Material Notes:
Scotchkote Urethane Floor Coating FB 857 has been specifically developed as a 100% solids protection system with a degree of flexibility for application to concrete and asphalt floor surfaces.Product Features:Combines good application characteristics with excellent corrosion protection and chemical resistanceDesigned for application by brush or roller Designed for use on concrete surfaces in combination with 3M Scotchkote Urethane Sealer 165CSAlso suitable for use on asphalt floor surfaces in combination with 3M Scotchkote Urethane Primer FB856.Information provided by 3M
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 10.8 MPa
1570 psi
ASTM D638
Elongation at Break 55 %
55 %
ASTM D412
Impact Test 12.43 J
9.168 ft-lb
ASTM D2794
Abrasion 80
80
[mg] per 1000 cycles, 1 kg, CS17 Wheel; ASTM D4060
Processing Properties Metric English Comments
Cure Time 300 min
5.00 hour
Touch Dry
960 min
16.0 hour
Hard Dry
10100 min
168 hour
Full Cure