Glast 1101 High-Strength General Purpose Epoxy Adhesive Description:#1101 is a light grayish-tan two part epoxy adhesive that was developed especially for difficult bonding problems involving similar or dissimilar materials. #1101 provides excellent adhe.. |
|||
Cure Time | 360 min | 6.00 hour | To depth of 3.2 mm |
Momentive Performance Materials RTV5242 Neutral Cure, One Component RTV Adhesive Sealant RTV5240 series sealants are alkoxy neutral cure, one-component, ready to use, electronic grade silicone adhesive sealants exhibiting high strength that will maintain a strong bond even when exposed .. |
|||
Cure Time | 360 min | 6.00 hour | To depth of 3.2 mm |
Momentive Performance Materials RTV5243 Neutral Cure, One Component RTV Adhesive Sealant RTV5240 series sealants are alkoxy neutral cure, one-component, ready to use, electronic grade silicone adhesive sealants exhibiting high strength that will maintain a strong bond even when exposed .. |
|||
Cure Time | 360 - 480 min | 6.00 - 8.00 hour | Tack-free |
Sika Industry SikaFlex 219 LM Low Modulus Polyurethane Sealant Sika 219 LM SikaFlex Low Modulus Polyurethane SealantThis is a high performance, low modulus polyurethane base, non-sag elastomeric sealant with excellent adhesion to a wide variety of substrates. M.. |
|||
Cure Time | 360 - 600 min @Temperature 23.9 °C |
6.00 - 10.0 hour @Temperature 75.0 °F |
|
Master Bond EP65HT Fast Setting Epoxy Resists High Temperatures Description: Master Bond EP65HT represents a highly innovative advance in epoxy technology in that it features the unusual combination of very fast cures and high temperature resistance. While typic.. |
|||
Cure Time | 360 min | 6.00 hour | 2 hrs @ 65°C + 4 hrs @ 130°C |
Tra-Con Tra-Bond 2208 Water White High Temperature Epoxy Adhesive TRA-BOND 2208 is a clear, almost water-white low viscosity epoxy adhesive system recommended for rigid laminating, filament winding, potting and bonding applications. This all-liquid formulation con.. |
|||
Cure Time | 360 min | 6.00 hour | 4 hrs @ 25°C + 2 hrs @ 65°C |
Tra-Con Tra-Cast 3104 Low Viscosity Epoxy Casting Compound TRA-CAST 3104 is a low viscosity, room temperature cure epoxy casting system developed for high performance production encapsulation and impregnating applications where filling fine intricate free s.. |
|||
Cure Time | 360 min | 6.00 hour | 4 hrs @ 25°C + 2 hrs @ 65°C |
Tra-Con Tra-Cast 3110 Low Density Epoxy Casting System TRA-CAST 3110 is a unicellular, low density, syntactic-foam epoxy resin casting system of medium viscosity that easily handles, mixes and cures at room temperature. Developed for industrial encapsul.. |
|||
Cure Time | 360 min | 6.00 hour | 4 hrs @ 25°C + 2 hrs @ 65°C |
Tra-Con Tra-Cast 3107 Low Shrinkage Epoxy Casting System TRA-CAST 3107 is a versatile epoxy casting system developed for high performance production potting, encapsulating, casting and tooling applications where low shrinkage, easy handling and flowabilit.. |
|||
Cure Time | 360 min | 6.00 hour | 4 hrs @ 25°C + 2 hrs @ 65°C |
Tra-Con Tra-Cast 3143 Fire Retardant Epoxy Casting Compound TRA-CAST 3143 has a low viscosity and long pot life. It is certified to the requirements of UL 94 V-O, and is recommended for rigid potting, laminating, transformer encapsulating, filament winding a.. |
|||
Cure Time | >= 360 min | >= 6.00 hour | |
Trelleborg Emerson & Cuming Stycast® 2762/17M-1 Two-Component Epoxy High Service Temp Encapsulant Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har.. |
|||
Cure Time | 360 min | 6.00 hour | Tack-Free Time |
3M AC-665 Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-665 Class B are two-part, manganese-cured, chromate containing, corrosion inhabiting sealants. These Sealants provide an effective barrier against the common causes of corros.. |
|||
Cure Time | 360 - 480 min | 6.00 - 8.00 hour | Tack Free Time, catalyzed with QM cat BLUE |
ACC QM 107 QSI Quantum Silicones 7 Durometer Condensation Cure Moldmaking Material QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is us.. |
|||
Cure Time | 360 - 480 min | 6.00 - 8.00 hour | Tack Free Time, catalyzed with QM cat BLUE |
ACC QM 118 QSI Quantum Silicones 18 Durometer Condensation Cured Moldmaking Material QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an.. |
|||
Cure Time | 360 - 480 min | 6.00 - 8.00 hour | Tack Free Time, catalyzed with QM cat BLUE |
ACC QM 122 QSI Quantum Silicones 22 Durometer Condensation Cured Moldmaking Material QM 122 is a two-component, room temperature condensation cure silicone material. The cured rubber is flexible with excellent mechanical and physical properties in addition to good shelf-life stabili.. |
|||
Cure Time | 360 min | 6.00 hour | Touch Dry |
3M Scotchkote™ 162HB Epoxy Coating 3M Scotchkote Epoxy Coating 163HB has been specifically developed as a 100% solids lining for the internals of pipes, tanks, vessels and other equipment in contact with fresh water, sea water, raw w.. |
|||
Cure Time | 360 min | 6.00 hour | Machining Time |
3M Scotchkote™ FG 512 Epoxy Ceramic Surfacer Scotchkote Epoxy Ceramic Surfacer FG 512 has been specifically developed as a ceramic enhanced epoxy repair coating for resurfacing and reforming metal machinery and equipment, such as pumps, impell.. |
|||
Cure Time | 360 min | 6.00 hour | Full Cure |
3M Scotch-Weld™ DP604NS Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesive DP-604NS is a black, rapid setting, two-component polyurethane. It is packaged as 1:1 ratio liquids in a duo-pak cartridge. With the squeeze of the trigger, the .. |
|||
Cure Time | 360 - 420 min | 6.00 - 7.00 hour | |
3M AC-370 Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-370 Class B are fast cure, low density polysulfide sealants suitable for fuel tank and fuselage applications. These two-component, manganese dioxide cured sealants are solven.. |
|||
Cure Time | 360 min | 6.00 hour | Hard Dry |
3M Scotchkote™ 165HB Urethane Coating 3M Scotchkote Urethane Coating 165HB is a two component 100% solids urethane coating used for the internal and external protection of steel and concrete pipes, tanks, and vessels. It can be used in .. |
|||
Cure Time | 360 - 480 min | 6.00 - 8.00 hour | Time to Handling Strength |
3M Scotch-Weld™ DP640 Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-part, non-sag urethane adhesives. They feature tough, flexible bonds with good adhesion to a wide variety of substrates especially wood and many properl.. |
|||
Cure Time | 360 min @Temperature 121 °C |
6.00 hour @Temperature 250 °F |
Alternate Cure |
Aremco Aremco-Bond™ 2315 High Performance Epoxide High Temperature, Low Viscosity, Potting Compound for Electrical Applications. |
|||
Cure Time | 360 min | 6.00 hour | Time to Handling Strength |
3M Scotch-Weld™ DP190 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Translucent is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Translucent but faster curing.Information provided by 3M |