Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 960 min | 16.0 hour | Functional cure |
ITW Devcon Flexane® Rubber Repair / Castable Urethane 80 Liquid, Black Information provided by ITW Devcon |
|||
Cure Time | 960 min | 16.0 hour | Functional cure |
ITW Devcon Flexane® Rubber Repair / Castable Urethane 94 Liquid, Black Information provided by ITW Devcon |
|||
Cure Time | 960 min | 16.0 hour | Functional cure |
ITW Devcon Metal Repair Bronze Putty (BR), Bronze Information provided by ITW Devcon |
|||
Cure Time | 960 min | 16.0 hour | Functional cure |
ITW Devcon Metal Repair Ceramic Repair Putty, Dark Blue Information provided by ITW Devcon |
|||
Cure Time | 960 min | 16.0 hour | Functional cure |
ITW Devcon Metal Repair Stainless Steel Putty (ST), Grey Information provided by ITW Devcon |
|||
Cure Time | 960 min | 16.0 hour | Functional cure |
ITW Devcon Metal Repair Titanium Putty, Grey Information provided by ITW Devcon |
|||
Cure Time | 960 min | 16.0 hour | Functional cure |
ITW Devcon Flexane® Rubber Repair / Castable Urethane High Performance Putty, Black Information provided by ITW Devcon |
|||
Cure Time | <= 960 min | <= 16.0 hour | Curing |
Silikony Polskie Gumosil AD-1 A/B Silicone Rubber Flexible with high resistance to tension |
|||
Cure Time | 960 min | 16.0 hour | 12hrs @ 25°C + 2hrs @ 65°C + 2 hrs @ 90°C |
Tra-Con Tra-Cast FS407 Low Viscosity High Temperature Epoxy Casting System TRA-CAST FS407 is a low viscosity, solvent-free epoxy casting system recommended for rigid industrial laminating, electrical potting and transformer or coil embedding applications that require the e.. |
|||
Cure Time | 960 min | 16.0 hour | 12hrs @ 25°C + 2hrs @ 65°C + 2hrs @ 90°C |
Tra-Con Tra-Bond 2211 High Temperature Epoxy Adhesive TRA-BOND 2211 is a low viscosity epoxy adhesive system recommended for industrial bonding applications where superior wetting and good mechanical and electrical insulation performance features are r.. |
|||
Cure Time | 960 - 1440 min @Temperature 93.3 °C |
16.0 - 24.0 hour @Temperature 200 °F |
|
Cotronics Duralco™ 132 500°F (260°C) Aluminum Filled Epoxy Aluminum filled epoxy that cures at room temperature to form machinable, thermally conductive bond lines. High heat transfer. Can be supplied as a “non-sag” putty.Applications: heat tacking, hea.. |
|||
Cure Time | 960 - 1440 min | 16.0 - 24.0 hour | |
Dow BETAMATE™ 7000/7050 L Epoxy Two component room temperature fast curing polyurethane structural adhesive with high elastic modulus.Information provided by Dow |
|||
Cure Time | 960 - 1440 min @Temperature 93.3 °C |
16.0 - 24.0 hour @Temperature 200 °F |
|
Cotronics Duralco™ 122 500°F (260°C) Nickel Filled Adhesive and Casting Epoxy Specially formulated to provide an economical alternative to silver filled electrically conductive epoxies. Applications: for use in applications where highest electrically conductivity not required.. |
|||
Cure Time | 960 - 1440 min @Temperature 93.3 °C |
16.0 - 24.0 hour @Temperature 200 °F |
|
Cotronics Duralco™ 128 500°F (260°C) Ceramic Filled Epoxy Ceramic filled, electrically resistant adhesive and potting compound. The ceramic fillers provide both high thermal conductivity and high dielectric strength. Cures at room temperature. Curing ca.. |
|||
Cure Time | 960 min | 16.0 hour | Hard Dry |
3M Scotchkote™ 152LV Epoxy Coating Scotchkote Epoxy Coating 152LV has been specifically developed as a surface tolerant anti corrosive coating for steel structures.Product Features:Combines good application characteristics with excel.. |
|||
Cure Time | 960 min | 16.0 hour | Hard Dry |
3M Scotchkote™ 162HB Epoxy Coating 3M Scotchkote Epoxy Coating 163HB has been specifically developed as a 100% solids lining for the internals of pipes, tanks, vessels and other equipment in contact with fresh water, sea water, raw w.. |
|||
Cure Time | 960 min | 16.0 hour | Machining Time |
3M Scotchkote™ 80BG 536 Urethane Elastomer Scotchkote Urethane Elastomer 80BG 536 has been specifically developed as an elastomeric system with a high degree of flexibility for resurfacing rubber components. Product Features:Properties simil.. |
