Fibre Glast 1101 High-Strength General Purpose Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Fibre Glast Developments Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fibre Glast 1101 High-Strength General Purpose Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description:#1101 is a light grayish-tan two part epoxy adhesive that was developed especially for difficult bonding problems involving similar or dissimilar materials. #1101 provides excellent adhesion to a wide variety of materials such as aluminum, steel, brass, concrete, brick, glass, stone, ceramics, tile, and wood. #1101 has very good handling characteristics. The mix ratio of 1 to 1 by weight or volume allows for easy measuring. It has a creamy, smooth viscosity. It is very easy to mix, and has good thixotropy for application to contoured or vertical surfaces without sag or runoff. #1101 cures relatively quickly, developing sufficient "green strength" to allow bonded items to be removed from the holding fixtures and handled within a few hours. The cured material has excellent strength as well as good resistance to weak acids, moisture and weather.Applications#1101 is an excellent adhesive for all types of bonding applications. It is very versatile, and can bond a wide variety of materials, so it becomes an effective tool in general shop situations. Often #1101 will outperform other supposed high performance materials, and give handling advantages as well. It has been successfully used for many years in a variety of general bonding uses as well as numerous production applications.Information provided by Fibre Glast Developments Corporation.
Physical Properties Metric English Comments
Density 1.51 g/cc
0.0546 lb/in³
ASTM D1475
Water Absorption <= 0.20 %
<= 0.20 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Shore D 90
90
Cured; ASTM D2240
Tensile Strength at Break 49.6 MPa
7200 psi
Cast bar; ASTM D638
Elongation at Break 6.0 %
6.0 %
ASTM D412
Compressive Yield Strength 98.6 MPa
14300 psi
ASTM D695
Adhesive Bond Strength 24.0 MPa
3480 psi
Lap Shear; Aluminum to Aluminum; ASTM D1002
Processing Properties Metric English Comments
Cure Time 180 - 240 min
3.00 - 4.00 hour
Handling strength in 3 to 4 hrs.
45.0 - 60.0 min

@Temperature 60.0 °C
0.750 - 1.00 hour

@Temperature 140 °F
Full cure in 45 to 60 mins at 140°F.
360 - 480 min

@Temperature 25.0 °C
6.00 - 8.00 hour

@Temperature 77.0 °F
Full Cure
Gel Time 20.0 - 30.0 min
20.0 - 30.0 min
Value for 1 lbm; ASTM D2471
Descriptive Properties Value Comments
Mix Ratio 1:1
Resin:Hardener by Volume
100:100
Resin:Hardener by Weight