Material Notes:
BC 6128 is a black, non-staining, silicon carbide filled, “die surface” surfacing resin. This thixotropic resin system provides excellent surface duplication along with good vertical coverage. Extended mold life due to superior wear resistance and hardness are the major benefits derived from its use. This heat resistant system may be used at room temperature without post-curing. For use above 150º F a post-cure is required. BC6128 can afford consistent use to 300º F if required. Does not contain VCHD or MDA. Designed for uses in: RTM and RIM molds, constructing vacuum form tools, injection and compression molds, and matched dies.Information provided by BCC Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.84 g/cc
1.84 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore D 92

@Temperature 23.9 °C
92

@Temperature 75.0 °F
Tensile Strength, Ultimate 51.4 MPa
7450 psi
Flexural Strength 81.4 MPa
11800 psi
Compressive Strength 199 MPa
28800 psi
Thermal Properties Metric English Comments
CTE, linear 37.8 µm/m-°C
21.0 µin/in-°F
Processing Properties Metric English Comments
Cure Time 960 min

@Temperature 24.0 °C
16.0 hour

@Temperature 75.2 °F
Pot Life 35 - 45 min

@Temperature 24.0 °C
35 - 45 min

@Temperature 75.2 °F
1 lb. mass
Descriptive Properties Value Comments
Mix Ratio 100:7 by weight, 100:13 by volume, resin/harder
Mixed Viscosity, Brookfield Thixotropic