|||
Cure Time | 960 min | 16.0 hour | Machining Time |
3M Scotchkote™ 80EG 531 Urethane Elastomer Scotchkote Urethane Elastomer 80EG 531 has been specifically developed as an elastomeric repair system with a high degree of flexibility for rebuilding and resurfacing rubber components.Product Feat.. |
|||
Cure Time | 960 min | 16.0 hour | Machining Time |
3M Scotchkote™ 80FG 532 Urethane Elastomer Scotchkote Urethane Elastomer 80FG 532 has been specifically developed as an elastomeric system with a high degree of flexibility for casting and molding rubber components.Product Features:Propertie.. |
|||
Cure Time | 960 min | 16.0 hour | Hard Dry |
3M Scotchkote™ FB 857 Urethane Floor Coating Scotchkote Urethane Floor Coating FB 857 has been specifically developed as a 100% solids protection system with a degree of flexibility for application to concrete and asphalt floor surfaces.Produc.. |
|||
Cure Time | 960 min | 16.0 hour | Hard Dry |
3M Scotchkote™ MC 145 Epoxy Primer Scotchkote Epoxy Primer MC 145 is a solvent based two component primer suitable for use on a wide range of metallic and glass reinforced plastic (GRP) surfaces prior to the application of Scotchkote.. |
|||
Cure Time | 960 min | 16.0 hour | Hard Dry |
3M Scotchkote™ UV 840 Urethane Coating Scotchkote Urethane Coating UV 840 has been developed to provide a durable gloss finish for use as the final coat of 3M coating systems in the construction and transport industries, where an ease of.. |
|||
Cure Time | 960 min | 16.0 hour | Hard Dry |
3M Scotchkote™ 445 Epoxy Slip Deterrent System Scotchkote Epoxy Slip Deterrent System 445 has been specifically developed as a 100% solids system for use with 3M Scotchkote Granular Aggregate to provide a slip deterrent finish to high risk floor.. |
|||
Cure Time | 960 min | 16.0 hour | Machining Time |
3M Scotchkote™ 60EG 533 Urethane Elastomer Scotchkote Urethane Elastomer 60EG 533 has been specifically developed as an elastomeric repair system with a high degree of flexibility for rebuilding and resurfacing rubber components.Product Feat.. |
|||
Cure Time | 960 min | 16.0 hour | Machining Time |
3M Scotchkote™ 60FG 534 Urethane Elastomer Scotchkote Urethane Elastomer 60FG 534 has been specifically developed as an elastomeric system with a high degree of flexibility for resurfacing rubber components.Product Features:Physical properti.. |
|||
Cure Time | 960 min | 16.0 hour | Hard Dry |
3M Scotchkote™ SP 810 Epoxy Sealer Scotchkote Epoxy Sealer SP 810 has been specifically developed as a low viscosity primer/sealer for concrete and cementitious surfaces prior to application of other Scotchkote 100% solids epoxy syst.. |
|||
Cure Time | 960 min @Temperature 24.0 °C |
16.0 hour @Temperature 75.2 °F |
|
BCC Products BC 5009 General Purpose Epoxy System BC5009 is a very low viscosity, modified, unfilled, room temperature curing, general purpose resin system. BC5009 is a clear-amber epoxy adhesive especially formulated for the bonding of wood and u.. |
|||
Cure Time | 960 min @Temperature 24.0 °C |
16.0 hour @Temperature 75.2 °F |
|
BCC Products BC 6126 Epoxy Surface Coat/Casting BC 6126 is a gray, low toxicity, aluminum filled, epoxy surface coat. This thixotropic resin system provides excellent surface duplication along with vertical coverage to 1/16 inch thickness. This h.. |
|||
Cure Time | 960 min @Temperature 24.0 °C |
16.0 hour @Temperature 75.2 °F |
|
BCC Products BC 6128 Epoxy, Hi-Heat, Abrasion Resistant BC 6128 is a black, non-staining, silicon carbide filled, “die surface” surfacing resin. This thixotropic resin system provides excellent surface duplication along with good vertical coverage. Ext.. |
|||
Cure Time | 960 min @Temperature 24.0 °C |
16.0 hour @Temperature 75.2 °F |
|
BCC Products BC 7009-1 Epoxy Casting BC 7009-1 is an iron filled, low-cost mass casting system. Thicknesses up to two inches in non-conductive molds, and four inches in conductive molds can be achieved without foaming or yielding exces.. |