Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Tra-Con Tra-Cast 3104 Low Viscosity Epoxy Casting Compound

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Tra-Con, Inc.
Trade Name Tra-Cast
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Cast 3104 Low Viscosity Epoxy Casting Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
TRA-CAST 3104 is a low viscosity, room temperature cure epoxy casting system developed for high performance production encapsulation and impregnating applications where filling fine intricate free space is required. This medium exotherm, low shrinkage system exhibits excellent flow and wetting characteristics. Its low viscosity allows for void-free filling and self-leveling in casting use, and excellent impregnation of fine wire transformers and coils. Fully cured TRA-CAST 3104 is a durable electrical insulator, dimensionally stable over a wide temperature range, and is resistant to moisture, gases, petroleum lubricants and fuels, salts, many mild acids and alkalis, and other organic and inorganic compounds. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
Mixed
Solids Content 100 %
100 %
Reactive Solids Content
Volatile Organic Compounds (VOC) Content 12 g/l
12 g/l
Water Absorption 0.0010 %
0.0010 %
After 24 hours
Viscosity 5000 cP

@Temperature 25.0 °C
5000 cP

@Temperature 77.0 °F
Mixed (sp #6, 10 rpm)
Mechanical Properties Metric English Comments
Hardness, Shore D 90
90
Adhesive Bond Strength 9.31 MPa
1350 psi
Lap shear, alum to alum, 72 hrs @ 25°C
12.4 MPa
1800 psi
Lap shear, alum to alum, 4 hrs @ 25°C + 2 hrs @ 65°C
Thermal Properties Metric English Comments
CTE, linear 89.7 µm/m-°C
49.8 µin/in-°F
Below Tg
214 µm/m-°C
119 µin/in-°F
Above Tg
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Glass Transition Temp, Tg 62.0 °C
144 °F
Ultimate Tg
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+14 ohm-cm
2.00e+14 ohm-cm
Dielectric Constant 4.6

@Frequency 1000 Hz
4.6

@Frequency 1000 Hz
Dielectric Strength 17.7 kV/mm
450 kV/in
Dissipation Factor 0.010

@Frequency 1000 Hz
0.010

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 360 min
6.00 hour
4 hrs @ 25°C + 2 hrs @ 65°C
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 30 min
30 min
Descriptive Properties Value Comments
Color Black
Heat Distortion Temperature °C 105
Mix Ratio, parts by weight 100/7
Resin/Hardener